In this work, a transparent nanostructured ceramic magnesium aluminate spinel (MgAl2O4) was fabricated by Spark Plasma Sintering (SPS) from commercial spinel nano-powders at different temperatures (1300, 1350 and 1400 °C). The sintered samples were thoroughly examined to assess their microstructural, optical, and mechanical properties. Various techniques such as SEM, AFM, spectrophotometer with an integrating sphere, instrumented Vickers indenter, Pin-on-Disk tribometer, scratch tester, and sandblasting device were employed to characterize the sintered samples. The results indicated the significant impact of the sintering temperature on the properties of the spinel samples. Particularly, the samples sintered at T = 1350 °C exhibited the highest Real In-line Transmission (RIT = 72% at 550 nm and 80% at 1000 nm). These samples demonstrated the highest hardness value (HV = 16.7 GPa) compared to those sintered at 1300 °C (HV = 15.6 GPa) and 1400 °C (HV = 15.1 GPa). The measured fracture toughness of the sintered samples increased substantially with increasing sintering temperature. Similarly, the tribological study revealed that the friction coefficient of the sintered spinel samples increased with the sintering temperature, and the spinel sintered at 1350 °C exhibited the lowest wear rate. Additionally, sandblasting and scratch tests confirmed the significant influence of the sintering temperature on the mechanical properties of the fabricated spinels. Overall, the spinel sintered at 1350 °C presented the best compromise in terms of all the evaluated properties.
21 September 2023 in Optical and Quantum Electronics
This work employs moiré interferometry to investigate the influence of sintering temperature and sandblasting on the optical and mechanical properties of magnesium aluminate spinel (MgAl2O4). S25CRX14 Spinel pellets were fabricated via Spark Plasma Sintering (SPS) at 1300 °C, 1350 °C, and 1400 °C. The sintered samples were subsequently analyzed before and after sandblasting. Moiré interferometry, a non-destructive and contactless technique based on the superposition of tow linear transmission gratings, has proven particularly suitable for detecting micro-defects in transparent materials. The analysis of moiré fringes provided essential insights into the presence and size of defects, enabling accurate quality assessment without altering the samples. Its high spatial resolution, allowed the detection of even low-contrast defects. The results confirmed that the sintering temperature and sandblasting significantly influenced the mechanical and optical properties of the S25CRX14 spinel samples. The specimens sintered at 1350 °C exhibited the highest light transmission and the superior hardness. In contrast, the samples sintered at 1400 °C showed a notable degradation in their optical and mechanical properties. In conclusion, the pellets sintered at 1350 °C demonstrated the most favorable overall performance. This study confirms that moiré interferometry is a straightforward, accurate, and highly effective method for evaluating transparent ceramics, with very low implementation costs.