The freezing–thawing method has been commonly used in the preparation of polyvinyl alcohol hydrogel magnetorheological plastomer (PVA HMRP). However, this method is complex and time consuming as it requires high energy consumption and precise temperature control. In this study, PVA HMRP was prepared using a chemically crosslinked method, where borax is used as crosslinking agent capable of changing the rheological properties of the material. Three samples of PVA HMRP with various contents of carbonyl iron particles (CIPs) (50, 60, and 70 wt.%) were used to investigate their rheological properties in both steady shear and dynamic oscillation modes. Results showed the occurrence of shear thickening behaviour at low shear rate (γ > 1 s−1), where the viscosity increased with the increased of shear rate. Moreover, the storage modulus of the samples also increased increasing the oscillation frequency from 0.1 to 100 Hz. Interestingly, the samples with 50, 60 70 wt.% of CIPs produced large relative magnetorheological (MR) effects at 4916%, 6165%, and 10,794%, respectively. Therefore, the inclusion of borax to the PVA HMRP can offer solutions for a wide range of applications, especially in artificial muscle, soft actuators, and biomedical sensors.
In this study, magnetorheological elastomer (MRE) was fabricated using an electromagnetic device with a new configuration mold at the orientation of 0°, 45° and 90°. This new curing concept enhanced the alignment of carbonyl iron particles (CIPs) within the silicone matrix in the presence of silicone oil (SO) during solidifying, by eliminating air gaps to prevent magnetic flux losses. Using a mold made of steel, which is a magnetic material, the mold functions as a guide for concentrated magnetic flux of 0.315 T to pass through the MRE sample. Scanning electron microscopy (SEM) was used to observe the surface morphology of the fabricated MRE samples particularly the alignment of the CIPs. The field-dependent dynamic properties of the MREs were measured using a rheometer. The analysis implied that the effectiveness of the MRE operating under shear deformation with this curing concept provided the highest magneto-induced modulus of 1.01 MPa when a 45° orientation mold is used, with relative magnetorheological (MR) effect value up to 918%, followed by 0° mold orientation with 0.79 MPa magneto-induced modulus and 646% relative MR effect. The high modulus properties offered by this MRE are believed to be potentially useful in industrial applications where a high range of stiffness is required particularly in the shear direction.