Aerogels are three-dimensional ultra-light porous structures whose characteristics make them exciting candidates for research, development and commercialization leading to a broad scope of applications ranging from insulation and catalysis to regenerative medicine and pharmaceuticals. Biopolymers have recently entered the aerogel foray. In order to fully realize their potential, progressive strategies dealing with production times and costs reduction must be put in place to facilitate the scale up of aerogel production from lab to commercial scale. The necessity of studying solvent/matrix interactions during solvent exchange and supercritical CO2 drying is presented in this study using calcium alginate as a model system. Four frameworks, namely (a) solvent selection methodology based on solvent/polymer interaction; (b) concentration gradient influence during solvent exchange; (c) solvent exchange kinetics based on pseudo second order model; and (d) minimum solvent concentration requirements for supercritical CO2 drying, are suggested that could help assess the role of the solvent in biopolymer aerogel production.
1 November 2019 in The Journal of Supercritical Fluids
Protein aerogel particles prepared by supercritical-CO2-drying (SCD) of ground whey protein (WP) hydrogels (20% w/w, pH 5.7) were converted into oleogels by dispersion in selected edible oils (castor, cod liver, corn, flaxseed, MCT, peanut and sunflower oil). The obtained oleogels were analysed for oil content, microstructure, rheological properties, and ATR-FTIR spectra. Except for castor oil, solid-like, plastic materials with comparable composition (80% oil, 20% WP) and rheological properties (G′~3.5 × 105 Pa, G″~0.20 × 105 Pa, critical stress~800 Pa, tanδ~0.060) were obtained. Optical and confocal microscopy showed that the generated structure was associated with the capillary-driven absorption of oil into the porous aerogel particles interconnected via particle-particle interactions. In this structure, the oil was stably entrapped. Results evidenced the reduced role of edible oil characteristics with the exception of castor oil, whose high polarity probably favoured particle–oil interactions hindering particle networking. This work demonstrates that WP aerogels could be regarded as versatile oleogel templates allowing the structuring of many edible oils into solid-like materials.
Chronic non-healing wounds represent a substantial economic burden to healthcare systems and cause a considerable reduction in quality of life for those affected. Approximately 0.5–2% of the population in developed countries are projected to experience a chronic wound in their lifetime, necessitating further developments in the area of wound care materials. The use of aerogels for wound healing applications has increased due to their high exudate absorbency and ability to incorporate therapeutic substances, amongst them trace metals, to promote wound-healing. This study evaluates the swelling behavior of Ca-Zn-Ag-loaded alginate aerogels and their metal release upon incubation in human sweat or wound fluid substitutes. All aerogels show excellent liquid uptake from any of the formulas and high liquid holding capacities. Calcium is only marginally released into the swelling solvents, thus remaining as alginate bridging component aiding the absorption and fast transfer of liquids into the aerogel network. The zinc transfer quota is similar to those observed for common wound dressings in human and animal injury models. With respect to the immune regulatory function of zinc, cell culture studies show a high availability and anti-inflammatory activity of aerogel released Zn-species in RAW 264.7 macrophages. For silver, the balance between antibacterial effectiveness versus cytotoxicity remains a significant challenge for which the alginate aerogels need to be improved in the future. An increased knowledge of the transformations that alginate aerogels undergo in the course of the fabrication as well as during wound fluid exposure is necessary when aiming to create advanced, tissue-compatible aerogel products.
Although the first reports on aerogels made by Kistler1 in the 1930s dealt with aerogels from both inorganic oxides (silica and others) and biopolymers (gelatin, agar, cellulose), only recently have biomasses been recognized as an abundant source of chemically diverse macromolecules for functional aerogel materials. Biopolymer aerogels (pectin, alginate, chitosan, cellulose, etc.) exhibit both specific inheritable functions of starting biopolymers and distinctive features of aerogels (80-99% porosity and specific surface up to 800 m2/g). This synergy of properties makes biopolymer aerogels promising candidates for a wide gamut of applications such as thermal insulation, tissue engineering and regenerative medicine, drug delivery systems, functional foods, catalysts, adsorbents and sensors. This work demonstrates the use of pressurized carbon dioxide (5 MPa) for the ionic cross linking of amidated pectin into hydrogels. Initially a biopolymer/salt dispersion is prepared in water. Under pressurized CO2 conditions, the pH of the biopolymer solution is lowered to 3 which releases the crosslinking cations from the salt to bind with the biopolymer yielding hydrogels. Solvent exchange to ethanol and further supercritical CO2 drying (10 - 12 MPa) yield aerogels. Obtained aerogels are ultra-porous with low density (as low as 0.02 g/cm3), high specific surface area (350 - 500 m2/g) and pore volume (3 - 7 cm3/g for pore sizes less than 150 nm).
In this work, nanostructured and transparent cellulose aerogels are synthesized via a purely salt induced approach from non‐modified microcrystalline cellulose type II. The production process requires in contrast to state of the art methods no pretreatment of cellulose or use of expensive cellulose‐solvents: it consists of hydrogel formation via cross‐linking of cellulose with calcium ions, a solvent exchange and a supercritical drying step. A systematic multiparameter study reveals that a high level of structural control is achievable: ratios of macro‐ to mesoporosity and the size of mesopores can be tailored by adjustment of the calcium ion content, while keeping a high overall porosity in the range of 92% – 96 %. The build‐up of homogeneous, fine pore structures results in a significant increase of the specific surface area as compared to conventional calcium‐free aerogels (684 vs. 300 m2 g−1). Remarkably, the Ca2+‐cross‐linking renders aerogels transparent, with Rayleigh scattering being the dominant scattering mechanism. Additional ion exchange to Ca2+ in the hydrogel‐state leads to further reduction of the pore size and to products with optimized optical properties, e.g., light transmission of 91% at an incidents light wavelength of 800 nm and a substrate thickness of 1.5 mm.