High-temperature reduction pretreatment (HTRP) is a process that can significantly improve the core quality of a billet. The existing flow stress data cannot meet the needs of simulation due to lack of high temperature data. To obtain the hot forming process parameters for the high-temperature reduction pretreatment process of 42CrMo steel, a hot compression experiment of 42CrMo steel was conducted on Gleeble-3500 thermal-mechanical at 1200–1350 °C with the rates of deformation 0.001–10 s−1 and the deformation of 60%, and its deformation behavior at elevated temperature was studied. In this study, the effects of flow stress temperature and strain rate on austenite grain were investigated. Moreover, two typical constitutive models were employed to describe the flow stress, namely the Arrhenius constitutive model of strain compensation and back propagation artificial neural network (BP ANN) model. The performance evaluation shows that BP ANN model has high accuracy and stability to predict the curve. The thermal processing maps under strains of 0.1, 0.2, 0.3, and 0.4 were established. Based on the analysis of the thermal processing map, the optimal high reduction process parameter range of 42CrMo is obtained: the temperature range is 1250–1350 °C, and the strain rate range is 0.01–1 s−1.
Controlling the segregation of alloying elements in steel can improve the uniformity of the structure and properties of the material. High Temperature Reduction Pretreatment (HTRP) is an effective technique to improve the internal quality of steel by generating plastic deformation in the core and providing the recrystallization energy. Comparative analysis was conducted to illustrate the effect of the HTRP on the internal quality of 42CrMo cast billets. To quantitatively analyze the recrystallization and diffusion mechanisms, the tested samples were measured using Scanning Electron Microscopy (SEM), Original Position Statistic Distribution Analysis (OPA) and Electron Probe Microanalysis (EPMA). The results show that the plastic deformation prompts the austenite to recrystallize. As the deformation of the HTRP sample increases, the recrystallized austenite grain size decreases significantly. It is also found that the statistical macro-segregation and micro-segregation ratios of substitutional elements Si, Mn, Cr and Mo decrease. The increase in austenite grain boundaries enables the increase in diffusion coefficient of the solid solution elements, which is the main reason for improving the segregation of the cast billet.
19 November 2020 in Journal of Iron and Steel Research International
The reduction pretreatment (RP) process is an effective method to improve billet quality, and the deformation recrystallization plays an important role in the process. Exploring the RP process parameters, a dynamic recrystallization model of GCr15 steel was established by the phase-field method and physical simulation. The recrystallization kinetics and flow stress curves during hot compression were simulated by using this mode. The effects of deformation parameters and initial grain size on the dynamic recrystallization were investigated. Moreover, by using the results obtained by Finite element method (FEM), dynamic recrystallization during the RP process was investigated though this model. It was found that increasing the deformation temperature, deformation rate and decreasing the initial grain size can promote the dynamic recrystallization kinetics. Large Zener-Hollomon parameters can enhance recrystallized grain refinement, while the recrystallized grain size was not affected by the initial grain size. During the RP process, when the reduction is insufficient (10%), partial recrystallization occurs in the billet. With the increase of reduction from 10% to 16%, the area of complete recrystallization increases gradually. When the reduction is the same, the recrystallization in the billet center increases with the decrease of casting speed. When the reduction is 10%, partial recrystallization occurs in the billet center at a casting speed of 0.7 m min−1, and fully recrystallization occurs in the billet center with a casting speed of 0.5 m min−1. Thus, when the reduction is difficult to increase further, the recrystallization in the billet center can be improved by decreasing the casting speed.
18 October 2024 in Metallurgical and Materials Transactions B
Owing to stringent service conditions, nickel-based superalloys must meet exceptionally high surface quality standards. After cold rolling, these alloys can blacken during annealing, affecting appearance and performance. The surface-element distribution of GH4169 alloy annealed under hydrogen protection was analyzed via XPS, and reaction free-energy changes were calculated using thermodynamic software. The blackened surface contained oxides and carbides, primarily Cr2O3, Cr(OH)3, TiO2, Nb2O5, NbC, and free carbon. Residual water vapor in the protective hydrogen gas and rolling-oil remnants generated C, CO2, CO, and H2O, which then reacted with the alloy during high-temperature annealing to form a blackened layer. The selective oxidation of Cr, Nb, and Ti, along with the inward diffusion of carbon, leads to the compositional differences observed in the blackened layer. Lowering the protective gas dew point, improving rolling oil, and effective degreasing eliminated blackening.