Lead free piezoelectric materials are being intensively investigated in order to substitute lead based ones, commonly used in many different applications. Among the most promising lead-free materials are those with modified NaNbO3, such as (K, Na)NbO3 (KNN) and (Ba, Na)(Ti, Nb)O3 (BTNN) families. From a ceramic processing point of view, high density single phase KNN and BTNN ceramics are very difficult to sinter due to the volatility of the alkaline elements, the narrow sintering temperature range and the anomalous grain growth. In this work, Spark Plasma Sintering (SPS) and high-energy ball milling (HEBM), following heat treatments (calcining and sintering), in oxidative (O2) atmosphere have been used to prepare single phase highly densified KNN (“pure” and Cu2+ or Li1+ doped), with theoretical densities ρth > 97% and BTNN ceramics (ρth - 90%), respectively. Using BTTN ceramics with a P4mm perovskite-like structure, we showed that by increasing the NaNbO3 content, the ferroelectric properties change from having a relaxor effect to an almost “normal” ferroelectric character, while the tetragonality and grain size increase and the shear piezoelectric coefficients (k15, g15 and d15) improve. For KNN ceramics, the results reveal that the values for remanent polarization as well as for most of the coercive field are quite similar among all compositions. These facts evidenced that Cu2+ may be incorporated into the A and/or B sites of the perovskite structure, having both hardening and softening effects.
18 December 2018 in Journal of the American Ceramic Society
In this work, (K0.48Na0.52)NbO3 (KNN) ceramics were prepared by using Spark Plasma Sintering (SPS) method applying different heating rates. The microstructural evolution of the ceramics was analyzed and the results were correlated with possible sintering mechanisms. The analysis revealed homogeneous microstructures with nanometric grains. It was noticed that with increasing the heating rate the grain size decreases and the bimodal grain growth is suppressed. The Master Sintering Curve was constructed and an apparent activation energy of 660 kJ/mol was determined. From this result, it was possible to predict the possible densification mechanisms present in the KNN by SPS route.
In this work, it was investigated the structural quality of the calcined (Na0.52,K0.48)NbO3 powders by two methods: by reacting the sodium carbonate with Nb2O5 in either monoclinic or orthorhombic phases and by using a fast calcination method. It was found that the degree and quality of the reactions among the precursor powders have a strong influence on the structural quality of the KNN powders. The data suggest that the reactions of transformation occur in two stages for conventionally calcined powders, in which the second reaction, at higher temperatures, leads to a better crystallization. On the other hand, fast calcination also reveals to be an effective method to produce well-crystallized KNN powders.