CVCharlotte Vichery
Charlotte Vichery
Jean-Marie NedelecJean-Marie Nedelec
Jean-Marie Nedelec
Thanks to their high biocompatibility and bioactivity, bioactive glasses are very promising materials for soft and hard tissue repair and engineering. Because bioactivity and specific surface area intrinsically linked, the last decade has seen a focus on the development of highly porous and/or nano-sized materials. This review emphasizes the synthesis of bioactive glass nanoparticles and materials design strategies. The first part comprehensively covers mainly soft chemistry processes, which aim to obtain dispersible and monodispersed nanoparticles. The second part discusses the use of bioactive glass nanoparticles for medical applications, highlighting the design of materials. Mesoporous nanoparticles for drug delivery, injectable systems and scaffolds consisting of bioactive glass nanoparticles dispersed in a polymer, implant coatings and particle dispersions will be presented.

25 March 2019 in ACS Omega
Verified
Journal Article
Open access
XKXavier Kesse
Xavier Kesse
CVCharlotte Vichery
Charlotte Vichery
Jean-Marie NedelecJean-Marie Nedelec
Jean-Marie Nedelec
The aim of this study was to investigate the effect of three synthesis parameters on the morphology and composition of nanosized binary bioactive glass particles (nBGPs) obtained through a modified Stöber process. Syntheses were conducted by varying only one parameter at a time while keeping the other parameters constant. As already mentioned in the literature, the ammonium hydroxide volume conditioned the size of the nanoparticles. Nonagglomerated monodispersed spherical particles with a diameter between 70 and 452 nm were produced. The quantity of calcium nitrate and the moment it was introduced in the sol had a tremendous impact on the quantity of calcium inserted and on the particle morphology and aggregation state. High Ca-content particles were obtained when the calcium precursor addition time was 1 h or less after the beginning of the sol–gel reaction but at the cost of a strong aggregation. A better control on the morphology, polydispersity and dispersibility of the nBGPs was achieved when the Ca(NO3)2 addition time was increased up to 6 h. However, a significant decrease of the quantity of Ca2+ inserted was also noticed. Using an intermediate (3 h) addition time, the quantity of calcium nitrate has been optimized to maximize the insertion of Ca2+ ions inside the silica particles. Finally, an optimum initial Ca/Si atomic ratio of 2, maximizing Ca insertion while limiting the salt quantity used, was found. It led to the synthesis of particles with a molar composition of 0.9SiO2–0.1CaO without any side effect on the particle stability and morphological characteristics.

29 September 2020 in ACS Applied Materials & Interfaces
Verified
Journal Article
Closed access
XKXavier Kesse
Xavier Kesse
AAAlexandre Adam
Alexandre Adam
SBSylvie Bégin-Colin
Sylvie Bégin-Colin
DMDamien Mertz
Damien Mertz
ELEric Larquet
Eric Larquet
Jean-Marie NedelecJean-Marie Nedelec
Jean-Marie Nedelec

22 January 2020 in ACS Applied Bio Materials
Verified
Journal Article
Open access
XKXavier Kesse
Xavier Kesse
CVCharlotte Vichery
Charlotte Vichery
AJAurelie Jacobs
Aurelie Jacobs
SDStéphane Descamps
Stéphane Descamps
Jean-Marie NedelecJean-Marie Nedelec
Jean-Marie Nedelec
Sol-gel derived bioactive glass nanoparticles (BGNs) are fascinating materials for bone regeneration. In the literature, it can be found that their specific surface area and their calcium content (Ca/Si ratio) are the two key parameters impacting strongly the particles bioactivity. Nevertheless, in most studies, in vitro bioactivity tests are performed on series of materials where both the composition and the specific surface area are varied. It is thus difficult to unravel the effect of each parameter independently. In this study, spherical and monodispersed BGNs with different Ca/Si ratio and similar specific surface area have been synthesized by a modified Stöber method in order to specify the impact of the calcium content only. The mineralization studies performed in simulated body fluid showed that the bioactivity increases with the amount of calcium incorporated in the glass matrix. However, this effect is not significant in the composition interval studied (7-15 %mol of CaO). Such a result proves that the effective Ca/Si ratio is not the major parameter which affects the bioactivity of sol-gel binary BGs. In vitro biocompatibility assessment during 3 and 7 days using human Mesenchymal Stem Cells in contact with the sample showing the fastest mineralization proved its non-cytotoxicity. Hence, biomedical applications can be intended for this sample.

15 June 2022 in Biomaterials Science
Verified
Journal Article
Closed access
PDF file
FVFlorestan Vergnaud
Florestan Vergnaud
XKXavier Kesse
Xavier Kesse
AJAurélie Jacobs
Aurélie Jacobs
FPFrancis Perton
Francis Perton
SBSylvie Bégin-Colin
Sylvie Bégin-Colin
Jean-Marie NedelecJean-Marie Nedelec
Jean-Marie Nedelec
γ-Fe2O3@SiO2–CaO NPs were designed. They show predicable and effective magnetic hyperthermia properties in clinically relevant conditions and promote hydroxyapatite growth in SBF. They could be used to heal bone defects due to tumor resection.

14 October 2023 in Materials
Verified
Journal Article
Open access
PDF file
FVFlorestan Vergnaud
Florestan Vergnaud
BMBenhur Mekonnen
Benhur Mekonnen
AAAbdelouahad El Abbassi
Abdelouahad El Abbassi
CVCharlotte Vichery
Charlotte Vichery
Jean-Marie NedelecJean-Marie Nedelec
Jean-Marie Nedelec
Multifunctional substitutes for bone tissue engineering have gained significant interest in recent years in the aim to address the clinical challenge of treating large bone defects resulting from surgical procedures. Sol–gel mesoporous bioactive glass nanoparticles (MBGNs) have emerged as a promising solution due to their high reactivity and versatility. The effect of calcium content on MBGNs textural properties is well known. However, the relationship between their composition, textural properties, and reactivity has not yet been thoroughly discussed in existing studies, leading to divergent conclusions. In this study, pristine and copper-doped binary MGBNs were synthesized by a modified Stöber method, using a cationic surfactant as pore-templating agent. An opposite evolution between calcium content (12–26 wt%) and specific surface area (909–208 m2/g) was evidenced, while copper introduction (8.8 wt%) did not strongly affect the textural properties. In vitro bioactivity assessments conducted in simulated body fluid (SBF) revealed that the kinetics of hydroxyapatite (HAp) crystallization are mainly influenced by the specific surface area, while the composition primarily controls the quantity of calcium phosphate produced. The MBGNs exhibited a good bioactivity within 3 h, while Cu-MBGNs showed HAp crystallization after 48 h, along with a controlled copper release (up to 84 ppm at a concentration of 1 mg/mL). This comprehensive understanding of the interplay between composition, textural properties, and bioactivity, offers insights for the design of tailored MBGNs for bone tissue regeneration with additional biological and antibacterial effects.