Barium tungstate (BaWO4) powders with various sintering temperatures, and BaWO4:Dy3+ phosphor samples with concentrations of different rare-earth (RE) activator ions (Dy3+, Sm3+, Tb3+) were prepared through co-precipitation. The structural, morphological, and photoluminescent characteristics of barium tungstate phosphors depend on the concentration of RE ions. The crystallographic characteristics of the synthesized BaWO4 were analyzed using X-ray diffraction (XRD) patterns. The size and shape of the crystalline particles were estimated based on images measured with a field emission scanning electron microscope (FE-SEM). As the sintering temperature of the BaWO4 particles increased from 400 °C to 1000 °C, the size of the particles gradually increased and showed a tendency to clump together. In the sample doped with 7 mol % Dy3+ ions, the intensity of all emission bands reached their maximum. The emission spectra of the RE3+-doped BaWO4 powders by excitation at 325 nm were composed of yellow (Dy3+), red (Sm3+), and green (Tb3+) band at 572, 640, and 544 nm. This indicates that most of the RE3+ ions absorbed the position without reversal symmetry in the BaWO4 lattice. These results propose that strong emission intensity and tunable color for the phosphors can be accomplished by rare-earth doped host with an suitable quantity. In addition, the phosphor thin films, having high transparency from aqueous colloidal solutions, were deposited on banknotes, and it is considered whether it is suitable for anti-counterfeiting applications.
Copper sulfide (CuS) thin films were deposited on a glass substrate at room temperature using the radio-frequency (RF) magnetron-sputtering method at RF powers in the range of 40–100 W, and the structural and optical properties of the CuS thin film were investigated. The CuS thin films fabricated at varying deposition powers all exhibited hexagonal crystalline structures and preferred growth orientation of the (110) plane. Raman spectra revealed a primary sharp and intense peak at the 474 cm−1 frequency, and a relatively wide peak was found at 265 cm−1 frequency. In the CuS thin film deposited at an RF power of 40 W, relatively small dense particles with small void spacing formed a smooth thin-film surface. As the power increased, it was observed that grain size and grain-boundary spacing increased in order. The binding energy peaks of Cu 2p3/2 and Cu 2p1/2 were observed at 932.1 and 952.0 eV, respectively. Regardless of deposition power, the difference in the Cu2+ state binding energies for all the CuS thin films was equivalent at 19.9 eV. We observed the binding energy peaks of S 2p3/2 and S 2p1/2 corresponding to the S2− state at 162.2 and 163.2 eV, respectively. The transmittance and band-gap energy in the visible spectral range showed decreasing trends as deposition power increased. For the CuS/tin sulfide (SnS) absorber-layer-based solar cell (glass/Mo/absorber(CuS/SnS)/cadmium sulfide (CdS)/intrinsic zinc oxide (i-ZnO)/indium tin oxide (ITO)/aluminum (Al)) with a stacked structure of SnS thin films on top of the CuS layer deposited at 100 W RF power, an open-circuit voltage (Voc) of 115 mA, short circuit current density (Jsc) of 9.81 mA/cm2, fill factor (FF) of 35%, and highest power conversion efficiency (PCE) of 0.39% were recorded.
In the present study, Cu2O films were deposited on a glass substrate via RF (radio frequency) magnetron sputtering under substrate temperature conditions that ranged from room temperature (RT, 25 °C) to 400 °C. The structural, compositional, and optical properties of the Cu2O films were analyzed in relation to the experimental variables by applying various measurement methods. The substrate temperature was a crucial factor in shaping the structural, compositional, and optical properties of the Cu2O films that were synthesized via RF-magnetron sputtering. Our findings revealed that the Cu2O films exhibited a cubic structure, which was confirmed by XRD analysis. Specifically, the (111) and (200) planes showed different trends with respect to the substrate temperature. The intensity of the (111) peak increased at 250 °C, and above 300 °C, the preferred orientation of the (111) plane was maintained. The grain size, which was determined via FE-SEM, displayed a positive correlation with the substrate temperature. Additionally, XPS analysis revealed that the binding energy (BE) of the Cu2O film sputtered at 400 °C was similar to that which was previously reported. Notably, the as-grown Cu2O film demonstrated the highest transmittance (15.9%) in the visible region, which decreased with increasing substrate temperature. Furthermore, the energy band gap (Eg) of the Cu2O films remained constant (2.51 eV) at low substrate temperatures (25 °C to 200 °C) but exhibited a slight increase at higher temperatures, reaching 2.57 eV at 400 °C.
