24 February 2022 in Minerals
Verified
Journal Article
Open access
PDF file
YCYan-Bo Chen
Yan-Bo Chen
YDYu Du
Yu Du
YGYu-Feng Guo
Yu-Feng Guo
XGXing-Min Guo
Xing-Min Guo
Secondary hematite (SH) is a serious factor resulting in reduction degradation of iron ore sinter in a blast furnace; however, until now, a quantitative study for SH formation had not been reported. In this work, the effects of gangue composition, including MgO, Al2O3 and SiO2, on the solid-state formation in the sintering process of iron ore fines were investigated quantitatively. It shows that the SH formation decreased from 67.84% to 46.11%, 35.44% and 22.37% after adding 1.0%, 3.0% and 5.0% MgO, respectively, while for Al2O3, the amount increased to 69.38%, 69.98% and 70.56%, respectively. For SiO2, the amount changed to 68.14%, 61.59% and 47.96%, respectively. Simultaneously, the magnetite (magnesioferrite) formation increased from 8.24% to 34.79%, 50.26% and 70.45% after adding 1.0%, 3.0% and 5.0% MgO, respectively. For Al2O3 and SiO2, the amount changed to 8.95%, 8.37%, 7.62% and 7.62%, 11.10%, 18.77%, respectively, compared with no gangue. This indicates that the SH formation increased with decrease in magnesioferrite. It was found that the decrease in SH formation relates to the diffusion of Mg2+ in magnesioferrite, which inhibits the solid-state formation of SH kinetically. A supposition was suggested that a maghemite existed at a high temperature, and decreased with an increase in MgO addition. This would be another reason to improve the degradation performance of iron ore sinter.

29 July 2022 in Materials
Verified
Journal Article
Open access
PDF file
RXRui Feng Xin
Rui Feng Xin
YDYu Du
Yu Du
XGXing-Min Guo
Xing-Min Guo
Al2O3 is a gangue component in iron ores, significantly influencing the formation and crystallization of calcium ferrite in the sintering process. But the mechanism of the Al2O3 effect on the crystallization of calcium ferrite is rarely reported. In this work, a crystallization device was designed to investigate the crystallization behavior of calcium ferrite in Fe2O3-CaO-SiO2-Al2O3 melt under non-isothermal conditions. XRD, SEM-EDS, and optical microscopy were used to identify the crystalline phase and the microstructure of samples. The result shows that the crystal morphology of SFCA changed in the order of strip, column, and needle as the Al2O3 content increased. The crystallization sequence of samples containing Al2O3 was observed as Ca4Fe14O25 (C4F14) → Fe2O3 → Ca3.18Fe15.48Al1.34O36 (SFCA-I) → CaFe2O4 (CF) → Ca5Si2(Fe, Al)18O36 (SFCA) → γ-Ca2SiO4 (C2S). The generation pathway of SFCA-I was found to be C4F14 + Si4+ + Al3+ → SFCA-I. Increasing the cooling rate can promote the formation of C4F14, SFCA-I, Fe2O3 and the amorphous phase. However, it prevented the crystallization of CF and SFCA while inhibiting the transformation of β-C2S to γ-C2S. When the Al2O3 content reached or exceeded 2.5 mass pct, the viscosity of Fe2O3-CaO-SiO2-Al2O3 melt increased sharply, resulting in the decrease in the crystal size of calcium ferrite.

17 May 2024 in Metallurgical and Materials Transactions B
Verified
Journal Article
Closed access
PDF file
YDYu Du
Yu Du
XGXing-Min Guo
Xing-Min Guo

15 November 2025 in Molecules
Verified
Journal Article
Open access
PDF file
YDYu Du
Yu Du
JSJianning Sun
Jianning Sun
BLBin Li
Bin Li
XDXueyan Du
Xueyan Du
Yongkun YangYongkun Yang
Yongkun Yang
XGXing-Min Guo
Xing-Min Guo
Magnetite (Fe3O4) is an essential material for enhancing microwave absorption performance and is widespread and abundant as a solid solution in natural minerals and metallurgical slags. In this work, the effect of Mg2+ on the structure, stabilization, and microwave absorption performance of magnesium-containing magnetite (MgxFe3−xO4) was investigated. On the basis of experiments on the reactions of Fe2O3 and MgO under different levels of pCO/(pCO + pCO2), MgxFe3−xO4 (x=0.0,0.2,0.4,0.6,1.0) was synthesized, and Mg2+ was found to inhibit the re-oxidation of magnetite. On this basis, the microwave absorption performance of various synthesized MgxFe3−xO4 samples was measured and analyzed, where Mg2+ was found to enhance the microwave absorption performance of Fe3O4, and the RLmin value of Mg0.2Fe2.8O4 increased to −50.43 dB compared to that of −19.20 dB for Fe3O4. Furthermore, the enhancement mechanism of Mg2+ was revealed through impedance matching, dielectric and magnetic loss tangents, and magnetization curves, where the Mg2+ ions were found to accelerate the hopping of electrons and change the impedance matching of MgxFe3−xO4 to a more ideal state.

14 April 2024 in Minerals
Verified
Journal Article
Open access
PDF file
YDYu Du
Yu Du
HGHui Guo
Hui Guo
XGXing-Min Guo
Xing-Min Guo
Calcium ferrite containing aluminum (CFA) is a precursor of the low-temperature bonding phase in the sintering process of iron ore fines for blast furnace ironmaking. Thus, improving the formation of CFA at lower temperature is very important for saving energy, improving efficiency and production. In this paper, the formation process of CFA was investigated at 1200 °C by reactions of alumina (Al2O3), respectively with a mixture of calcium oxide (CaO) and hematite (Fe2O3) and monocalcium ferrite (CF) as a recognized initial product, as well as reaction of Al-containing hematite (Hss) with CF. The result confirmed that CF is an intermediate product formed easily in the sintering process, and it may react with excessive Fe2O3 to generate an alpha-calcium iron oxide (Ca2Fe15.50O25) as a new phase. It was found that CFA can be formed directly by reactions of CF with Hss and Ca2Fe15.50O25 with Al2O3, while the reaction of CF with Al2O3 is more helpful in generating Ca2Fe15.5O25 rather than CFA, simultaneously forming a calcium aluminum oxide (CaAl2O4, CA; CaAl4O7, CA2). It was revealed that the appearance of CA and CA2 is a main reason to hinder CFA formation in the sintering process of iron ore fines.