Thermoplastic polyurethane (TPU) composites with eutectic gallium (Ga) and indium (In) (eGaIn) fillings of 0 wt%–75 wt% were prepared using the electrostatic spinning method. Field emission scanning electron microscopy (SEM), X-ray diffraction (XRD), and Fourier-transform infrared (FTIR) spectroscopy were used to characterize the eGaIn NDs/TPU composites. To evaluate their X-ray shielding properties, Phy-X/PSD and WinXCom were employed to calculate the mass attenuation coefficients, linear attenuation coefficients, half-value layers, tenth value layers, mean free paths, and adequate atomic numbers of the eGaIn NDs/TPU composites. The SEM results indicated that the eGaIn nanodroplets were evenly distributed throughout the TPU fibers, and the flowable eGaIn was well-suited for interfacial compatibility with the TPU. A comparison of the eGaIn NDs/TPU composites with different content levels showed that the composite with 75 wt% eGaIn had the highest μm at all the evaluated energies, indicating a superior ability to attenuate X-rays. This non-toxic, lightweight, and flexible composite is a potential material for shielding against medical diagnostic X-rays.
The preparation of binary alloys by surfactant-assisted chemical reduction in aqueous solution at room temperature has become a hot topic. In this article low melting point tin/indium (Sn/In) nanoparticles are synthesized. The formation process of the alloy was studied. Scanning electron microscopy, energy spectrometry, and X-ray diffraction are used to determine the morphology, composition, and crystal structure of the nanoparticles. Study found that fully alloyed indium-tin nanoparticles can be obtained by wet chemical method and the main phases of indium-tin alloy are β-phase (In3Sn) and γ-phase (InSn4). However, the Sn phase appears at a low content of indium (40 wt%). When the content of indium increases to 45 (wt%), the tin phase disappears. In addition, the most important finding is that the composition of the indium-tin alloy can be changed by ratio control, and the content of In3Sn increases with the increase of indium content. The relative content of In3Sn attains a maximum when the content of indium increases to 60 (wt%). In contrast, the content of InSn4 decreases. Finally, differential scanning calorimetry measurements is performed to understand the melting behavior of the nanoparticles and low melting temperatures are achieved for a wide range of indium compositions (from 40% to 60%). The melting temperature is found to be in the range of 125–132 °C and it increased with increasing In3Sn (also the increase of indium content). This gives us a new understanding into the binary alloy nano-system and gives important information for the application of low temperature alloy solders. The choice of composition can be based on the corresponding melting point.
A room-temperature liquid metal battery with a solid lithium anode electrode and gallium–tin (Ga–Sn) alloy cathode electrode is reported. The Li‖Ga–Sn battery has fast reaction kinetics, a satisfactory specific capacity, high energy efficiency, good rate performance, and stable cyclic reversibility, which is a promising choice for power grid energy storage applications. More details can be found in article number 2100330, Jin Hu, Kaijun Wang, and co-workers.