The oxidation of chromium in air at 700 °C was investigated with a focus on point defect behavior and transport during oxide layer growth. A comprehensive set of characterization techniques targeted characteristics of chromium oxide microstructure and chemical composition analysis. TEM showed that the oxide was thicker with longer oxidation times and that, for the thicker oxides, voids formed at the metal/oxide interface. PAS revealed that the longer the oxidation time, there was an overall reduction in vacancy-type defects, though chromium monovacancies were not found in either case. EIS found that the longer oxidized material was more electrochemically stable and that, while all oxides displayed p-type character, the thicker oxide had an overall lower charge carrier density. Together, the results suggest anion oxygen interstitials and chromium vacancy cluster complexes drive transport in an oxidizing environment at this temperature, providing invaluable insight into the mechanisms that regulate corrosion.
1 February 2023 in Journal of the Electrochemical Society
The kinetics of passive oxide film formation, its thickening, and composition on Ni-22Cr and Ni-22Cr-6Mo wt% alloys were investigated at selected anodic potentials. Experiments were performed in acidic and alkaline sulfate environments using a number of characterization techniques including a combination of potentiodynamic polarization, on-line atomic emission spectro-electrochemistry (AESEC), in situ potentiostatic passive film growth, along with in situ neutron reflectometry (NR) and ex situ X-ray photoelectron spectroscopy (XPS). The roles of solution pH and Mo on the passivation behavior were discussed in terms of thermodynamic and kinetic factors governing passivation. The pH was found to have an impact on the relative chemical compositions of passive film of the Ni-22Cr alloy but not noticeably for the Ni-22Cr-6Mo alloy. Ni-rich films formed early during the passivation process while Cr(III) enrichment was observed at longer times, albeit less extensively than observed previously in Cl− solutions. The fraction of Cr(III) cations also increased with alloying of Mo at low and high pH demonstrating a strong effect of Mo on Cr(III) content during aqueous passivation in Ni based superalloys, however, a larger effect is seen in Cl−. This is a noteworthy finding as Mo is usually assumed to mainly influence pit and crevice stabilization.
The thermodynamic stability of chromium in the Cr0, Cr2+, and Cr3+ oxidation states considering various F− ion coordination compounds was investigated in molten LiF–NaF-KF (FLiNaK) eutectic salt. Potential fluoride ion activity (F− and CrF3−) diagrams were constructed to predict the most stable Cr oxidation states as a function of anion activity, solvation state of chromium ions and potential at 600 °C. The Gibbs free energies of these compounds were estimated by utilizing a combined cyclic voltammetry – Nernst theory analysis approach in FLiNaK salt. To verify the constructed diagrams, X-ray diffraction was utilized after exposure of Cr at various applied potentials to determine whether compounds detected in solidified FLiNaK salts agreed with thermodynamic calculations. This work aims to identify key thermodynamic factors that are significant to chromium corrosion for molten salt nuclear reactor applications. The F− stability region spans the entire region where spontaneous corrosion of Cr occurs. Cr may be oxidized to Cr2+ and Cr3+ in the presence HF (due to moisture as an impurity) spontaneously except some conditions of p1/2H2/aHF etc. This situation is not changed qualitatively for various states of solvation between oxidized Cr solute in F− solvent and this aspect is substantially similar for the two cases (pair 1: Cr0/CrF3−/ CrF63−; pair 2: Cr0/CrF42−/CrF52−) considered in this work.
The manuscript revisits the corrosion behavior of pure Cr in molten FLiNaK salt at 600 °C from the perspective of corrosion electrochemistry. In this work, the potential-dependent, rate-limiting charge-transfer, and salt film-mediated mass-transport controlled regimes of Cr corrosion in FLiNaK at 600 °C are investigated. The kinetic and thermodynamic parameters that limit electrodissolution and the consideration of grain orientation on these regimes are elucidated. At low Cr(III) concentrations, the corrosion process is governed by charge transfer control at low overpotentials and is crystal orientation dependent. However, when Cr(III) concentrations are high or when there is a high overpotential, the formation of a metal fluoride salt film on the Cr surface shifts the kinetic behavior to be governed by mass transport control at all anodic potentials with a surface morphology controlled by salt film deposition location and identity. Evan’s diagrams were developed to consolidate and elucidate these observations. These findings were supported by an examination of the post-corrosion microstructure, X-ray diffraction of solidified salts, and thermo-kinetics analysis in each corrosion regime.
1 August 2024 in Journal of the Electrochemical Society
The dealloying corrosion behavior of the FCC Ni20Cr (wt%) in molten LiF-NaF-KF (FLiNaK) salts at 600 °C under varying applied potentials was investigated. Using in-operando electrochemical techniques and a multi-modal suite of characterization methods, we connect electrochemical potential, thermodynamic stability, and electro-dissolution kinetics to the corrosion morphologies. Notably, under certain potential regimes, a micron-scale bicontinuous structure, characterized by a network of interconnected pores and ligaments riched with the composition of the more noble (MN) element, becomes prominent. At other potentials both MN and less noble (LN) elements dealloy but at different rates. The dealloying process consists of lattice and grain boundary diffusion of Cr to the metal/salt interface, interphase Cr oxidation, accompanied by surface diffusion of Ni to form interconnected ligaments. At higher potentials, the bicontinuous porous structure undergoes further surface coarsening. Concurrently, Cr(II), Cr(III), and Ni(II) begin to dissolve, with the dissolution of Ni occurring at a significantly slower rate. When solid-state transport of Cr is exceeded by the interfacial rates, dealloying depths are limited.