The effects of 0.1 wt.% Sc and 0.1 wt.% Zr addition in AA5182 on microstructure and mechanical properties were investigated. Results show that Al3(ScxZr1−x) dispersoids formed in AA5182. Observation of ingots microstructures showed that the grain size of 5182-Sc-Zr alloy was 56% lower than that of based AA5182. Isothermal annealing between 230 °C and 500 °C for 2 h was performed to study the recrystallization, tensile properties and dispersoid coarsening. The recrystallization was inhibited by the dispersoids, and the alloy microstructure remained deformed after annealing. Al3(ScxZr1−x) in AA5182 was stable when annealing below 400 °C, while parts of dispersoids coarsened significantly when heating at 500 °C. The addition of Sc and Zr allowed YS of 5182 alloy to achieve 247.8 MPa, which is 100 MPa higher than the corresponding AA5182. The contributions of Orowan strengthening and grain boundary strengthening were obtained by calculation.
Hot compression experiments were performed on alloy 5182 with small additions of Sc and Zr. The 5182 alloy containing Sc and Zr is critical for expanding the 5182 alloy’s range of applications, and a thorough understanding of its thermal processing behavior is of great importance to avoid processing defects. Alloy microstructure, including grain structures and Al3(ScxZr1−x) dispersoids were analyzed by EBSD and TEM. Stable flow stresses were observed below a strain rate of 1 s−1 for the Sc-Zr containing alloy. The results of constitutive models, with and without strain−compensation, and artificial neural network (ANN) were used to compare to the experimental results. The Al3(ScxZr1−x) dispersoid data was introduced into the ANN model as a nonlinear influence factor. Addition of the Al3(ScxZr1−x) dispersoid information as input data improved the accuracy and practicality of the artificial neural network in predicting the deformation behavior of the alloy. The squared correlation coefficients of ANN prediction data reached 0.99.