The flow pattern is vital for the metallurgical performance of continuous casting tundishes. The purpose of this study was to design and optimize the flow characteristics inside a four-strand tundish. Numerical simulations and water model experiments were validated and utilized to investigate the flow behavior. The effect of different flow rates in the original tundish was evaluated; two modified retaining walls and a new ladle shroud were designed for optimization. The molten steel inside the original tundish tends to be more active as the flow rate increases from 3.8 L/min to 6.2 L/min, which results in a reduction in dead volume from 36.47% to 17.59% and better consistency between different outlets. The dead volume and outlet consistency inside the tundish are improved significantly when the modified walls are applied. The proper design of the diversion hole further enhances the plug volume from 6.39% to 13.44% of the tundish by forming an upstream circular flow in the casting zone. In addition, the new trumpet ladle shroud demonstrates an advantage in increasing the response time from 152.5 s to 167.5 s and alleviating the turbulence in the pouring zone, which is beneficial for clean steel production.
In recent years, the shipbuilding industry has experienced a growing demand for tighter control and higher strength requirements in thick steel plate welding. Electro-gas welding (EGW) is a high heat input welding method, widely used to improve the welding efficiency of thick plates. Modelling the EGW process of thick steel plates has been challenging due to difficulties in accurately depicting the heat source path movement. An EGW experiment on 30 mm thickness E36 steel plates was conducted in this study. A semi-ellipsoid heat source model was implemented, and its movement was mathematically expressed using linear, sinusoidal, or oscillate-stop paths. The geometry of welding joints, process variables, and steel composition are taken from industrial scale experiments. The resulting thermal evolutions across all heat source-path approaches were verified against experimental observations. Practical industrial recommendations are provided and discussed in terms of the fusion quality for E36 steel plates with a heat input of 157 kJ/cm. It was found that the oscillate-stop heat path predicts thermal profile more accurately than the sinusoidal function and linear heat path for EGW welding of 30 mm thickness and above. The linear heat path approach is recommended for E36 steel plate thickness up to 20 mm, whereas maximum thickness up to 30 mm is appropriate for sinusoidal path, and maximum thickness up to 35 mm is appropriate for oscillate-stop path in EGW welding, assuming constant heat input.
Marine steel requires excellent toughness and corrosion resistance in a low-temperature seawater environment. In this study, corrosion tests on E40 steel were performed, including electrochemical testing of the weld metal and heat-affected zone, dynamic corrosion testing in a simulated seawater environment, and the analysis and comparison of results obtained using different methods. The corrosion resistance of E40 was determined by measuring the saturation current density of the anodic dissolution of the steel in a corrosive medium by an electrochemical method. Under laboratory conditions, the corrosion resistance was investigated under simulated seawater. The results showed that regions with uneven microhardness corresponded to the inhomogeneity of the corrosion potential, with measured fluctuations of up to 40 mV. Nanoscale corrosive–aggressive non-metallic inclusions served as a substrate for the deposition of titanium and niobium carbonitrides, thereby weakening the corrosion resistance. The corrosion rate of the base metal was 1.16–1.64 mm/year, which was slightly higher than that of the heat-affected zone. The influence of deposition on the corrosion performance of welded joints under different deoxygenation processes was studied, and the deposition composition was controlled by a deoxygenation process to improve the corrosion resistance of the steel plate.