A surface sensitivity study was performed on different transition-metal dichalcogenides (TMDs) under ambient conditions in order to understand which material is the most suitable for future device applications. Initially, Atomic Force Microscopy and Scanning Electron Microscopy studies were carried out over a period of 27 days on mechanically exfoliated flakes of 5 different TMDs, namely, MoS2, MoSe2, MoTe2, HfS2, and HfSe2. The most reactive were MoTe2 and HfSe2. HfSe2, in particular, showed surface protrusions after ambient exposure, reaching a height and width of approximately 60 nm after a single day. This study was later supplemented by Transmission Electron Microscopy (TEM) cross-sectional analysis, which showed hemispherical-shaped surface blisters that are amorphous in nature, approximately 180–240 nm tall and 420–540 nm wide, after 5 months of air exposure, as well as surface deformation in regions between these structures, related to surface oxidation. An X-ray photoelectron spectroscopy study of atmosphere exposed HfSe2 was conducted over various time scales, which indicated that the Hf undergoes a preferential reaction with oxygen as compared to the Se. Energy-Dispersive X-Ray Spectroscopy showed that the blisters are Se-rich; thus, it is theorised that HfO2 forms when the HfSe2 reacts in ambient, which in turn causes the Se atoms to be aggregated at the surface in the form of blisters. Overall, it is evident that air contact drastically affects the structural properties of TMD materials. This issue poses one of the biggest challenges for future TMD-based devices and technologies.
3 September 2019 in npj 2D Materials and Applications
In this work, we present a comprehensive theoretical and experimental study of quantum confinement in layered platinum diselenide (PtSe2) films as a function of film thickness. Our electrical measurements, in combination with density functional theory calculations, show distinct layer-dependent semimetal-to-semiconductor evolution in PtSe2 films, and highlight the importance of including van der Waals interactions, Green’s function calibration, and screened Coulomb interactions in the determination of the thickness-dependent PtSe2 energy gap. Large-area PtSe2 films of varying thickness (2.5–6.5 nm) were formed at 400 °C by thermally assisted conversion of ultra-thin platinum films on Si/SiO2 substrates. The PtSe2 films exhibit p-type semiconducting behavior with hole mobility values up to 13 cm2/V·s. Metal-oxide-semiconductor field-effect transistors have been fabricated using the grown PtSe2 films and a gate field-controlled switching performance with an ION/IOFF ratio of >230 has been measured at room temperature for a 2.5–3 nm PtSe2 film, while the ratio drops to <2 for 5–6.5 nm-thick PtSe2 films, consistent with a semiconducting-to-semimetallic transition with increasing PtSe2 film thickness. These experimental observations indicate that the low-temperature growth of semimetallic or semiconducting PtSe2 could be integrated into the back-end-of-line of a silicon complementary metal-oxide-semiconductor process.
The authors investigate the implications of amorphizing ion implants on the crystalline integrity of sub- wide fin field-effect transistors (FinFETs). Recrystallization of thin body silicon is not as straightforward as that of bulk silicon because the regrowth direction may be parallel to the silicon surface rather than terminating at it. In sub- wide FinFETs surface proximity suppresses crystal regrowth and promotes the formation of twin boundary defects in the implanted regions. In the case of a amorphization depth, random nucleation and growth leads to polycrystalline silicon formation in the top of the fin, despite being only from the crystalline silicon seed.
Time evolution of the chemical profile, electrical activity, and regrowth of P implanted in Ge at a concentration above the maximum equilibrium solubility is investigated at rapid thermal annealing temperature. During the first anneal, a second, epitaxial regrowth of a part of the amorphous layer leads to P trapping in substitutional sites at a level of about . However, nonsubstitutional P atoms frozen in the crystal at high concentration during recrystallization form large, inactive precipitates of peculiar circular shape. Simultaneously, long annealing time leads to continuing, extensive P out- and indiffusion affecting both the P chemical profile and junction sheet resistance.
The recently observed phenomenon of boron uphill diffusion during low-temperature annealing of ultrashallow ion-implanted junctions in silicon has been investigated. It is shown that the effect is enhanced by preamorphization, and that an increase in the depth of the preamorphized layer reduces uphill diffusion in the high-concentration portion of boron profile, while increasing transient enhanced diffusion in the tail. The data demonstrate that the magnitude of the uphill diffusion effect is determined by the proximity of boron and implant damage to the silicon surface.
We investigate scalability, performance and variability of high aspect ratio trigate FinFETs fabricated with 193 nm immersion lithography and conventional dry etch. FinFETs with fin widths down to 5nm are achieved with record aspect ratios of 13. Excellent nMOS and pMOS performance is demonstrated for narrow fins and short gates. Further improvement in nMOS performance can be achieved by eliminating access resistance that is currently attributed to poor re-crystallization of implantation damage in narrow fins. Fully-depleted FinFETs show strongly improved short channel effect (SCE) control when the fin width is scaled, even without halo-implants. Nearly ideal DIBL and sub-threshold slope (SS) are achieved down to 30nm gate length. Low leakage devices are realized by combining a fully depleted channel, HfSiO high-k dielectric, mid-gap TiN metal electrodes, and aggressive fin width scaling. Symmetrical threshold voltages (±0.35 V) are achieved. It is demonstrated that selective epitaxial growth on source and drain regions is essential to limit parasitic resistance in narrow fin devices. Parametric spread is dominated by gate length variations in short devices but within-die fin width variations are still evident for long devices.