The major goal of this study is to enhance the mechanical and metallurgical characteristics of rail steel grade R260 joined by thermite welding under various preheating conditions, including preheating time and gas pressure. Mainly two conditions, referred to as the Normal Condition and Improved Condition, are carried out for experiments. Prior to welding, the Normal Condition was preheated using liquefied petroleum gas (LPG) and oxygen gas pressures of 1 bar and 4.5 bar for 3 min, and the Improved Condition was preheated using liquefied petroleum gas and oxygen gas pressures of 1.2 bar and 4.5 bar for 6 min and 30 s. To investigate the mechanical and physical properties, micro-Vickers hardness tests, tensile tests and slow bending tests were also carried out. Welded metal in Normal Condition has many defects, including gas holes and shrinkage cavities. When comparing the Normal Condition to the Improved Condition, the Improved Condition demonstrates significantly more bending load and deflection. Specifically, the thermite welded rail sample of Improved Condition demonstrated a remarkable ability to endure bending loads of 108 tonnes and a deflection of 16 mm, and this sample remained unbroken until it exceeded 50% of the standardized deflection limit (10 mm). In addition, the average hardness values for the Improved Condition of the weld metal zone and the heat-affected zone were 331 HV and 289 HV, respectively. The Normal Condition produced an unsatisfactory fracture surface after slow bending test. This was caused by weld defects at the thermite weld due to inappropriate preheating.
This research investigated the corrosion behavior of standard current metal inert gas weld repair for 6082-T6 aluminum alloy using ER5356 filler metal. The new and repaired (NW and RW) welds were studied. The welds comprised the weld metal (WM), the heat affected zone (HAZ) (solid solution and softened zones), and the base metal (BM). The study focused on investigating electrochemical corrosion using polarization and electrochemical impedance spectroscopy (EIS) methods in 3.5% NaCl solutions, especially in HAZ, including metallurgical and mechanical examinations. The BM containing an α-Al matrix with Al(Fe,Mn)Si and Mg2Si phases exhibited the maximum hardness (70–104 HV0.1). The WM hardness decreased (67–76 HV0.1) with the α-Al, β-Mg3Al2, and Mg2Si phases. Despite having comparable phases to BM, HAZs showed lower hardness (Solid HAZ: 70–82 HV0.1) due to more intermetallic phases. The RW’s softened HAZ revealed the minimum hardness (52–63 HV0.1) compared to that of the NW (55–70 HV0.1). Besides, the tensile strength of the RW (179.7 MPa) was also lower than that of the NW (174.4 MPa) because of the reheating effect. The electrochemical corrosion results indicated that the BM exhibited the maximum corrosion resistance (the lowest corrosion current density (icorr), the highest corrosion potential (Ecorr), and the charge transfer resistance (Rct)), followed by the HAZ and the WM, respectively. The softened HAZ demonstrated better corrosion resistance than the solid solution HAZ. Conversely, the over-aging effect reduced the softened zone’s pitting corrosion resistance (Ep) compared to the solid solution zone. The RW exhibited inferior corrosion resistance compared to the NW due to increased intermetallic phases, which was consistent with the mechanical results. However, the RW’s softened HAZ corrosion characteristics were inconsistent with its mechanical properties; its hardness and tensile strength were the lowest, but its corrosion resistance was not. Pitting corrosion was observed on the weld surfaces using the SEM.