Archana Sinha

Ms. Archana Sinha


Research Focus & Metrics

Academic Career Length

14Years (2013-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
7 July 2022 in Progress in Photovoltaics: Research and Applications
Verified
Journal Article
Open access
ASArchana Sinha
Archana Sinha
JQJiadong Qian
Jiadong Qian
SMStephanie L. Moffitt
Stephanie L. Moffitt
KHKatherine Hurst
Katherine Hurst
KTKent Terwilliger
Kent Terwilliger
PHPeter Hacke
Peter Hacke
Degradation from ultraviolet (UV) radiation has become prevalent in the front of solar cells due to the introduction of UV‐transmitting encapsulants in photovoltaic (PV) module construction. Here, we examine UV‐induced degradation (UVID) in various commercial, unencapsulated crystalline silicon cell technologies, including bifacial silicon heterojunction (HJ), interdigitated back contact (IBC), passivated emitter and rear contact (PERC), and passivated emitter rear totally diffused (PERT) solar cells. We performed UV exposure tests using UVA‐340 fluorescent lamps at 1.24 W·m−2 (at 340 nm) and 45°C through 4.02 MJ·m−2 (2000 h). Our results showed that modern cell architectures are more vulnerable to UVID, leading to a significant power decrease (−3.6% on average; −11.8% maximum) compared with the conventional aluminum back surface field (Al‐BSF) cells (<−1% on average). The power degradation is largely caused by the decrease in short‐circuit current and open‐circuit voltage. A greater power decrease is observed in bifacial cells with rear‐side exposure compared with those with front‐side exposure, indicating that the rear side is more susceptible to UV damage. Secondary ion mass spectroscopy (SIMS) confirmed an increase in hydrogen concentration near the Si/passivation interface in HJ and IBC cells after UV exposure; the excess of hydrogen could result in hydrogen‐induced degradation and subsequently cause higher recombination losses. Additionally, surface oxidation and hot‐carrier damage were identified in PERT cells. Using a spectral‐based analysis, we obtained an acceleration factor of 5× between unpackaged cells (containing a silicon nitride antireflective coating on the front) in the UV test and an encapsulated module (with the front glass and encapsulant blocking 90% of the UV at 294 nm and 353 nm, respectively) in outdoor conditions. From the analytical calculations, we show that a UV‐blocking encapsulant can reduce UV transmission in the module by an additional factor of ~50.

1 October 2016 in Solar Energy Materials and Solar Cells
Verified
Journal Article
Closed access
ASArchana Sinha
Archana Sinha
OSO.S. Sastry
O.S. Sastry
RGRajesh Gupta
Rajesh Gupta

3 August 2021 in Journal of Physics D: Applied Physics
Verified
Journal Article
Closed access
ASArchana Sinha
Archana Sinha
DSDana B Sulas-Kern
Dana B Sulas-Kern
MOMichael Owen-Bellini
Michael Owen-Bellini
LSLaura Spinella
Laura Spinella
SUSona Ulicna
Sona Ulicna
LSLaura T Schelhas
Laura T Schelhas
Glass/glass (G/G) photovoltaic (PV) module construction is quickly rising in popularity due to increased demand for bifacial PV modules, with additional applications for thin-film and building-integrated PV technologies. G/G modules are expected to withstand harsh environmental conditions and extend the installed module lifespan to greater than 30 years compared to conventional glass/backsheet (G/B) modules. With the rapid growth of G/G deployment, understanding the outdoor performance, degradation, and reliability of this PV module construction becomes highly valuable. In this review, we present the history of G/G modules that have existed in the field for the past 20 years, their subsequent reliability issues under different climates, and methods for accelerated testing and characterization of both cells and packaging materials. We highlight some general trends of G/G modules, such as greater degradation when using poly(ethylene-co-vinyl acetate) encapsulants, causing the industry to move toward polyolefin-based encapsulants. Transparent backsheets have also been introduced as an alternative to the rear glass for decreasing the module weight and aiding the effusion of trapped gaseous degradation products in the laminate. New amendments to IEC 61215 standard protocols for G/G bifacial modules have also been proposed so that the rear side power generation and UV exposure will be standardized. We further summarize a suite of destructive and non-destructive characterization techniques, such as current–voltage scans, module electro-optical imaging, adhesion tests, nanoscale structural/chemical investigation, and forensic analysis, to provide deeper insights into the fundamental properties of the module materials degradation and how it can be monitored in the G/G construction. This will set the groundwork for future research and product development.