In this study, a porous Ni-foam support was employed to enhance the capacitance of nickel cobaltite (NiCo2O4) electrodes designed for supercapacitors. The hydrothermal synthesis method was employed to grow NiCo2O4 as an active material on Ni-foam. The NiCo2O4 sample derived from hydrothermal synthesis underwent subsequent post-heat treatment at temperatures of 250 °C, 300 °C, and 350 °C. Thermogravimetric analysis of the NiCo2O4 showed that weight loss due to water evaporation occurs after 100 °C and enters the stabilization phase at temperatures above 400 °C. The XRD pattern indicated that NiCo2O4 grew into a spinel structure, and the TEM results demonstrated that the diffraction spots (DSs) on the (111) plane of the sample annealed at 350 °C were more pronounced than those of other samples. The specific capacitance of the NiCo2O4 electrodes exhibited a decrease with increasing current density across all samples, irrespective of the annealing temperature. The electrode annealed at 350 °C recorded the highest specific capacitance value. However, the capacity retention rate of the NiCo2O4 electrode revealed a deteriorating trend, declining to 88% at 250 °C, 75% at 300 °C, and 63% at 350 °C, as the annealing temperature increased.
The precursor prepared by co-precipitation method was sintered at various temperatures to synthesize crystalline manganese tungstate (MnWO4). Sintered MnWO4 showed the best crystallinity at a sintering temperature of 800 °C. Rare earth ion (Dysprosium; Dy3+) was added when preparing the precursor to enhance the magnetic and luminescent properties of crystalline MnWO4 based on these sintering temperature conditions. As the amount of rare earth ions was changed, the magnetic and luminescent characteristics were enhanced; however, after 0.1 mol.%, the luminescent characteristics decreased due to the concentration quenching phenomenon. In addition, a composite was prepared by mixing MnWO4 powder, with enhanced magnetism and luminescence properties due to the addition of dysprosium, with epoxy. To one of the two prepared composites a magnetic field was applied to induce alignment of the MnWO4 particles. Aligned particles showed stronger luminescence than the composite sample prepared with unsorted particles. As a result of this, it was suggested that it can be used as phosphor and a photosensitizer by utilizing the magnetic and luminescent properties of the synthesized MnWO4 powder with the addition of rare earth ions.
This study examines the impact of varying oxygen flow rates on the properties of Cu2O thin films deposited via radio frequency (RF) magnetron sputtering. X-ray diffraction (XRD) analysis showed a phase transition from cubic Cu2O to a mixed Cu2O and CuO phase, eventually forming a Cu4O3 tetragonal structure as oxygen content increased. The surface morphology and cross-sectional structure of Cu2O thin films observed through field emission scanning electron microscopy (FE-SEM) were found to vary significantly depending on the oxygen flow rate. X-ray photoelectron spectroscopy (XPS) indicated notable variations in the chemical states of copper and oxygen. The Cu 2p spectra revealed peaks around 933 eV and 953 eV for all samples, with the S01 sample (deposited with only argon gas) exhibiting the lowest intensity. The S02 sample showed the highest peak intensity, which then gradually decreased from S03 to S06. The O 1s spectra followed a trend with peak intensity being highest in S02 and decreasing with further oxygen flow rates, indicating the formation of complex oxides such as Cu4O3. UV-Vis-NIR spectroscopy results demonstrated a decrease in transmittance and optical band gap energy with increasing oxygen content, suggesting a decline in crystallinity and an increase in defects and impurities. These findings underscore the critical role of precise oxygen flow rate control in tailoring the structural, morphological, compositional, and optical properties of Cu2O thin films for specific electronic and optical applications.