In this work, we studied the evolution of vacancy-like defects and the formation of brittle precipitates in a reduced-activation V−Cr−Mn medium-entropy alloy. The evolution of local electronic circumstances around Cr and Mn enrichments, the vacancy defects, and the CrMn3 precipitates were characterized by using scanning electron microscopy with energy-dispersive spectroscopy, X-ray diffraction, and positron annihilation spectroscopy. The microstructure measurements showed that the Mn and Cr enrichments in the as-cast sample significantly evolved with temperature, i.e., from 400 °C, the Cr/Mn-segregated regions gradually dissolved into the matrix and then disappeared, and from 900 °C to 1000 °C, they existed as CrMn3 precipitates. The crystallite size of the phase corresponding to CrMn3 precipitates was about 29.4 nm at 900 °C and 43.7 nm at 1000 °C. The positron annihilation lifetime results demonstrated that the vacancies mediated the migration of Cr and Mn, and Cr and Mn segregation finally led to the formation of CrMn3 precipitates. The coincidence Doppler broadening results showed that the characteristic peak moved to the low-momentum direction, due to an increase in the size of the vacancy defects at the interface and the formation of CrMn3 precipitates.
1 April 2018 in International Journal of Electrochemical Science
Cyanide pollution refers to the environmental pollution caused by cyanide and its compounds. As a derivative of cyanide, the leakage and excessive discharge of hydrogen cyanide will cause great harm to the surrounding animal and plant environment. Rapid detection of hydrogen cyanide can avoid some unnecessary environmental pollution. Based on the principle of non dispersive infrared(NDIR) detection, the infrared absorption of hydrogen cyanide at 3.0 μm and 14.3 μm was selected as the qualitative and quantitative basis. Two NDIR sensors were designed to detect 3.0 μm and 14.3 μm infrared absorption respectively after assembly. The standard curve between the concentration of hydrogen cyanide and the voltage response value was determined, and the performance of the two sensors was tested. Their detection ranges is 10ppm-3000ppm and 22ppm-3000ppm respectively. The maximum response time is less than 11s and RSD < 2%. After comparing the performance of the two sensors, the display values of the different sensors were processed. Finally, the two sensors were assembled into one sensor, the hydrogen cyanide concentration was displayed with one indication and different gases were mixed with hydrogen cyanide to pass into the gas chamber, which improved the anti-interference ability.