To satisfy the most stringent criteria in terms of new cardiovascular stents, pure Zn was alloyed with 1 wt pct of Mg and subsequently subjected to plastic deformation, using conventional hot extrusion followed by multi-pass hydrostatic extrusion. A detailed microstructural and textural characterization of the obtained materials was conducted, and mechanical properties were assessed at each pass of deformation process. In contrast to pure Zn, hydrostatically extruded low-alloyed Zn is characterized by a remarkable increase in strength and ductility (YS = 383 MPa, E = 23 pct), exceeding the values needed for stents. Such behavior is associated with a dual microstructure containing fine-grained Zn, alternatively arranged with bands of a fragmented eutectic. Extensive grain refinement was achieved due to the process of continuous dynamic recrystallization. Hydrostatic extrusion changes the initial $$ \langle 10\bar{1}0\rangle $$ fiber texture to a 〈0002〉 and $$ \langle 10\bar{1}1\rangle $$ double fiber texture in which the 〈0002〉 component decreases with each pass of hydrostatic extrusion. The gradual evolution of texture components was simulated using a visco-plastic self-consistent model, which confirmed that, during hydrostatic extrusion, secondary slip systems were activated involving mostly the pyramidal one.
The study is concerned with the mechanical properties of Zn and three Zn–Mg double alloys with Mg concentrations: 0.5%, 1.0% and 1.5% in the form of rods with a diameter of 5 mm as potential materials for use in biodegradable medical implants, such as vascular stents. The materials were cast, next conventionally hot extruded at 250 °C and finally, hydrostatically extruded (HE) at ambient temperature. Occasionally HE process was carried at liquid nitrogen temperature or in combination with the ECAP process. After HE, the microstructure of the alloys was made up of fine-grained αZn of mean grain size ~1 μm in a 2-phase coat of 50–200 nm nano-grains of the fine αZn + Mg2Zn11 eutectic. The 3 to 4-fold reduction of grain size as a result of HE allowed an increase in yield strength from 100% to over 200%, elongation to fracture from 100% to thirty fold and hardness over 50% compared to the best literature results for similar alloys. Exceptions accounted for elongation to fracture in case of Zn-0.5 Mg alloy and hardness in case of Zn-1.5 Mg alloy, both of which fell by 20%. For the Zn-0.5 Mg and Zn–1Mg alloys, after immersion tests, no corrosive degradation of plasticity was observed. Achieving these properties was the result of generating large plastic deformations at ambient temperature due to the application of high pressure forming with the cumulative HE method. The results showed that Zn–Mg binary alloys after HE have mechanical and corrosive characteristics, qualifying them for applications in biodegradable implants, including vascular stents.
The mechanical properties such as compressive strength and nanohardness were investigated for Pinctada margaritifera mollusk shells. The compressive strength was evaluated through a uniaxial static compression test performed along the load directions parallel and perpendicular to the shell axis, respectively, while the hardness and Young modulus were measured using nanoindentation. In order to observe the crack propagation, for the first time for such material, the in-situ X-ray microscopy (nano-XCT) imaging (together with 3D reconstruction based on the acquired images) during the indentation tests was performed. The results were compared with these obtained during the micro-indentation test done with the help of conventional Vickers indenter and subsequent scanning electron microscopy observations. The results revealed that the cracks formed during the indentation start to propagate in the calcite prism until they reach a ductile organic matrix where most of them are stopped. The obtained results confirm a strong anisotropy of both crack propagation and the mechanical strength caused by the formation of the prismatic structure in the outer layer of P. margaritifera shell.
High plasticity of bioabsorbable stents, either cardiac or ureteral, is of great importance in terms of implants’ fabrication and positioning. Zn-Cu constitutes a promising group of materials in terms of feasible deformation since the superplastic effect has been observed in them, yet its origin remains poorly understood. Therefore, it is crucial to inspect the microstructural evolution of processed material to gain an insight into the mechanisms leading to such an extraordinary property. Within the present study, cold-rolled Zn-Cu alloys, i.e., Zn with addition of 1 wt.% and 5 wt.% of Cu, have been extensively investigated using scanning electron microscopy as well as transmission electron microscopy, so as to find out the possible explanation of superior plasticity of the Zn-Cu alloys. It has been stated that the continuous dynamic recrystallization has a tremendous impact on superior plasticity reported for Zn-1Cu alloy processed by rolling to 90% of reduction rate. The effect might be supported by static recrystallization, provoking grain growth and thereby yielding non-homogeneous microstructures. Such heterogeneous microstructure enables better formability since it increases the mean free path for dislocation movement.
8 March 2024 in Journal of Materials Research and Technology