4 November 2019 in Nature Nanotechnology
14 May 2020 in IEEE Journal of Photovoltaics
Encapsulant discoloration is a well-known field degradation mode of crystalline-silicon photovoltaic modules, particularly in the hot climate zones. The discoloration rate is influenced by several weathering factors, such as UV light, module temperature, and humidity, as well as the permeability of oxygen into the module. In this article, a rate dependence model employing the modified Arrhenius equations to predict the degradation rate for encapsulant discoloration in different climates is presented. Two modeling approaches are introduced, which utilize the field and accelerated UV testing degradation data in conjunction with the field meteorological data to determine the acceleration factor for encapsulant browning. A novel method of accelerated UV stress testing at three simultaneous module temperatures in a single environmental chamber test run is implemented to estimate the activation energy for browning. The test was performed on three field-retrieved modules to capture the wear-out failure mechanism. The degradation in short-circuit current Isc rather than maximum power is used as a decisive parameter for the discoloration analysis. Furthermore, the developed model has been used to predict the Isc degradation rate for the Arizona field characterized by a hot and dry climate and is validated against the field-measured value. It has also been applied to other climate types, e.g., the cold and dry climate of New York.
5 October 2020 in IEEE Journal of Photovoltaics
The longevity of solar photovoltaic modules depends on the durability and reliability of their components, one of which is the solder bonds in interconnect ribbons. The solder joints experience stresses from thermal cycling and constant elevated temperatures (40 °C–70 °C) in regular field operation leading to thermo-mechanical fatigue and intermetallic compound formation. To study the end-of-life wear-out mechanisms and to obtain activation energy of solder bond degradation, two field-aged modules from Arizona—a 21-year-old Solarex MSX60 module (with Sn62Pb36Ag2 at the solder joints) and an 18-year-old Siemens M55 module (with Sn60Pb40 at the solder joints)—underwent 800 and 400 modified thermal cycles, respectively. Using three heating blankets, each module had three temperature zones maintained at 85, 95, and 105 °C during the 15-min hot dwell time of the thermal cycle. Cell-level series resistance data obtained from three temperature zones enabled the calculation of activation energy for solder bond degradation for the MSX60 and the M55 modules to be 0.12 eV and 0.35 eV, respectively. From each temperature zone in both modules, busbar-solder samples were obtained, imaged through SEM, and analyzed with energy-dispersive X-ray spectroscopy. In the MSX60 module with traces of Ag in the solder material, phase segregation and growth were primarily observed at high temperatures. For M55 modules without Ag in the solder material, major phase segregation was observed in all temperature zones. The IMC thickness for both modules increased with increasing module temperature. The beneficial effect of Ag in solder material on mitigating solder bond degradation is presented.
1 November 2019 in IEEE Journal of Photovoltaics