The influence of aluminum mole fraction of AlxGa1-xN/AlyGa1-yN multiple quantum wells (MQWs) on the optical polarization, light extraction efficiency (LEE) and external quantum efficiency (EQE) of deep ultra violet light emitting diodes in the wavelength range between 264 and 220 nm is investigated. The on-wafer EQE decreases from 0.6% to 0.00013% in this wavelength range. Polarization resolved photoluminescence and electroluminescence measurements show a change from dominant transverse-electric to dominant transverse-magnetic polarized light emission with increasing aluminum mole fraction in the MQW. The quantitative agreement with k·p calculations allow to ascribe this shift to a change of the characteristic of the Γ7+ valance band. Ray tracing simulations predict a reduction of the on-wafer LEE from 4% to 1.5%. Therefore the dramatic drop of the EQE in this wavelength range cannot be attributed to a drop in LEE and is most likely dominated by charge carrier injection and radiative recombination efficiency.
Deep UV-LEDs (DUV-LEDs) emitting at 233 nm with an emission power of (1.9 ± 0.3) mW and an external quantum efficiency of (0.36 ± 0.07) % at 100 mA are presented. The entire DUV-LED process chain was optimized including the reduction of the dislocation density using epitaxially laterally overgrown AlN/sapphire substrates, development of vanadium-based low resistance n-metal contacts, and employment of high thermally conductive AlN packages. Estimated device lifetimes above 1500 h are achieved after a burn-in of 100 h. With the integration of a UV-transparent lens, a strong narrowing of the far-field pattern was achieved with a radiant intensity of 3 mW/sr measured at 20 mA.
We report on the performance of AlGaN-based deep ultraviolet light-emitting diodes (UV-LEDs) emitting at 265 nm grown on stripe-patterned high-temperature annealed (HTA) epitaxially laterally overgrown (ELO) aluminium nitride (AlN)/sapphire templates. For this purpose, the structural and electro-optical properties of ultraviolet-c light-emitting diodes (UVC-LEDs) on as-grown and on HTA planar AlN/sapphire as well as ELO AlN/sapphire with and without HTA are investigated and compared. Cathodoluminescence measurements reveal dark spot densities of , , , and in multiple quantum well samples on as-grown planar AlN/sapphire, HTA planar AlN/sapphire, ELO AlN/sapphire, and HTA ELO AlN/sapphire, respectively, and are consistent with the threading dislocation densities determined by transmission electron microscopy (TEM) and high-resolution X-ray diffraction rocking curve. The UVC-LED performance improves with the reduction of the threading dislocation densities (TDDs). The output powers (measured on-wafer in cw operation at 20 mA) of the UV-LEDs emitting at 265 nm were 0.03 mW (planar AlN/sapphire), 0.8 mW (planar HTA AlN/sapphire), 0.9 mW (ELO AlN/sapphire), and 1.1 mW (HTA ELO AlN/sapphire), respectively. Furthermore, Monte Carlo ray-tracing simulations showed a 15% increase in light-extraction efficiency due to the voids formed in the ELO process. These results demonstrate that HTA ELO AlN/sapphire templates provide a viable approach to increase the efficiency of UV-LEDs, improving both the internal quantum efficiency and the light-extraction efficiency.
The electrical and structural properties of V/Al-based n-contacts on with an Al mole fraction ranging from to are investigated. Ohmic n-contacts are obtained up to with a contact resistivity of whereas for higher Al mole fraction the IV characteristics are rectifying. Transmission electron microscopy reveals a thin crystalline AlN layer formed at the metal/semiconductor interface upon thermal annealing. Compositional analysis confirmed an Al enrichment at the interface. The interfacial nitride-based layer in n-contacts on is partly amorphous and heavily contaminated by oxygen. The role and resulting limitations of Al in the metal stack for n-contacts on n-AlGaN with very high Al mole fraction are discussed. Finally, ultraviolet C (UVC) LEDs grown on and emitting at 232 nm are fabricated with an operating voltage of 7.3 V and an emission power of 120 μW at 20 mA in cw operation.
We report on AlGaN-based tunnel heterojunctions grown by metalorganic vapor phase epitaxy enabling fully transparent UVC LEDs by eliminating the absorbing p-AlGaN and p-GaN layers. Furthermore, the electrical characteristics can be improved by exploiting the higher conductivity of n-AlGaN layers as well as a lower resistance of n-contacts. UVC LEDs with AlGaN:Mg/AlGaN:Si tunnel junctions exhibiting single peak emission at 268 nm have been realized, demonstrating effective carrier injection into the AlGaN multiple quantum well active region. The incorporation of a low band gap interlayer enables effective tunneling and strong voltage reduction. Therefore, the interlayer thickness is systematically varied. Tunnel heterojunction LEDs with an 8 nm thick GaN interlayer exhibit continuous-wave emission powers near thermal rollover. External quantum efficiencies of 1.4% at a DC current of 5 mA and operating voltages of 20 V are measured on-wafer. Laterally homogeneous emission is demonstrated by UV-sensitive electroluminescence microscopy images. The complete UVC LED heterostructure is grown in a single epitaxy process including in situ activation of the magnesium acceptors.
4 June 2021 in Journal of Physics D: Applied Physics
The light extraction efficiency (LEE), external quantum efficiency (EQE), and current–voltage characteristics of deep ultraviolet light emitting diodes (DUV-LEDs) with different aluminum mole fractions in the p-AlGaN layers have been investigated. Optimizing the p-AlGaN layer composition requires a tradeoff between reducing the absorption losses and limiting the increases in the p-contact resistance and operation voltage. AlGaN multiple quantum well LEDs emitting around 263 nm with different AlGaN:Mg short period super lattices (p-SPSL) ranging from x = 33% (UV-absorbing) to x = 68% (UV-transparent) average aluminum mole fraction have been explored. DUV-LEDs with different p-contact metals and UV-reflectivities have been characterized by electroluminescence measurements and analyzed by ray-tracing simulations. The comparison shows an increased operating voltage and a five-fold increase of the on-wafer EQE with a maximum value of 3.0% for DUV-LEDs with UV-transparent p-SPSL (x = 68%) and UV-reflective indium contacts in comparison to LEDs with a UV-absorbing p-SPSL (x = 33%). Ray-tracing simulations show that the increase in EQE can be partially ascribed to a 2.5-fold improved LEE in combination with a two-fold increase in internal quantum efficiency.