The potential-pH diagram, a graphical representation of the thermodynamically predominant reaction products in aqueous corrosion, is originally proposed for the corrosion of pure metals. The original approach only leads to stoichiometric oxides and hydroxides as the oxidation products. However, numerous experiments show that non-stoichiometric oxide scales are prevalent in the aqueous corrosion of alloys. In the present study, a room temperature potential-pH diagram considering oxide solid solutions, as a generalization of the traditional potential-pH diagram with stoichiometric oxides, is constructed for an FCC single-phase multi-principal element alloy (MPEA) based on the CALculation of PHAse Diagram method. The predominant reaction products, the ions in aqueous solution, and the cation distribution in oxides are predicted. The oxide solid solution is stabilized by the mixing free energy (or mixing entropy) and the stabilizing effect becomes more significant as the temperature increases. Consequently, solid solution oxides are stable in large regions of the potential-pH diagram and the mixing free energy mostly affects the equilibrium composition of the stable oxides, while the shape of stable regions for oxides is mostly determined by the structure of the stable oxides. Agreements are found for Ni2+, Fe2+, and Mn2+ between the atomic emission spectroelectrochemistry measurements and thermodynamic calculations, while deviations exist for Cr3+ and Co2+ possibly due to surface complexation with species such as Cl− and the oxide dissolution. By incorporating the solution models of oxides, the current work presents a general and more accurate way to analyze the reaction products during aqueous corrosion of MPEAs.
21 November 2017 in Journal of the Electrochemical Society
The role of dealloying in the corrosion resistance of MgZn2 has been investigated for the first time. The elemental dissolution kinetics of a synthetic, nominally pure MgZn2 intermetallic compound was investigated and compared with pure Mg and Zn in 30 mM NaCl with pH = 10.1. Atomic emission spectroelectrochemistry was used to monitor Zn and Mg dissolution as a function of time at open circuit, during linear scan polarization, and at various applied potentials. Zn and Mg displayed a mutual inhibitive effect at open circuit which was explained by the formation of Mg depleted Zn / Zn oxide film. Polarization experiments revealed a Type II dealloying mechanism in which Zn and Mg dissolve simultaneously and congruently above the critical potential, Ec, while preferential Mg dissolution dominates below Ec. Preferential Mg dissolution leads to the formation of a Mg depleted metallic Zn layer which suppresses further Mg dissolution. In oxygen saturated electrolyte, O2 reduction was the major cathodic reaction on Zn but was completely inhibited on Mg. The intense cathodic reduction of O2 on Zn led to a cathodic dissolution of Zn, probably due to the increased interfacial pH.
1 November 2020 in Surface and Coatings Technology
The kinetics of passive oxide film formation, its thickening, and composition on Ni-22Cr and Ni-22Cr-6Mo wt% alloys were investigated at selected anodic potentials. Experiments were performed in acidic and alkaline sulfate environments using a number of characterization techniques including a combination of potentiodynamic polarization, on-line atomic emission spectro-electrochemistry (AESEC), in situ potentiostatic passive film growth, along with in situ neutron reflectometry (NR) and ex situ X-ray photoelectron spectroscopy (XPS). The roles of solution pH and Mo on the passivation behavior were discussed in terms of thermodynamic and kinetic factors governing passivation. The pH was found to have an impact on the relative chemical compositions of passive film of the Ni-22Cr alloy but not noticeably for the Ni-22Cr-6Mo alloy. Ni-rich films formed early during the passivation process while Cr(III) enrichment was observed at longer times, albeit less extensively than observed previously in Cl− solutions. The fraction of Cr(III) cations also increased with alloying of Mo at low and high pH demonstrating a strong effect of Mo on Cr(III) content during aqueous passivation in Ni based superalloys, however, a larger effect is seen in Cl−. This is a noteworthy finding as Mo is usually assumed to mainly influence pit and crevice stabilization.
1 May 2021 in Journal of the Electrochemical Society
The identity of passivating oxides on multi-principal element alloys is of great interest as their optimization offers the potential for exceptional corrosion resistance in aqueous solutions over a broad range of potential and pH. This study focuses on a non-equiatomic Ni38Fe20Cr22Mn10Co10solid solution alloy and tracks the fate of each alloying element during linear sweep voltammetry, low and intermediate potential holds in the passive potential domain as well as during open circuit relaxation after anodic polarization in slightly acidified Cl−solution. Ni dissolves at all potentials investigated in this work, Fe and Co are incorporated into oxides or hydroxides in low concentrations whilst Cr and Mn are enriched at passive potentials. At low passivating potentials, Mn(II) dissolves and is incorporated in minor amounts in oxides containing large concentrations of Cr(III). Considerable enrichment in Mn(II)-species occurs relative to Cr(III) in the oxide at 0.1 V vs SCE. Electrochemical impedance spectroscopy suggests the presence of layered oxides with marginal passivation at high Mn(II) levels. The formation of these oxides depends on a combination of thermodynamic and kinetic factors as well as the sequence of passivation.