14 May 2020 in IEEE Journal of Photovoltaics
Verified
Journal Article
Closed access
ASArchana Sinha
Archana Sinha
HGHamsini Gopalakrishna
Hamsini Gopalakrishna
ASArun Bala Subramaniyan
Arun Bala Subramaniyan
DJDeepak Jain
Deepak Jain
JOJaewon Oh
Jaewon Oh
GTGovindaSamy TamizhMani
GovindaSamy TamizhMani
Encapsulant discoloration is a well-known field degradation mode of crystalline-silicon photovoltaic modules, particularly in the hot climate zones. The discoloration rate is influenced by several weathering factors, such as UV light, module temperature, and humidity, as well as the permeability of oxygen into the module. In this article, a rate dependence model employing the modified Arrhenius equations to predict the degradation rate for encapsulant discoloration in different climates is presented. Two modeling approaches are introduced, which utilize the field and accelerated UV testing degradation data in conjunction with the field meteorological data to determine the acceleration factor for encapsulant browning. A novel method of accelerated UV stress testing at three simultaneous module temperatures in a single environmental chamber test run is implemented to estimate the activation energy for browning. The test was performed on three field-retrieved modules to capture the wear-out failure mechanism. The degradation in short-circuit current Isc rather than maximum power is used as a decisive parameter for the discoloration analysis. Furthermore, the developed model has been used to predict the Isc degradation rate for the Arizona field characterized by a hot and dry climate and is validated against the field-measured value. It has also been applied to other climate types, e.g., the cold and dry climate of New York.

1 January 2021 in Solar Energy Materials and Solar Cells
Verified
Journal Article
Closed access
JNJimmy M. Newkirk
Jimmy M. Newkirk
INIllya Nayshevsky
Illya Nayshevsky
ASArchana Sinha
Archana Sinha
ALAdam M. Law
Adam M. Law
QXQianFeng Xu
QianFeng Xu
DMDavid C. Miller
David C. Miller

29 June 2022 in Progress in Photovoltaics: Research and Applications
Verified
Journal Article
Open access
LSLaura Spinella
Laura Spinella
SUSona Ulicna
Sona Ulicna
ASArchana Sinha
Archana Sinha
DSDana B. Sulas‐Kern
Dana B. Sulas‐Kern
MOMichael Owen‐Bellini
Michael Owen‐Bellini
LSLaura T. Schelhas
Laura T. Schelhas
Glass/glass (G/G) photovoltaic modules are quickly rising in popularity, but the durability of modern G/G packaging has not yet been established. In this work, we examine the interfacial degradation modes in G/G and glass/transparent backsheet modules under damp heat (DH) with and without system bias voltage, comparing emerging polyolefin elastomer (POE) and industry‐standard poly(ethylene‐co‐vinyl acetate) (EVA) encapsulants. We investigate the transport of ionic species at cell/encapsulant interfaces, demonstrating that POE limits both sodium and silver ion migration compared with EVA. Changes to the chemical structures of the encapsulants at the cell/encapsulant interfaces demonstrate that both POE and EVA are more susceptible to degradation in modules with a transparent backsheet than in the G/G configuration. Adhesion testing reveals that POE and EVA have comparable critical debond energies after the DH exposures regardless of system bias polarity. The results of this study indicate that the interfacial degradation mechanisms of G/G appear to be similar to those of conventional glass/backsheet modules. For emerging materials, our results demonstrate that POE offers advantages over EVA but that transparent backsheets may accelerate encapsulant degradation due to increased moisture ingress when compared with the G/G structure.