High-strength and stiffness materials can further increase the lightweight construction potential of additive manufacturing. One way to achieve this, is to produce particle-reinforced aluminum matrix composites (PAMCs). A significant increase in strength can be achieved with ceramic particles smaller than 6 μm and a volume fraction of 20 to 30 % in other metallurgical processes. Due to the larger interparticle forces compared to the gravitational force, such powder mixtures are not flowable and cannot be recoated in PBF-LB with static recoaters like rubber lips and metal blades. Two approaches were compared to solve this problem. Firstly, the new broadband ultrasonic excitation of the recoater metal combs and secondly, flow enhancing with nanoparticles. The influence of the approaches was investigated by image analysis of the recoated layers for defects in an SLM 280 HL 1.0. Broadband vibration enables reliable recoating of AlSi10Mg powders mixed with up to 20 vol% 6 μm boron carbide particles without layer defects. Combined with TiC nanoparticle coating, 25 vol% are possible. The solution can securely be operated in build jobs.
29 January 2026 in The International Journal of Advanced Manufacturing Technology
With the increasing industrial implementation of additively manufactured metal parts, the welding of such components gains importance. Due to size limitations of laser powder-bed fusion (PBF-LB) machines and design constraints, subsequent joining processes are required. However, the weld seam quality of PBF-LB manufactured parts, particularly aluminum parts, is still limited by pore formation in the weld seam. These pores are believed to be primarily caused by the agglomeration of hydrogen. Therefore, this study investigates the pore formation during laser beam welding of PBF-LB manufactured AlSi10Mg parts by means of in-situ high-speed synchrotron X-ray imaging. In addition, an in-situ laser powder drying process is investigated to reduce the hydrogen content of PBF-LB manufactured aluminum parts in order to prevent the formation of hydrogen porosity during the subsequent welding process. Results show that pores predominantly form in the interdendritic region at the solidification front due to the locally increased hydrogen concentration. By applying laser powder drying, the hydrogen content can be reduced by up to 25%, thereby effectively preventing the formation of hydrogen pores.
In powder bed fusion with laser beam (PBF-LB), two process-induced defects by pore formation are known: local spherical pores by the keyhole effect and geometrically undefined pores caused by lack of fusion. Both pore types are heterogeneously distributed and can be used for lightweight or damping design applications. The achievable porosity is limited to around 13%. This article presents a novel process-controlled method enabling the targeted and reproducible manufacturing of solid parts with regularly distributed cavities, currently up to 60% porosity in AlSi10Mg, using the balling effect. This eliminates the need for time-consuming digital pre-processing work.