The effects of the shapes (needle and round) and volume fractions (low and high) of microscale particles in Al-Si-Mg-Cu-based alloys on recrystallization behavior, texture evolution, mechanical properties, and formability are investigated. The recrystallized grain size decreases as the size and volume fraction of the particles decrease and increase, respectively, regardless of the particle shape. The investigated alloys with a relatively low volume fraction of 0.7 to 2.4 vol.% exhibit higher efficiency particle-stimulated nucleation (PSN) than alloys with a high volume fraction of 6.0 to 21.0 vol.%. This is because the interaction between the particles and dislocations cannot be greatly promoted when the volume fraction of the particles is large enough to form agglomerates. The sheets with round-shaped particles exhibit higher yield strength (YS) and elongation (EL) than sheets with needle-shaped particles. The improvement in YS is due to the combined effects of grain refinement and particle strengthening, and the EL is improved by reducing the probability of cracking at the tips of round-shaped particles. The sheets with round-shaped particles exhibit relatively higher average plastic strain ratio () and planar anisotropy (∆r) than the sheets with needle-shaped particles, owing to the development of Goss {110} or rotated-Goss {110} orientations.
The presence of Al7Cu2Fe particles, formed due to Fe impurities in Al-Zn-Mg-Cu alloys, significantly impacts mechanical properties and formability, which is crucial for the use of these alloys in the automotive and aerospace industries. In this study, we prepared Al-Zn-Mg-Cu-based alloy sheets with large (LF), small (SF), and no (NF) Al7Cu2Fe particles to explore their effects on recrystallization and mechanical behavior. These sheets were fabricated using controlled cooling rates and subsequent thermo-mechanical processing. Fine dispersion of Al7Cu2Fe particles in the SF sheet led to a substantial reduction in grain size (16.5 μm) and an increase in yield strength (168.6 MPa), albeit with lower ductility (24.6%). In contrast, the NF sheet exhibited a lower yield strength (141.5 MPa) but superior ductility (35.8%) due to the absence of Al7Cu2Fe particles, which prevented premature fracture. The SF sheet demonstrated lower anisotropy in ductility due to the uniform recrystallized grain orientations, while the LF and NF sheets exhibited significant anisotropy in yield strength. These findings indicate that optimizing Al7Cu2Fe particle dispersion is key to balancing the strength, ductility, and anisotropy in Al-Zn-Mg-Cu alloys.
The influence of as-cast grain size on recrystallization and the related mechanical properties of Al–Zn–Mg–Cu-based alloys was investigated. Grain sizes ranging from 163 to 26 μm were achieved by adding Ti, Cr and Mn, and ZnO nano-particles, which acted as heterogeneous nucleation sites. A decrease in the as-cast grain size led to a corresponding reduction in the recrystallized grain size from 54 to 13 μm. Notably, as-cast grain sizes below 100 μm provided additional nucleation sites at grain boundaries, allowing for a reasonable prediction of recrystallized grain size. Finer grains also contributed to enhanced mechanical properties, with yield strength increasing as recrystallized grain size decreased without significant loss of elongation. Additional strengthening was observed due to η-precipitates at grain boundaries, further improving the properties of fine-grained sheets.
6 November 2024 in Materials Science and Engineering: A
This study investigated the effects of aging profiles on the precipitate formation and the corresponding strengthening and deformation behaviors of Al–Mg–Zn alloys. The alloys subjected to natural aging (NA) demonstrated significantly enhanced ductility at equivalent stress levels compared to those subjected to artificial aging (AA). In AA-treated alloys, η′ and η-phases with incoherent interfaces were formed, while GP zones and solute clusters were dominantly exhibited in the NA-treated alloy with a coherent interface with the matrix. Due to the change in interface bonding, the dislocation movement and pinning behavior after deformation are varied depending on the aging conditions of Al–Mg–Zn alloy sheet. Thus, the elongation to fracture of the NA alloy sheet was improved compared to that of the AA alloy sheet because of the enhanced work-hardening capacity and the thin precipitate-free zone (PFZ). Deformation textures and dislocation densities varied between NA and AA treatments, as revealed by electron backscatter diffraction (EBSD) and kernel average misorientation (KAM) analysis. The interactions between the precipitates, dislocations, and the PFZ in the AA- and NA-treated alloys were analyzed via transmission electron microscopy (TEM). The insights gained from this research provide a valuable foundation for industrial applications, particularly in sectors demanding lightweight, high-strength materials, where optimizing the aging process can lead to significant performance improvement and cost savings.