Neysha Lobo-Ploch

Neysha Lobo-Ploch

Auto-generated profile, based on publicly available information

Neysha Lobo-Ploch

Ferdinand‐Braun‐Institut (FBH) Berlin Germany

Research Focus & Metrics

Academic Career Length

12Years (2015-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
14 September 2020 in Applied Physics Letters
Verified
Journal Article
Closed access
PDF file
NLNeysha Lobo-Ploch
Neysha Lobo-Ploch
FMFrank Mehnke
Frank Mehnke
LSLuca Sulmoni
Luca Sulmoni
HCHyun Kyong Cho
Hyun Kyong Cho
MGMartin Guttmann
Martin Guttmann
MKMichael Kneissl
Michael Kneissl
Deep UV-LEDs (DUV-LEDs) emitting at 233 nm with an emission power of (1.9 ± 0.3) mW and an external quantum efficiency of (0.36 ± 0.07) % at 100 mA are presented. The entire DUV-LED process chain was optimized including the reduction of the dislocation density using epitaxially laterally overgrown AlN/sapphire substrates, development of vanadium-based low resistance n-metal contacts, and employment of high thermally conductive AlN packages. Estimated device lifetimes above 1500 h are achieved after a burn-in of 100 h. With the integration of a UV-transparent lens, a strong narrowing of the far-field pattern was achieved with a radiant intensity of 3 mW/sr measured at 20 mA.

14 December 2020 in Applied Physics Letters
Verified
Journal Article
Closed access
PDF file
JRJan Ruschel
Jan Ruschel
JGJohannes Glaab
Johannes Glaab
NSNorman Susilo
Norman Susilo
SHSylvia Hagedorn
Sylvia Hagedorn
SWSebastian Walde
Sebastian Walde
MKMichael Kneissl
Michael Kneissl
The impact of different AlN/sapphire template technologies [i.e., planar, epitaxial lateral overgrown (ELO), and high temperature annealed sputtered ELO] is studied with respect to the operation-induced degradation of 265 nm UVC LEDs. UVC LEDs with identical heterostructures were grown on templates providing different threading dislocation densities in the range of 0.8 × 109 cm−2 to 5.8 × 109 cm−2. A long-term stress experiment was performed on batches of LEDs, which were operated at a direct current of 200 mA corresponding to a current density of 60 A/cm2 and at a heat sink temperature of 20 °C. The UVC LEDs on templates with lower threading dislocation densities were found to provide a higher optical power and to degrade slower during 2000 h of operation. The experiment demonstrates an extrapolated L70 lifetime of more than 10 000 h for the high temperature annealed sputtered ELO technology. The results suggest that degradation is caused by operation-induced activation of defects whose density scales with the dislocation density.

3 January 2022 in Journal of Applied Physics
Verified
Journal Article
Open access
PDF file
JGJ. Glaab
J. Glaab
JRJ. Ruschel
J. Ruschel
NPN. Lobo Ploch
N. Lobo Ploch
HCH. K. Cho
H. K. Cho
FMF. Mehnke
F. Mehnke
MKM. Kneissl
M. Kneissl
The impact of the operation parameters current and temperature on the degradation of AlGaN-based 233 nm far-ultraviolet-C LEDs is investigated. The observed effects can be divided into two groups: First, a rapid reduction in the optical power to about 50%–30% of the initial value during the first ∼100 h of operation, which is accompanied by an increase in the current below the diffusion voltage from 0.3 to about 1 μA, and a reduction in the hydrogen concentration in the p-side close to the active region. The second group is represented by a gradual reduction of the optical power, which runs in parallel to the effects in the first group and dominates for operation times ≥100 h. The reduction of the optical power is due to a decrease in the slope of the optical power–current characteristic. All effects are accelerated at increased stress currents and current densities—the reduction in the optical power at low (∼20 mA) and high measuring current (∼80 mA) scales with the current to the power of three. For example, after 250 h of operation, the relative optical power at a measuring current of 20 mA has decreased to about 40% when the LED was operated at a stress current of 20 mA and to <10% for a stress current of 100 mA. Furthermore, temperature has no significant impact on the reduction of the optical power during operation, i.e., the relative optical power reduced to about 25% after 250 h both when the LEDs were operated at 20 °C and when they were operated at 75 °C.

8 December 2022 in Physica Status Solidi (a)
Verified
Journal Article
Open access
AMAnton Muhin
Anton Muhin
MGMartin Guttmann
Martin Guttmann
VMVerena Montag
Verena Montag
NSNorman Susilo
Norman Susilo
EZEviathar Ziffer
Eviathar Ziffer
MKMichael Kneissl
Michael Kneissl
The electro‐optical characteristics of deep ultraviolet light‐emitting diodes (DUV LEDs) emitting at 265 nm and grown on AlN/sapphire templates with different threading dislocation densities, i.e., high‐temperature annealed (HTA) AlN, epitaxially laterally overgrown (ELO) AlN, and HTA‐ELO AlN are analyzed. The external quantum efficiency of each individual device is separated into maximum radiative recombination efficiency, carrier injection efficiency, and light extraction efficiency. This is achieved by combining an ABC‐model‐based fit of the current‐dependent external quantum efficiency together with calibrated Monte Carlo ray‐tracing simulations. A maximum radiative recombination efficiency between 50% and 60% is estimated for DUV LEDs grown on ELO and HTA‐ELO AlN/sapphire, whereas the values for devices grown on HTA AlN/sapphire are around 45%. The extracted radiative recombination efficiency does not scale with the measured threading dislocation density (TDD), even when accounting for the inhomogeneous TDD in the AlN base layers. This discrepancy is attributed to the formation of dislocation half‐loops introduced by additional compressive strain caused by the HTA process and may result in the formation of additional nonradiative recombination centers in the AlGaN multi‐quantum well region. In addition, the carrier injection efficiency values ranging from 45% to 55% are determined for devices grown on all three templates.

27 March 2023 in Applied Physics Letters
Verified
Journal Article
Open access
PDF file
JRJan Ruschel
Jan Ruschel
JTJens Wolfgang Tomm
Jens Wolfgang Tomm
JGJohannes Glaab
Johannes Glaab
TKTim Kolbe
Tim Kolbe
AKArne Knauer
Arne Knauer
SESven Einfeldt
Sven Einfeldt
InAlGaN-based UVB light-emitting diodes with an emission wavelength of 310 nm were operated at an elevated nominal current density of 200 A/cm2 and a heatsink temperature of 29 °C. The spatial intensity distributions of the electroluminescence and photoluminescence were measured before, during, and after dc stress. A decreasing homogeneity of the spatial intensity distributions with operation time was observed. It is concluded that the current density distribution changes during operation. Furthermore, the active region degrades more rapidly in the areas of higher current density. By quantitatively evaluating the current density distribution, it is proposed that a decreasing radiative recombination efficiency of the active region is causing the decrease in the total optical power of the LEDs during operation.

13 November 2015
Verified
Book Chapter
Closed access
PDF file
JRJens Rass
Jens Rass
NLNeysha Lobo-Ploch
Neysha Lobo-Ploch