Novel polymeric flame retardants based on two acrylamides and 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide (DOPO) or 5,5-dimethyl-[1,3,2]dioxaphosphinane-2-oxide (DDPO) are described for several applications in HexFlow® RTM6, a high-performance epoxy resin. Neat resin samples and carbon fiber-reinforced composites were tested for their glass transition temperatures (dynamic mechanical analysis), thermal stability (thermogravimetric analyses), flammability (UL94) and flame-retardant performance (Cone Calorimetry). Additionally, the fiber degradation occurring during combustion of carbon fiber-reinforced epoxy resins was observed by scanning electron microscopy to show the fiber protecting effect of these flame retardants. Whereas DOPO-containing polyacrylamides acting mainly in the gas phase showed the best flame retardant efficiency, DDPO-containing polyacrylamides acting mainly in the condensed phase showed the best fiber protection. A mixed polyacrylamide was synthesized to combine these effects. This thermoplastic is soluble in the resin and, therefore, suitable for injection molding processes. Interlaminar shear strength measurements showed no negative effect of the flame retardant. The versatility of these flame retardants is shown by investigations dealing with boehmite as synergist in neat resin samples.
This study focuses on understanding and prediction of short-term thermal degradation of polymer matrix composites. One sided irradiation of two commercial composites (HexPly® 8552/IM7 and M18-1/G939) is carried out on specimens of various thickness (2, 4, 6 mm) at different heat fluxes (50 and 80 kW/m2) for various exposure times prior to ignition. The aim is to correlate the amount of the applied thermal energy with the heat damage and the residual mechanical strength. Among the two primary components of each matrix the epoxy resin is observed to degrade faster than the thermoplastic under thermal load, as measured by IR spectroscopy. A correlation is achieved between the interlaminar shear strengths and the relative amount of the residual matrix components. The interlaminar shear strengths and degradation processes are assessed in dependence of the applied energy per volume. The derived relationships and a chemometric analysis of IR spectra, can be used to rapidly estimate mechanical properties, as well as other properties of specimens with unknown thermal preload. Degradation processes are discussed in detail.
Commercially available carbon fiber reinforced polymer matrix composite panels (Hexply® M18-1/G939 and 8552/IM7) with different thicknesses (1-6 mm) were exposed to continuous-wave high-energy laser radiation at various laser powers up to 10 kW under static conditions. The perforation times, the size of the damaged volume and the residual compressive strengths are determined and correlated to the irradiation parameters. It is found that for the time of perforation, the damaged volume, which is approximated by a cylinder shaped model, correlates linearly with the laser energy imposed onto the sample surface. This relationship can be used for a prediction of the perforation time for various laser powers, material thicknesses and laser spot diameters. Increasing laser energy results in a decay of residual compressive strength after impact. Visual inspection as well as micro-focused computed X-ray tomography and scanning electron microscopy indicate a small area of thermal damage outside the laser spot. Additionally, infrared spectroscopy characterizes incipient heat damage most sensitively.