Igor Igor Barényi

Dr. Igor Igor Barényi


Research Focus & Metrics

Academic Career Length

13Years (2014-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
6 June 2020 in Metals
Verified
Journal Article
Open access
PDF file
MKMichal Krbaťa
Michal Krbaťa
MEMaros Eckert
Maros Eckert
JMJozef Majerik
Jozef Majerik
IBIgor Igor Barényi
Igor Igor Barényi
Tool steels are used in technological processes of forming and cutting and as cutting tools due to their good mechanical properties. During their working cycle, steels are exposed to several aggressive conditions, such as thermal stress, fatigue and various forms of wear. In this article, the selected 90MnCrV8 tool steel slid against the Si3N4 testing ceramic bearing ball. All measurements were performed on a universal tribometric device UMT TriboLab (TA Instruments, New Castle, Delaware, USA) under dry conditions. The main objective of the performed experiments was to analyse the frictional properties and compare the wear of the 90MnCrV8 tested tool steel in contact with the 6.35 mm diameter ceramic ball at different friction speeds. In this measurement evaluation, the authors of the article mainly focused on the influence of the magnitude of the peripheral speed on the wear change and coefficient of friction. Further analysis was focused on the change of surface roughness of the counterpart ceramic balls as well as of the tested tool steel samples. Experimental results show the fact that tested tool steels, which can also be considered as high strength steels, can also successfully represent wear-resistant steels. It has been shown experimentally that increasing the friction speed also leads to significant degradation of the material on the sample surface. Finally, the effect of hardness on wear has also been experimentally demonstrated. The Si3N4 ceramic ball with its high strength also behaves like an abrasive, thus increasing the wear rate on the experimental tool steel samples.

20 January 2023 in Materials
Verified
Journal Article
Open access
PDF file
SKStepan Kolomy
Stepan Kolomy
JSJosef Sedlak
Josef Sedlak
JZJan Zouhar
Jan Zouhar
MSMartin Slaný
Martin Slaný
MBMarek Benč
Marek Benč
JMJozef Majerik
Jozef Majerik
This paper deals with the study of high-strength M300 maraging steel produced using the selective laser melting method. Heat treatment consists of solution annealing and subsequent aging; the influence of the selected aging temperatures on the final mechanical properties—microhardness and compressive yield strength—and the structure of the maraging steel are described in detail. The microstructure of the samples is examined using optical and electron microscopy. The compressive test results show that the compressive yield strength increased after heat treatment up to a treatment temperature of 480 °C and then gradually decreased. The sample aged at 480 °C also exhibited the highest observed microhardness of 562 HV. The structure of this sample changed from the original melt pools to a relatively fine-grained structure with a high fraction of high-angle grain boundaries (72%).

20 May 2020 in Materials
Verified
Journal Article
Open access
PDF file
MKMichal Krbaťa
Michal Krbaťa
MEMaros Eckert
Maros Eckert
LBLenka Bartosova
Lenka Bartosova
IBIgor Igor Barényi
Igor Igor Barényi
JMJozef Majerik
Jozef Majerik
PRPetra Rendkova
Petra Rendkova
Tool steels are used in stamping, shearing processes, and as cutting tools due to their good mechanical properties. During their working cycle, steels are subject to aggressive conditions such as heat stress, fatigue, and wear. In this paper, three tool steels, namely X153CrMoV12, X37CrMoV5-1, and X45NiCrMo4 were selected against two types of bearing balls, ZrO2 and X46Cr1. All measurements were performed on a UMT TriboLab universal tribometric instrument under dry conditions. The main objective of the experiment was to analyze and compare tool steel wear in contact with two kinds of bearing balls with a diameter of 4.76 mm. This evaluation is focused on the hardness, surface roughness, and microstructure of all samples and on the impact of the input parameters on the resulting wear. All three types of tool steels were measured in the basic annealed state and, subsequently, in the state after hardening and tempering. Experimental results show that tool steels, belonging to high strength steels, can successfully represent wear resistant steels. The content of carbide elements, their size, and shape in the microstructure play an important role in the friction process and subsequent wear. Three types of loads were used and compared in the experiments 30, 60, and 90 N. Increasing the load results in significant degradation of the material on the sample surface. Lastly, the impact of hardness and roughness of materials on wear has also been proven. If abrasive wear occurs in the friction process, there is a greater degree of wear than that of adhesive wear. This is due to less abrasive particles, which behave like a cutting wedge and are subject to subsequent deformation strengthening due to the load increase, which adversely affects the further friction process. Analysis of the results showed that the ZrO2 ceramic ball showed significantly better wear values when compared to the X46Cr13 stainless steel ball. It also improves the values of the coefficient of friction with respect to the type of wear that occurs when the experimental materials and counterparts are in contact.

