In this study, the grain growth behaviour of ZnO-V2O5-based ceramics with 0.25–0.75 mol% additions of PrMnO3 was systematically investigated during sintering from 850 °C to 925 °C. with the aim to control the ZnO grain size for their application as varistors. It was found that with the increased addition of PrMnO3, in addition to the decrease in the average grain size, the grain size distribution also narrowed and eventually changed from a bimodal to unimodal distribution after a 0.75 mol% PrMnO3 addition. The grain growth control was achieved by a pinning effect of the secondary ZnCr2O4 and PrVO4 phases at the ZnO grain boundaries. The apparent activation energy of the ZnO grain growth in these ceramics was found to increase with increased additions of PrVO4, hence the observed reduction in the ZnO grain sizes.
Fe-Al2O3 composites were prepared by pressureless sintering, using Bayan Obo iron concentrate and bauxite as the main raw materials, activated carbon was added as the reducing agent. The effects of different bauxite additions on the phase composition, microstructures, mechanical properties, and the corrosion-resistance were investigated. The results show that the average grain size of alumina decreased as the bauxite content increased. In addition, bauxite contains TiO2, CaO, and MgO, that can form a liquid phase at high temperature, causing the heat capacity of the micro-zone around the metal phase to be different, which leads to a change of undercooling and further affects the dislocation density of the metal phase. The plastic deformation ability of the metal phase can be improved with the low dislocation density. Fracture mechanism analysis indicated that the metal phase absorbed energy through plastic deformation. The optimum performance of the sample was as follows: the flexural strength was 310 MPa, the hardness 12.14 GPa, the alkali resistance 98.32%, and the acid resistance 95.44%.