Selective Laser Melting (SLM) technology is a new kind of additive manufacturing technology developed in in the last decade. Measurement and control of stress in metal forming layer is the basic problem of SLM forming parts. Critical Refraction Longitudinal (LCR) wave method was used to measure stress. The acoustic-elastic formulas for measuring stresses in SLM 316L stainless steel forming parts manufactured using meander, stripe, and chess board scanning strategies, respectively, were established based on static load tensile test. The experimental results show that the acoustic time difference of LCR wave in SLM specimen manufactured with 316L stainless steel increases linearly with the increase of stress when the tensile stress is less than critical stress (372 MPa, 465 MPa, and 494 MPa). Due to the inhomogeneous deformation of the anisotropic SLM forming layer and the dimple-micropore aggregation fracture mechanism, the acousto-elastic curve fluctuates up and down along the irregular curve when the tensile stress is larger than critical stress. The results of corroboration experiments show that nondestructive measurement of stress in SLM forming specimen can be realized by using LCR wave method. The scanning strategy can significantly affect the tensile strength and yield strength of SLM forming specimen. The stresses were all in tension stress state at the edge of the specimens, whatever scanning strategy was used. Sub-area scanning and scanning sequence of alternate and intersect were adopted, which can effectively reduce the stress in the SLM forming specimen. The overall stress values of SLM forming specimen manufactured using chess board scanning strategy were smaller than that using meander and stripe strategies. The distribution of stress were more uniform.
This paper studies the effects of different combinations of scanning strategies between layers on the surface quality, tensile properties, and microstructure of samples in a laser beam powder bed fusion (L-PBF) formation experiment of Ti-6Al-4V titanium alloy. The purpose of this experiment was to improve the comprehensive performance of the piece by selecting the optimal combination of scanning strategies. The results show that the surface roughness of the L-PBF specimen was the lowest under the combination of the CHESS scanning strategy, reaching 14 μm. The surface hardness of the samples was generally higher with the LINE scanning strategy and the angle offset of 90°, reaching 409 HV. The overall density of the samples was higher under the combination of CHESS scanning strategies, reaching 99.88%. Among them, the CHESS&45° sample had the best comprehensive properties, with a density of 99.85%, a tensile strength of up to 1125 MPa, a yield strength of 912 MPa, and an elongation of 8.2%. The fractured form was a ductile fracture, with many dimple structures. Compared with the CHESS scanning strategy, the tensile properties of the CHESS&45° samples were improved by 12.8%. The microstructure of the L-PBF sample was mainly composed of the primary β phase and α’ martensite phase. The upper surface of the CHESS scanning strategy combination sample had a clear melt channel, and the distribution of each phase was uniform. A certain number of columnar β crystals were distributed in the longitudinal section of the sample, which was paralleled to the build direction. The columnar β crystals of CHESS&45° were relatively coarse, which enhanced the tensile properties of the sample.
To improve the quality of thick powder bed and realize the matching of thick powder bed and thin powder bed in the later stage, the influence of process parameters for the single-track, multi-layer fabrication, relative density, surface quality, defect, remelting, and boundary optimization performance of different layer thicknesses of Ti-6Al-4V fabricated by selective laser melting were investigated. It is more conducive to the stable forming of single-track when the point distance is half the diameter of the laser beam, and the exposure time is appropriately extended. The thin powder bed needs the corresponding point distance and exposure time under the laser power of 280–380 W to obtain high-density specimens. The thick powder bed needs to be able to ensure the formation of high-quality specimens under the smaller point distance and longer exposure time under higher laser power of 380 W. Both thick powder bed and thin powder bed will cause un-melted defects between molten pools, spheroidization defects caused by splashing, and microporous defects. The remelting process can significantly improve the surface quality of the formed specimen, but the surface quality of the thick powder bed is worse than that of the thin powder bed. The boundary quality of thick powder bed is worse than that of thin powder bed, and the boundary shape has a greater influence on the quality of the SLM forming boundary. Different strategies should be adopted to form the boundary of different shapes. Increasing the boundary count and increasing the laser power are more conducive to the improvement of boundary quality.