Heon Kang

Prof. Heon Kang

orcid

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
8 February 2022 in Materials
Verified
Journal Article
Open access
PDF file
KCKwangmin Choi
Kwangmin Choi
JSJaeHyuck Shin
JaeHyuck Shin
HKHeon Kang
Heon Kang
To increase the utilization of die-cast Mg alloys with various shapes in a variety of environments, the corrosion behaviors of commercial die-cast Mg alloys with different thicknesses were investigated in neutral and alkali solutions at ambient temperature. A decrease in the thickness of a specimen leads to an increase in cooling and solidification rates, which, in turn, decreases the size of the eutectic β phases and the interphase distance, thus improving the hardness of the specimen. Specimens with relatively large β phases were more corroded under neutral conditions due to severe galvanic corrosion at the interface between α-Mg and the β phases, whereas they were protected by passivation films formed on the substrate in the alkaline solution. However, in the case of the alloy with thin thickness and high solidification rate, the fine β phases improved corrosion resistance by forming a net structure that acted as a barrier to corrosion propagation of the α matrix. These results suggest that the size and distribution of the eutectic phases should be appropriately controlled, depending on the environment.

9 November 2022 in Materials
Verified
Journal Article
Open access
PDF file
JJJeon Jonggyu
Jeon Jonggyu
SLSangjun Lee
Sangjun Lee
JKJoonseok Kyeong
Joonseok Kyeong
SSSe Eun Shin
Se Eun Shin
HKHeon Kang
Heon Kang
The effects of the shapes (needle and round) and volume fractions (low and high) of microscale particles in Al-Si-Mg-Cu-based alloys on recrystallization behavior, texture evolution, mechanical properties, and formability are investigated. The recrystallized grain size decreases as the size and volume fraction of the particles decrease and increase, respectively, regardless of the particle shape. The investigated alloys with a relatively low volume fraction of 0.7 to 2.4 vol.% exhibit higher efficiency particle-stimulated nucleation (PSN) than alloys with a high volume fraction of 6.0 to 21.0 vol.%. This is because the interaction between the particles and dislocations cannot be greatly promoted when the volume fraction of the particles is large enough to form agglomerates. The sheets with round-shaped particles exhibit higher yield strength (YS) and elongation (EL) than sheets with needle-shaped particles. The improvement in YS is due to the combined effects of grain refinement and particle strengthening, and the EL is improved by reducing the probability of cracking at the tips of round-shaped particles. The sheets with round-shaped particles exhibit relatively higher average plastic strain ratio (r¯) and planar anisotropy (∆r) than the sheets with needle-shaped particles, owing to the development of Goss {110} or rotated-Goss {110} orientations.

3 December 2024 in Materials
Verified
Journal Article
Open access
PDF file
JJJeon Jonggyu
Jeon Jonggyu
SLSangjun Lee
Sangjun Lee
JJJeheon Jeon
Jeheon Jeon
MKMaru Kang
Maru Kang
HKHeon Kang
Heon Kang
The presence of Al7Cu2Fe particles, formed due to Fe impurities in Al-Zn-Mg-Cu alloys, significantly impacts mechanical properties and formability, which is crucial for the use of these alloys in the automotive and aerospace industries. In this study, we prepared Al-Zn-Mg-Cu-based alloy sheets with large (LF), small (SF), and no (NF) Al7Cu2Fe particles to explore their effects on recrystallization and mechanical behavior. These sheets were fabricated using controlled cooling rates and subsequent thermo-mechanical processing. Fine dispersion of Al7Cu2Fe particles in the SF sheet led to a substantial reduction in grain size (16.5 μm) and an increase in yield strength (168.6 MPa), albeit with lower ductility (24.6%). In contrast, the NF sheet exhibited a lower yield strength (141.5 MPa) but superior ductility (35.8%) due to the absence of Al7Cu2Fe particles, which prevented premature fracture. The SF sheet demonstrated lower anisotropy in ductility due to the uniform recrystallized grain orientations, while the LF and NF sheets exhibited significant anisotropy in yield strength. These findings indicate that optimizing Al7Cu2Fe particle dispersion is key to balancing the strength, ductility, and anisotropy in Al-Zn-Mg-Cu alloys.