20 October 2019 in Metals
Verified
Journal Article
Open access
PDF file
MKMichal Krbaťa
Michal Krbaťa
MEMaros Eckert
Maros Eckert
DKDaniel Krizan
Daniel Krizan
IBIgor Igor Barényi
Igor Igor Barényi
IMIvana Mikušová
Ivana Mikušová
Analysis of the high temperature plastic behavior of high-strength steel X153CrMoV12 was developed in the temperature range of 800–1200 °C and the deformation rate in the range of 0.001–10 s−1 to the maximum value of the true strain 0.9%. Microstructural changes were observed using light optical microscopy (LOM) as well as atomic force microscopy (AFM). The effect of hot deformation temperature on true stress, peak stress and true strain was evaluated from the respective flow curves. Based on these results, steel transformation was discussed from the dynamic recovery and recrystallization point of view. Furthermore, a present model, taking into account the Zener–Hollomon parameter, was developed to predict the true stress and strain over a wide range of temperatures and strain rates. Using constitutive equations, material parameters and activation energy were derived, which can be subsequently applied to other models related to hot deformation behavior of selected tool steels. The experimental data were compassed to the ones obtained by the predictive model with the correlation coefficient R = 0.98267. These results demonstrate an appropriate applicability of the model for experimental materials in hot deformation applications.

19 June 2023 in Materials
Verified
Journal Article
Open access
PDF file
MKMichal Krbaťa
Michal Krbaťa
RCRóbert Cíger
Róbert Cíger
MKMarcel Kohutiar
Marcel Kohutiar
MEMaros Eckert
Maros Eckert
IBIgor Igor Barényi
Igor Igor Barényi
NBNaďa Beronská
Naďa Beronská
The paper deals with the dilatometric study of high-alloy martensitic tool steel with the designation M398 (BÖHLER), which is produced by the powder metallurgy process. These materials are used to produce screws for injection molding machines in the plastic industry. Increasing the life cycle of these screws leads to significant economic savings. This contribution focuses on creating the CCT diagram of the investigated powder steel in the range of cooling rates from 100 to 0.01 °C/s. JMatPro® API v7.0 simulation software was used to compare the experimentally measured CCT diagram. The measured dilatation curves were confronted with a microstructural analysis, which was evaluated using a scanning electron microscope (SEM). The M398 material contains a large number of carbide particles that occur in the form of M7C3 and MC and are based on Cr and V. EDS analysis was used to evaluate the distribution of selected chemical elements. A comparison of the surface hardness of all samples in relation to the given cooling rates was also carried out. Subsequently, the nanoindentation properties of the formed individual phases as well as the carbides, where the nanohardness and reduced modulus of elasticity (carbides and matrix) were evaluated.

15 July 2023 in Materials
Verified
Journal Article
Open access
PDF file
MKMichal Krbaťa
Michal Krbaťa
RCRóbert Cíger
Róbert Cíger
MKMarcel Kohutiar
Marcel Kohutiar
MSMaria Sozańska
Maria Sozańska
MEMaros Eckert
Maros Eckert
MSMartin Slaný
Martin Slaný
The presented work deals with the investigation of mechanical tribological properties on Inconel 625 superalloy, which is welded on a 16Mo3 steel pipe. The wall thickness of the basic steel pipe was 7 mm, while the average thickness of the welded layer was 3.5 mm. The coating was made by the cold metal transfer (CMT) method. A supercritical bending of 180° was performed on the material welded in this way while cold. The mechanical properties evaluated were hardness, wear resistance, coefficient of friction (COF) and change in surface roughness for both materials. The UMT Tribolab laboratory equipment was used to measure COF and wear resistance by the Ball-on-flat method, which used a G40 steel pressure ball. The entire process took place at an elevated temperature of 500 °C. The measured results show that the materials after bending are reinforced by plastic deformation, which leads to an increase in hardness and also resistance to wear. Superalloy Inconel 625 shows approximately seven times higher rate of wear compared to steel 16Mo3 due to the creation of local oxidation areas that support the formation of abrasive wear and do not create a solid lubricant, as in the case of steel 16Mo3. Strain hardening leads to a reduction of possible wear on Inconel 625 superalloy as well as on 16Mo3 steel. In the case of the friction process, the places of supercritical bending of the structure showed the greatest resistance to wear compared to the non-deformed structure.