View All Publications
31 July 2018 in Applied Sciences
Verified
Journal Article
Open access
PDF file
NGNathalie Godin
Nathalie Godin
PRPascal Reynaud
Pascal Reynaud
Gilbert FantozziGilbert Fantozzi
Gilbert Fantozzi
Acoustic emission is a part of structural health monitoring (SHM) and prognostic health management (PHM). This approach is mainly based on the activity rate and acoustic emission (AE) features, which are sensitive to the severity of the damage mechanism. A major issue in the use of AE technique is to associate each AE signal with a specific damage mechanism. This approach often uses classification algorithms to gather signals into classes as a function of parameters values measured on the signals. Each class is then linked to a specific damage mechanism. Nevertheless, each recorded signal depends on the source mechanism features but the stress waves resulting from the microstructural changes depend on the propagation and acquisition (attenuation, damping, surface interactions, sensor characteristics and coupling). There is no universal classification between several damage mechanisms. The aim of this study is the assessment of the influence of the type of sensors and of the propagation distance on the waveforms parameters and on signals clustering.

16 June 2017 in Materials
Verified
Journal Article
Open access
PDF file
ERElie Racle
Elie Racle
NGNathalie Godin
Nathalie Godin
PRPascal Reynaud
Pascal Reynaud
Gilbert FantozziGilbert Fantozzi
Gilbert Fantozzi
The fatigue behavior of a Ceramic Matrix Composite (CMC) at intermediate temperature under air is investigated. Because of the low density and the high tensile strength of CMC, they offer a good technical solution to design aeronautical structural components. The aim of the present study is to compare the behavior of this composite under static and cyclic loading. Comparison between incremental static and cyclic tests shows that cyclic loading with an amplitude higher than 30% of the ultimate tensile strength has significant effects on damage and material lifetimes. In order to evaluate the remaining lifetime, several damage indicators, mainly based on the investigation of the liberated energy, are introduced. These indicators highlight critical times or characteristic times, allowing an evaluation of the remaining lifetime. A link is established with the characteristic time around 25% of the total test duration and the beginning of the matrix cracking during cyclic fatigue.

13 December 2019 in Ceramics
Verified
Journal Article
Open access
PDF file
HHHussein Hammoud
Hussein Hammoud
VGVincent Garnier
Vincent Garnier
Gilbert FantozziGilbert Fantozzi
Gilbert Fantozzi
ELEtienne Lachaud
Etienne Lachaud
STSolène Tadier
Solène Tadier
An investigation of MgAl2O4 spinel and Y3Al2O5 (YAG) materials sintered by spark plasma sintering (SPS) was performed. The optical properties of the materials are modified depending on the powder source and the SPS sintering conditions. Spectrophotometer and Raman analysis are presented in this work, along with optical and scanning electron microscope (SEM) observations and cathodoluminescence analysis. The results show a correlation between carbon contamination and the optical properties of the materials. Herein, the source of the contamination is explained, along with its genesis and diffusion. The carbon contamination originates from the powder itself (carbonates), as well as the SPS environment (papiex® graphite foil, graphite die, graphite felt) to form carbon clusters. During the high-temperature SPS process, carbon from those carbon clusters diffuses, resulting in an increase in the contamination volume, thereby increasing the light absorption.

