Thermoelectric properties of pure polycrystalline CaMnO3 ceramics were significantly enhanced by increasing sintering holding time from 1 to 24 h. The Seebeck coefficient values were reduced while the sintering holding time was increased, and the DC electrical conductivity was enhanced from 255 S/m to 1.748 S/m. This same effect was observed in electronic thermal conductivity, increasing from 5x10-3 to 3.5x10-2W/m K, whereas the lattice thermal conductivity decreased from 5.0 to 4.0 W/m K at 873K. Overall, CaMnO3 ceramic sintered for 24 h demonstrated the best performance, which presented a Figure-of-Merit value of about 0.03. The grain size of the samples ranged from 2.79 µm to 6.45 µm, due to the sintering holding time, directly influencing the high-temperature thermoelectric properties of CaMnO3 ceramics.
Ca3Co4O9 powders and ceramics were synthesized and sintered using microwave-assisted heating method.Another batch of powders was calcined by the conventional heating method and this powder was used to produce ceramics sintered by microwave sintering aiming to compare with those prepared by microwave method. The formation of the phases based on calcination method and time was assessed by X-ray diffractometry. The synthesis and sintering methods affected various properties of the ceramics, including grain size, density, phase amount, Seebeck coefficient, thermal conductivity and electrical conductivity. Microwave heating method reduced the time required for the powder synthesis and sintering of ceramics. Ceramics produced using powder obtained by the conventional method presented Figure of Merit (ZT) values of approximately 0.04. However, these values were reduced for the ceramics produced by microwave heating reaching a value of about 0.02. The evaluation of the thermoelectric properties of the Ca3Co4O9 ceramics suggests that the main issue to enhance the Figure of Merit of the CCO ceramics is related to density and Ca3Co4O9 phase amount present in the ceramics.