Jan Štefan

Dr. Jan Štefan

orcid

Research Focus & Metrics

Academic Career Length

13Years (2014-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 September 2019 in Results in Physics
Verified
Journal Article
Open access
MŠMartin Ševčík
Martin Ševčík
JZJan Zídek
Jan Zídek
JNJitka Nejezchlebová
Jitka Nejezchlebová
JŠJan Štefan
Jan Štefan
AMAnna Machová
Anna Machová
PLPavel Lejček
Pavel Lejček

19 August 2021 in Applied Sciences
Verified
Journal Article
Open access
PDF file
JŠJan Štefan
Jan Štefan
SPSlavomír Parma
Slavomír Parma
RMRené Marek
René Marek
JPJiří Plešek
Jiří Plešek
CCConstantin Ciocanel
Constantin Ciocanel
HFHeidi Feigenbaum
Heidi Feigenbaum
This paper develops an experimental technique to evaluate the initial yield surfaces of metallic materials, as well as to study their evolution during plastic flow. The experimental tracing of yield surfaces is necessary for deriving and calibrating more robust phenomenological models of directional distortional hardening. Such models can be used to characterize the behavior of structures experiencing complicated and demanding loading modes, such as multiaxial ratcheting. The experimental technique developed in this work uses thin-walled tubular specimens, along with a servo-hydraulic machine, under various modes of tension/compression and torque. Identification of the onset of plastic flow is based on a small proof equivalent plastic strain evaluated from the outputs of a contact biaxial extensometer firmly attached to a specimen surface. This allows for evaluation of both the initial yield surface, as well as theevolved yield surface after a plastic prestrain. Throughout a test, continuous and fully automatized evaluation of elastic moduli and proof plastic strain is assured through algorithms written in C# language. The current technique is shown to provide promising results to effectively capture the yield surfaces of conventional metallic materials.

1 January 2014 in Procedia Materials Science
Verified
Journal Article
Open access
JŠJan Štefan
Jan Štefan
JSJan Siegl
Jan Siegl
MKMiloš Kytka
Miloš Kytka
The Reactor pressure vessel is a main component of a nuclear power plant's primary circuit. WWER 440 is one of the most widely used nuclear reactors of the second generation. The main structural material of the WWER 440 is the base metal, ferritic steel 15Kh2MFA. For the purpose of anti-corrosive protection, the pressure vessels’ inner surface is covered with austenitic cladding. The cladding is made from the stainless steels Sv 07Kh25N13 (first layer) and Sv 08Kh19N10G2B (second layer). In frame of pressure vessel materials properties surveillance, fractographic analysis was performed on specimens (both in the neutron-irradiated and non-irradiated state) subjected to static fracture toughness testing. Specimens were collected from the area of the interfaces of the base metal and the austenitic cladding layers. Detailed fractographic analysis of fractured specimens was undertaken. Based on fractographic findings, individual failure micromechanisms taking place during the crack propagation across the materials’ interfaces were determined and described. The obtained results were used to find the relationship between the failure micromechanism changes and fracture toughness values. The fractographic analysis also offered information about the influence of the neutron irradiation on the failure micromechanisms

10 August 2022 in Journal of Applied Physics
Verified
Journal Article
Closed access
PDF file
AUAlena Uhnáková
Alena Uhnáková
AMAnna Machova
Anna Machova
MJMichaela Janovska
Michaela Janovska
MŠMartin Ševčík
Martin Ševčík
JŠJan Štefan
Jan Štefan
PLPavel Lejček
Pavel Lejček
This paper is devoted to an experimental and 3D atomistic study of the influence of loading rate on fracture toughness in dilute Fe–Si alloys and in bcc iron. We analyze new and previous experimental results from fracture tests performed at room temperature on bcc iron–silicon single crystals with edge cracks (1¯10) [110] (crack plane/crack front). The specimens of single edge notch-type were loaded in tension mode I under different loading rates. The ductile–brittle behavior at the crack front was monitored online via optical microscopy together with external force and prolongation of the specimens. About 30% decrease in fracture toughness was monitored in the new experiment under the highest loading rate. The nanoscopic processes produced by the crack itself were studied at room temperature via 3D molecular dynamics (MD) simulations in bcc iron under equivalent boundary conditions as in experiments to reveal (explain) the sensitivity of the crack to loading rate. For this purpose, this MD study utilizes the self-similar character of linear fracture mechanics. The results show that the emission of blunting dislocations from the crack is the most difficult under the highest loading rate, which leads to the reduced fracture toughness of the atomistic sample. This is in a qualitative agreement with the experimental (macro) results. Moreover, MD indicates that there may be some synergetic (resonant) effect between the loading rate and thermal activation that promotes dislocation emission.

20 October 2021 in Metals
Verified
Journal Article
Open access
PDF file
JŠJan Štefan
Jan Štefan
JSJan Siegl
Jan Siegl
JAJan Adámek
Jan Adámek
RKRadim Kopřiva
Radim Kopřiva
MFMichal Falcník
Michal Falcník
This paper is dedicated to an experimental program focused on the evaluation of microstructure and failure mechanisms of WWER 440 type nuclear reactor pressure vessel cladding made from Sv 08Kh19N10G2B stainless steel. Static fracture toughness tests performed on standard precracked single edge bend specimens revealed extreme variations in fracture toughness values, J0.2. Fractured halves of test specimens were subject to detailed fractographic and metallographic analyses in order to identify the causes of this behavior and to determine the relationship between local microstructure, failure mode and fracture toughness. Results indicated that fracture toughness of the cladding was adversely affected by the brittle cracking of sigma particles which caused a considerable decrease in local ductile tearing resistance. Extreme variations in relative amounts of sigma phase, as well as the extreme overall structural heterogeneity of the cladding determined in individual specimens, provided a reasonable explanation for variations in fracture toughness values.

1 January 2022
Verified
Conference Paper
Open access
JSJ. Svárovský
J. Svárovský
SPS. Parma
S. Parma
JŠJan Štefan
Jan Štefan
CCC. Ciocanel
C. Ciocanel
HFH. P. Feigenbaum
H. P. Feigenbaum
JPJ. Plešek
J. Plešek