29 October 2024 in Materials
Verified
Journal Article
Open access
PDF file
JJJeon Jonggyu
Jeon Jonggyu
SLSangjun Lee
Sangjun Lee
JJJeheon Jeon
Jeheon Jeon
MKMaru Kang
Maru Kang
HKHeon Kang
Heon Kang
The influence of as-cast grain size on recrystallization and the related mechanical properties of Al–Zn–Mg–Cu-based alloys was investigated. Grain sizes ranging from 163 to 26 μm were achieved by adding Ti, Cr and Mn, and ZnO nano-particles, which acted as heterogeneous nucleation sites. A decrease in the as-cast grain size led to a corresponding reduction in the recrystallized grain size from 54 to 13 μm. Notably, as-cast grain sizes below 100 μm provided additional nucleation sites at grain boundaries, allowing for a reasonable prediction of recrystallized grain size. Finer grains also contributed to enhanced mechanical properties, with yield strength increasing as recrystallized grain size decreased without significant loss of elongation. Additional strengthening was observed due to η-precipitates at grain boundaries, further improving the properties of fine-grained sheets.

16 January 2023 in Materials
Verified
Journal Article
Open access
PDF file
SLSangjun Lee
Sangjun Lee
HKHeon Kang
Heon Kang
DBDong Hyun Bae
Dong Hyun Bae
The crack propagation behavior of Al containing Mg–Si clusters is investigated using molecular dynamics (MD) simulations to demonstrate the relationship between the natural aging time in Al–Si–Mg alloys and ductility. Experimental results show that the elongation at failure decreases with natural aging. There are few studies on the relationship between natural aging and ductility because of the difficult observation of Mg–Si clusters. To solve the difficulty, cracked Al containing Mg–Si clusters of varying sizes are assumed for the MD simulations. A larger Mg–Si cluster in Al results in earlier crack opening and dislocation emission. Moreover, as the Mg–Si cluster size increases, the stress near the crack tip becomes more concentrated. This causes rapid crack propagation, a similar effect to that of crack tip sharpening. As a result of long-term natural aging, the cracks expand rapidly. The influence of geometry is also investigated. Crack lengthening and thickness reduction negatively impact the fracture toughness, with the former having a larger impact than the latter. Although there are several discrepancies in the practical deformation conditions, the simulation results can help to more thoroughly understand natural aging in Al–Si–Mg alloys.

21 September 2022 in Materials
Verified
Journal Article
Open access
PDF file
SLSangjun Lee
Sangjun Lee
HKHeon Kang
Heon Kang
JJJeon Jonggyu
Jeon Jonggyu
DBDong Hyun Bae
Dong Hyun Bae
The influence of cluster composition and the addition of vacancies on the decomposition behavior of clusters during artificial aging in Al–Si–Mg alloys were analyzed according to the kinetic Montel Carlo model. Clusters with a balanced composition (Mg/(Mg + Si) = 0.5) were the most difficult to decompose. In addition, the cluster decomposition was slower when more vacancies were added to the cluster. Among Si, Mg, and vacancies, vacancies most significantly affect decomposition. The clusters with Mg/(Mg + Si) ≤ 0.4 strongly trap vacancies, which can be classified as hardly decomposable vacancy-rich clusters. The clustering behavior during natural aging and the effect of pre-aging were analyzed using the Kinetic Monte Carlo model. Pre-aging slows down cluster formation due to the lowered vacancy concentration. In addition, the overall composition of the clusters changes to easily decomposable clusters after pre-aging. Thus, not only is the number of clusters reduced but also the clusters are more easily decomposable when pre-aging is performed.