It is a useful way to stabilize the elements of heavy metal in the glass-ceramics with the form of ions due to the environmental pollution of heavy metal, such as Cr. The glass-ceramics of excellent combination properties were prepared, and the effect of stabilizing Cr-containing stainless steel slag with different concentrations of nitric acid leaching test were investigated. It was found that the major crystalline phase was diopside or anorthite with or without the amount stainless steel slag. Moreover, the continuous refinement of grains exhibited with the increase of amount of stainless steel slag. The results indicated that the excellent physical and mechanical properties, including density (2.9 g/cm3), hardness (729.27HV0.3), bending strength (222.9 MPa), and the solid solution of Cr in excess of 0.00057% for the glass-ceramics were related to the change of microstructure and phase structure. There showed the potential for reusing and detoxifying stainless steel slag.
31 October 2018 in Journal of Materials Science: Materials in Electronics
Mg2Ni-type Mg2Ni1−xCox (x = 0, 0.1, 0.2, 0.3, 0.4) alloys were fabricated by melt spinning technique. The structures of the as-spun alloys were characterized by X-ray diffraction (XRD) and transmission electron microscopy (TEM). The hydrogen absorption and desorption kinetics of the alloys were measured by an automatically controlled Sieverts apparatus. The electrochemical hydrogen storage kinetics of the as-spun alloys was tested by an automatic galvanostatic system. The results show that the as-spun (x = 0.1) alloy exhibits a typical nanocrystalline structure, while the as-spun (x = 0.4) alloy displays a nanocrystalline and amorphous structure, confirming that the substitution of Co for Ni notably intensifies the glass forming ability of the Mg2Ni-type alloy. The melt spinning treatment notably improves the hydriding and dehydriding kinetics as well as the high rate discharge ability (HRD) of the alloys. With an increase in the spinning rate from 0 (as-cast is defined as spinning rate of 0 m/s) to 30 m/s, the hydrogen absorption saturation ratio () of the (x = 0.4) alloy increases from 77.1 to 93.5%, the hydrogen desorption ratio () from 54.5 to 70.2%, the hydrogen diffusion coefficient (D) from 0.75 × 10−11 to 3.88 × 10−11 cm2/s and the limiting current density IL from 150.9 to 887.4 mA/g.
Impurity removal and modification of rare earth concentrate powder were conducted by roasting weak acid-weak alkali leaching to obtain the active components of denitrification catalysts. NH3 selective catalytic reduction catalyst samples were prepared by mixing and kneading with pseudo-γ-Al2O3 boehmite as carrier. The results showed that the Ce7O12 content in the active component samples increased and dispersed more evenly. The grain size of the samples was refined, the specific surface area increased, and the active sites exposed more. Ce coexists in the form of Ce3+ and Ce4+. Fe coexists in the form of Fe3+ and Fe2+, but Fe3+ is abundant. Some Ce, La, Nd, Pr, Fe, Mn, and other components formed solid melts during preparation, which increased the synergistic catalytic effect. The denitrification efficiency of the catalyst sample was 92.8% under the conditions of reaction temperature 400 °C, NO content was 600 ppm, NH3/NO ratio was 1.5, and O2 concentration was 4%.
Fe-Al2O3 composites were prepared by pressureless sintering, using Bayan Obo iron concentrate and bauxite as the main raw materials, activated carbon was added as the reducing agent. The effects of different bauxite additions on the phase composition, microstructures, mechanical properties, and the corrosion-resistance were investigated. The results show that the average grain size of alumina decreased as the bauxite content increased. In addition, bauxite contains TiO2, CaO, and MgO, that can form a liquid phase at high temperature, causing the heat capacity of the micro-zone around the metal phase to be different, which leads to a change of undercooling and further affects the dislocation density of the metal phase. The plastic deformation ability of the metal phase can be improved with the low dislocation density. Fracture mechanism analysis indicated that the metal phase absorbed energy through plastic deformation. The optimum performance of the sample was as follows: the flexural strength was 310 MPa, the hardness 12.14 GPa, the alkali resistance 98.32%, and the acid resistance 95.44%.