24 March 2020 in Materials
Verified
Journal Article
Open access
PDF file
Longbiao LiLongbiao Li
Longbiao Li
PRPascal Reynaud
Pascal Reynaud
Gilbert FantozziGilbert Fantozzi
Gilbert Fantozzi
Cycle-dependent damage evolution in self-healing, 2.5D woven Hi-NicalonTM SiC/[Si-B-C] and 2D woven Hi-NicalonTM SiC/[SiC-B4C] ceramic-matrix composites (CMCs) at 600 and 1200 °C was investigated. The cycle-dependent damage parameters of internal friction, dissipated energy, Kachanov’s damage parameter, and broken fiber fraction were obtained to describe damage development in self-healing CMCs. The relationships between cycle-dependent damage parameters and multiple fatigue damage mechanisms were established. The experimental fatigue damage development of self-healing Hi-NicalonTM SiC/[Si-B-C] and Hi-NicalonTM SiC/[SiC-B4C] composites was predicted for different temperatures, peak stresses, and loading frequencies. The cycle-dependent damage evolution of self-healing Hi-NicalonTM SiC/[Si-B-C] and Hi-NicalonTM SiC/[SiC-B4C] composites depends on temperature, testing environment, peak stress, and loading frequency. For the Hi-NicalonTM SiC/[Si-B-C] composite, temperature is a governing parameter for the fatigue process. At an elevated temperature of 600 °C in an air atmosphere, the internal frictional parameter of Hi-NicalonTM SiC/[Si-B-C] composite decreases first and then increases with applied cycle number; however, at an elevated temperature of 1200 °C in an air atmosphere, the internal frictional parameter of Hi-NicalonTM SiC/[Si-B-C] composite decreases with applied cycle number, and the interface shear stress at 1200 °C is much lower than that at 600 °C. For Hi-NicalonTM SiC/[SiC-B4C] composite at 1200 °C, loading frequency is a governing parameter for the fatigue process. The degradation rate of interface shear stress is much higher at the loading frequency of 0.1 Hz than that at the loading frequency of 1 Hz.

3 February 2016 in Applied Sciences
Verified
Journal Article
Open access
PDF file
NGNathalie Godin
Nathalie Godin
PRPascal Reynaud
Pascal Reynaud
MRMohamed R’mili
Mohamed R’mili
Gilbert FantozziGilbert Fantozzi
Gilbert Fantozzi
Non-oxide fiber-reinforced ceramic-matrix composites are promising candidates for some aeronautic applications that require good thermomechanical behavior over long periods of time. This study focuses on the behavior of a SiCf/[Si-B-C] composite with a self-healing matrix at intermediate temperature under air. Static fatigue experiments were performed below 600 °C and a lifetime diagram is presented. Damage is monitored both by strain measurement and acoustic emission during the static fatigue experiments. Two methods of real-time analysis of associated energy release have been developed. They allow for the identification of a characteristic time that was found to be close to 55% of the measured rupture time. This critical time reflects a critical local energy release assessed by the applicability of the Benioff law. This critical aspect is linked to a damage phase where slow crack growth in fibers is prevailing leading to ultimate fracture of the composite.

31 May 2023 in Ceramics
Verified
Journal Article
Open access
PDF file
KHKhadidja Hoggas
Khadidja Hoggas
SBSALIM BENAISSA
SALIM BENAISSA
ACAbdelbaki Cherouana
Abdelbaki Cherouana
SBSofiane Bouheroum
Sofiane Bouheroum
AAAbdenacer Assali
Abdenacer Assali
Gilbert FantozziGilbert Fantozzi
Gilbert Fantozzi
In this work, a transparent nanostructured ceramic magnesium aluminate spinel (MgAl2O4) was fabricated by Spark Plasma Sintering (SPS) from commercial spinel nano-powders at different temperatures (1300, 1350 and 1400 °C). The sintered samples were thoroughly examined to assess their microstructural, optical, and mechanical properties. Various techniques such as SEM, AFM, spectrophotometer with an integrating sphere, instrumented Vickers indenter, Pin-on-Disk tribometer, scratch tester, and sandblasting device were employed to characterize the sintered samples. The results indicated the significant impact of the sintering temperature on the properties of the spinel samples. Particularly, the samples sintered at T = 1350 °C exhibited the highest Real In-line Transmission (RIT = 72% at 550 nm and 80% at 1000 nm). These samples demonstrated the highest hardness value (HV = 16.7 GPa) compared to those sintered at 1300 °C (HV = 15.6 GPa) and 1400 °C (HV = 15.1 GPa). The measured fracture toughness of the sintered samples increased substantially with increasing sintering temperature. Similarly, the tribological study revealed that the friction coefficient of the sintered spinel samples increased with the sintering temperature, and the spinel sintered at 1350 °C exhibited the lowest wear rate. Additionally, sandblasting and scratch tests confirmed the significant influence of the sintering temperature on the mechanical properties of the fabricated spinels. Overall, the spinel sintered at 1350 °C presented the best compromise in terms of all the evaluated properties.