This paper addresses the effect of Mn (2%, fixed) and Co (2, 4, and 6%, varied) substitution on the structural, optical, dielectric and magnetic responses of ZnO nanoparticles synthesized by the co-precipitation chemical route. The X-ray diffraction analysis confirms the hexagonal wurtzite structure of ZnO. The incorporation of co-doping in the ZnO host, indicated by peak shifting in the XRD patterns, enhanced the crystallite size of the Mn/Co dual-doped ZnO nanoparticles. The FTIR spectra show a characteristic peak around 875 cm−1 assigned to Zn–O stretching, this validates the formation of the wurtzite structure of ZnO. Raman spectroscopy reveals the characteristic band of the wurtzite structure of ZnO nanoparticles along with coupled vibration modes of Mn/Co with the donor defect states in the doped samples. Enhanced optical absorption in the visible region and a significant red-shift in the absorption band edge were found due to doping. The optical band gap is found to decrease from 3.45 eV to 3.15 eV when Co doping increases up to 6%. The dielectric properties, strongly frequency-dependent, decrease with increasing Co doping while the electrical conductivity increases. Ferromagnetism is observed in all the doped samples, and its origin is attributed to an increase in oxygen vacancies which form bound magnetic polarons. It can be inferred that the doping of Mn and Co can be an effective tool to tune the physical properties of ZnO nanoparticles for potential spintronics and high-frequency applications.
In this study, phytochemical assisted nanoparticle synthesis was performed using Muntingia calabura leaf extracts to produce copper oxide nanoparticles (CuO NPs) with interesting morphology. Scanning electron microscope (SEM) and transmission electron microscope (TEM) analysis of the biosynthesized CuO NPs reveal formation of distinct, homogeneous, and uniform sized CuO nanorods structure with thickness and length of around 23 nm and 79 nm, respectively. Based on Fourier-transform infrared (FTIR) analysis, the unique combinations of secondary metabolites such as flavonoid and polyphenols in the plant extract are deduced to be effective capping agents to produce nanoparticles with unique morphologies similar to conventional chemical synthesis. X-ray diffraction (XRD) analysis verified the monoclinical, crystalline structure of the CuO NPs. The phase purity and chemical identity of the product was consolidated via X-Ray photoelectron spectroscopy (XPS) and Raman spectroscopic data which indicate the formation of a single phase CuO without the presence of other impurities. The direct and indirect optical band gap energies of the CuO nanorods were recorded to be 3.65 eV and 1.42 eV.
Electronic devices featuring biomimetic behaviour as electronic synapses and neurons have motivated the emergence of a new era in information and humanoid robotics technologies. In the human body, a nociceptor is a unique sensory neuron receptor that is capable of detecting harmful signals, leading to the central nervous system initiating a motor response. Herein, a nickel-doped zinc oxide (NZO)/Au based memristor is fabricated for the first time and characterized for artificial nociceptor application. For this, the introduction of a nickel-doped zinc oxide (NZO) layer between P++-Si and Au electrodes is used to eliminate the surface effects of the NZO layer, resulting in improved volatile threshold switching performance. Depending on the intensity, duration, and repetition rate of the external stimuli, this newly created memristor exhibits various critical nociceptive functions, including threshold, relaxation, allodynia, and hyperalgesia. The electron trapping/detrapping to/from the traps in the NZO layer is responsible for these nociceptive properties. This kind of NZO-based device produces a multifunctional nociceptor performance that is essential for applications in artificial intelligence systems, such as neural integrated devices with nanometer-sized features.
The structure parameters of the synthesize ZnO, Zn 0.96 Gd 0.04 O and Zn
0.96−
x Gd 0.04 Co x O (Co = 0, 0.01, 0.03, 0.04) diluted magnetic semiconductor nanotubes.
5 September 2021 in Journal of Materials Science: Materials in Electronics