Iron oxides are considered promising electrode materials owing to their capability of lithium storage, but their poor conductivity and large volume expansion lead to unsatisfactory cycling stability. In this paper, an inexpensive, highly effective, and facile approach to the synthesis of Fe3O4 nanoparticles/reduced graphene oxide composite (Fe3O4/RGO) is designed. The synthesized Fe3O4/RGO composite exhibits high reversible capability and excellent cyclic capacity as an anode material in lithium-ion batteries (LIBs). A reversible capability of 701.8 mAh/g after 50 cycles at a current density of 200 mA·g−1 can be maintained. The synergetic effect of unique structure and high conductivity RGO promises a well soakage of electrolyte, high structure stability, leading to an excellent electrochemical performance. It is believed that the study will provide a feasible strategy to produce transition metal oxide/carbon composite electrodes with excellent electrochemical performance for LIBs.
In this study, we engineered a sub-70 nm nanocomposite of ZnO/Zn2TiO4 using a low-temperature solution-phase method with titanium isopropoxide and zinc acetate as precursors, and isopropyl alcohol and water as solvents. The investigation focused on nanocomposite growth by varying precursor and surfactant concentrations and their efficiency within different pH ranges. All three ZnO/Zn2TiO4 nanocomposites exhibited hexagonal wurtzite ZnO and Zn2TiO4 structures. The crystallite size in these nanocomposites ranged from 39.50 nm to 62.67 nm for ZnO and 21.24 nm to 26.15 nm for Zn2TiO4. Morphological observations using FESEM revealed the formation of dispersed cotton packet-like nanocomposites with sizes ranging from 18 to 350 nm. FTIR analysis showed peaks indicative of Ti–O and Zn–O bond formation, and EDX spectrum confirmed the presence of Ti, O, and Zn. UV spectrums and photocatalytic investigations confirmed the successful formation of ZnO/Zn2TiO4 nanocomposites with notable photocatalytic degradation efficiency for methylene blue dye under various conditions. These findings suggest the potential applicability of the synthesized nanocomposites for environmental pollutant degradation.
In the current research work, palladium (Pd) nanoparticles were electrochemically deposited on a nitrogen doped montmorillonite (CNx-MMT) support using the underpotential deposition (UPD) method. The prepared Pd based composite electrode was studied as an electrocatalyst for methanol fuel oxidation. The catalysts and the supporting materials montmorillonite, acid activated montmorillonite, and nitrogen doped montmorillonite (MMT, HMMT and CNx-HMMT) were characterized by Fourier transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), scanning electron microscopy (SEM), and energy dispersive X-ray spectroscopy (EDS) and electrochemical characterization by cyclic voltammetry (CV). The results indicated that Pd supported on CNx-HMMT possesses enhanced electrocatalytic activity and stability compared to commercial Pd/C, which was attributed to its higher electrochemical surface area (ECSA) (23.00 m2 g−1). The results demonstrated the potential application of novel Pd/CNx-HMMT composite nanomaterial as electrocatalysts for methanol electrooxidation in direct methanol fuel cells (DMFCs).
In this work, we report the engineering of a sub-70 nm nanocomposite of ZnO/Zn2TiO4 using a low-temperature solution-phase method. Titanium isopropoxide and zinc acetate were used as precursors, and isopropyl alcohol and water were used as solvents. The investigation focused on the growth of nanocomposites by varying the concentrations of precursors and surfactants, as well as their efficiency within different pH ranges. All three ZnO/Zn2TiO4 nanocomposites consist of hexagonal wurtzite ZnO and Zn2TiO4 structures in the three nanocomposites. The crystallite size in three ZnO/Zn2TiO4 nanocomposites, with a hexagonal wurtzite ZnO structure, were measured to be 62.67, 40.34, and 39.50 nm. The crystallite size values in three ZnO/Zn2TiO4 nanocomposites were 26.15 nm, 25.36 nm, and 21.24 nm, respectively, with Zn2TiO4. Morphological observations, conducted using FESEM, reveal the formation of three ZnO/Zn2TiO4 nanocomposites across the entire sample. These nanocomposites resemble dispersed cotton packets, with sizes ranging from 18 to 350 nm. Peaks in the range of 610-1250cm-1 are attributed to Ti-O bond formation and peak located at 1350-1450 cm-1 are attributed to Zn-O bond formation. Also, EDX spectrum reveals peaks for various sample components such as Ti, O and Zn. UV spectrums confirmed the formation of three nanocomposite of ZnO/Zn2TiO4 as showing two peaks for each sample. Photocatalytic investigation carried out by analyzing the UV-Visible absorption spectra of methylene blue dye on the surface of ZnO/Zn2TiO4 nanocomposites, dye degradation at various irradiation time intervals, dye degradation at varied catalyst concentrations and the influence of pH on dye-degradation. Furthermore, the said nanocomposites were used to degrade environmental pollutant (Methylene blue dye). Different sets of experiments were conducted under ambient conditions which show an excellent photo catalytic degradation efficiency.