High tensile strains in Ge are currently studied for the development of integrated laser sources on Si. In this work, we developed specific Germanium-On-Insulator 200 mm wafer to improve tolerance to high strains induced via shaping of the Ge layers into micro-bridges. Building on the high crystalline quality, we demonstrate bi-axial tensile strain of 1.9%, which is currently the highest reported value measured in thick (350 nm) Ge layer. Since this strain is generally considered as the onset of the direct bandgap in Ge, our realization paves the way towards mid-infrared lasers fully compatible with CMOS fab technology.
With the advent of high-brilliance synchrotron sources, the issue of beam damage on the samples deserves proper attention. It is especially true for operando studies in batteries, since the intense photon fluxes are commonly used to probe ever finer effects. Here we report on the causes and consequences of synchrotron X-ray beam damage in batteries, based on the case study of operando X-ray diffraction. We show that beam damage is caused by the mingled actions of dose and dose rate. The aftereffects can lie in a broad range, from mild modifications of the crystalline structure to artificial phase transitions, and can thus impede or bias the understanding of the mechanisms at play. We estimate the doses at which the different effects appear in two materials, suggesting that it could be expanded to other materials with the same technology. We also provide recommendations for the design of operando synchrotron experiments.
Advanced anode material designs utilizing dual phase alloy systems like Si/FeSi2 nano-composites show great potential to decrease the capacity degrading and improve the cycling capability for Lithium (Li)-ion batteries. Here, we present a multi-scale characterization approach to understand the (de-)lithiation and irreversible volumetric changes of the amorphous silicon (a-Si)/crystalline iron-silicide (c-FeSi2) nanoscale phase and its evolution due to cycling, as well as their impact on the proximate pore network. Scattering and 2D/3D imaging techniques are applied to probe the anode structural ageing from nm to μm length scales, after up to 300 charge-discharge cycles, and combined with modeling using the collected image data as an input. We obtain a quantified insight into the inhomogeneous lithiation of the active material induced by the morphology changes due to cycling. The electrochemical performance of Li-ion batteries does not only depend on the active material used, but also on the architecture of its proximity.