Copper sulfide (CuS) thin films were deposited on a glass substrate at room temperature using the radio-frequency (RF) magnetron-sputtering method at RF powers in the range of 40–100 W, and the structural and optical properties of the CuS thin film were investigated. The CuS thin films fabricated at varying deposition powers all exhibited hexagonal crystalline structures and preferred growth orientation of the (110) plane. Raman spectra revealed a primary sharp and intense peak at the 474 cm−1 frequency, and a relatively wide peak was found at 265 cm−1 frequency. In the CuS thin film deposited at an RF power of 40 W, relatively small dense particles with small void spacing formed a smooth thin-film surface. As the power increased, it was observed that grain size and grain-boundary spacing increased in order. The binding energy peaks of Cu 2p3/2 and Cu 2p1/2 were observed at 932.1 and 952.0 eV, respectively. Regardless of deposition power, the difference in the Cu2+ state binding energies for all the CuS thin films was equivalent at 19.9 eV. We observed the binding energy peaks of S 2p3/2 and S 2p1/2 corresponding to the S2− state at 162.2 and 163.2 eV, respectively. The transmittance and band-gap energy in the visible spectral range showed decreasing trends as deposition power increased. For the CuS/tin sulfide (SnS) absorber-layer-based solar cell (glass/Mo/absorber(CuS/SnS)/cadmium sulfide (CdS)/intrinsic zinc oxide (i-ZnO)/indium tin oxide (ITO)/aluminum (Al)) with a stacked structure of SnS thin films on top of the CuS layer deposited at 100 W RF power, an open-circuit voltage (Voc) of 115 mA, short circuit current density (Jsc) of 9.81 mA/cm2, fill factor (FF) of 35%, and highest power conversion efficiency (PCE) of 0.39% were recorded.
CdS films with a wide range of substrate temperatures as deposition parameters were fabricated on Corning Eagle 2000 glass substrates using RF magnetron sputtering. The crystallographic structure, microscopic surface texture, and stoichiometric and optical properties of each CdS film deposited at various substrate temperatures were observed to be highly temperature-dependent. The grown CdS thin films revealed a polycrystalline structure in which a cubic phase was mixed based on a hexagonal wurtzite phase. The relative intensity of the H(002)/C(111) peak, which represents the direction of the preferential growth plane, enhanced as the temperatures climbed from 25 °C to 350 °C. On the contrary, the intensity of the main growth peak at the higher temperatures of 450 °C and 500 °C was significantly reduced and exhibited amorphous-like behavior. The sharp absorption edge revealed in the transmission spectrum shifted from the long wavelength to the short wavelength region with the rise in the substrate temperature. The bandgap showed a tendency to widen from 2.38 eV to 2.97 eV when the temperatures increased from 25 °C to 350 °C. The CdS films grown at the temperatures of 450 °C and 500 °C exhibited glass-like transmittance with almost no interference fringes of light, which resulted in wide bandgap values of 3.09 eV and 4.19 eV, respectively.