10 February 2017 in Modern Chemistry
Verified
Journal Article
Open access
PDF file
TMTahir Mehmood
Tahir Mehmood
AMAiman Mukhtar
Aiman Mukhtar
To understand the growth mechanism of Ag and Cu nanowires we have studied the effect of workfunction on the metal nanowire growth by XRD, SEM and Potentiostat. Under the same potential and overpotential, the metal with a smaller workfunction has a higher current density, i.e. current density for Ag is higher than of Cu nanowires. Likewise metals, the plane with smaller workfunction grows faster than with the larger workfunction, thus the preferential growth plane is (220) for both metals. We argued that the current arises from electrons tunneling from metal surface to hydrated metal and hydrogen ions. The metal with a smaller workfunction has a thinner barrier for tunneling, thus leading to a higher current density. It is found that deposition method have no such effect on the structure of deposited nanowires.

27 April 2021 in Materials
Verified
Journal Article
Open access
PDF file
XCXiaoming Cao
Xiaoming Cao
GLGu Liyuan
Gu Liyuan
SHShike Hu
Shike Hu
AMAiman Mukhtar
Aiman Mukhtar
KWKaiming Wu
Kaiming Wu
A lot of nanomaterials are using T1-T2 dual mode magnetic resonance (MR) contrast agents (CAs), but multilayer nanowire (NW) with iron (Fe) and manganese (Mn) as T1-T2 dual modal CAs has not been reported yet. Herein, we synthesized a Fe/Mn multilayer NW with an adjustable Fe layer, as T1-T2 dual-mode CAs. The relaxation performance of Fe/Mn multilayer NW was studied at 1.5 T. Results show that, when the length of the Fe layer is about 10 nm and the Mn is about 5 nm, the r1 value (21.8 mM−1s−1) and r2 value (74.8 mM−1s−1) of the Fe/Mn multilayer NW are higher than that of Mn NW (3.7 mM−1s−1) and Fe NW (59.3 mM−1s−1), respectively. We predict that our Fe/Mn multilayer NW could be used as T1-T2 dual mode MRI CAs in the near future.

6 June 2017 in American Journal of Electromagnetics and Applications
Verified
Journal Article
Open access
PDF file
AMAiman Mukhtar
Aiman Mukhtar
BKBabar Shahzad Khan
Babar Shahzad Khan
TMTahir Mehmood
Tahir Mehmood
Single crystalline cobalt nickel (Co-Ni) alloy nanowires are successfully fabricated using direct current (DC) electrodeposition with in the nanopore of highly ordered anodized aluminum oxide (AAO) template. SEM studies show that the average diameter of the alloy nanowires is approximately equal to 50 nm which corresponds to the pore size of the AAO template. Energy-dispersive X-ray (EDX) analysis confirmed that the Co-Ni alloy nanowires are deposited with 56.48:43.52 atomic ratios. We believe that at high potential the current density of Co nanowires is higher than depositing Ni nanowires which are clear by polarization curves, so content of Co increases in deposited Co 56.48 Ni 43.52 alloy nanowires. Single crystalline Co 56.48 Ni 43.52 alloys can be useful in future to compose and synthesize other metal nanostructures via template-based electrodeposition.

31 December 2016 in The Nucleus
Verified
Journal Article
Open access
PDF file
AMAiman Mukhtar
Aiman Mukhtar
TMT. Mehmood
T. Mehmood
The coexistence of both hcp and fcc phases for Co nanowires was studied in this work. Both hcp and fcc Co nanowires with diameter of ~ 50nm were successfully prepared by adjusting the deposition parameters. The systematic results show the effect of electrolytic cell with different cobalt sulfate concentration and different deposition temperatures with same pH and potential for the formation of (fcc and hcp) Co nanowires. The fabricated nanowires were characterized by X-ray diffraction, and the morphology of the electrodeposited nanowires was explored by scanning electron microscope.