An in-situ, catalyst-free method for synthesizing 3C-SiC ceramic nanowires (SiCNWs) inside carbon–carbon (C/C) composites was successfully achieved. Obtained samples in different stages were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), and Raman scattering spectroscopy. Results demonstrated that the combination of sol-gel impregnation and carbothermal reduction was an efficient method for in-situ SiCNW synthesis, inside C/C composites. Thermal properties and mechanical behaviors—including out-of-plane and in-plane compressive strengths, as well as interlaminar shear strength (ILLS) of SiCNW modified C/C composites—were investigated. By introducing SiCNWs, the initial oxidation temperature of C/C was increased remarkably. Meanwhile, out-of-plane and in-plane compressive strengths, as well as interlaminar shear strength (ILLS) of C/C composites were increased by 249.3%, 109.2%, and 190.0%, respectively. This significant improvement resulted from simultaneous reinforcement between the fiber/matrix (F/M) and matrix/matrix (M/M) interfaces, based on analysis of the fracture mechanism.
A SiC ceramic coating was prepared on carbon/carbon composites by pack cementation. The phase composition and microstructure of the coated specimens were characterized using X-ray diffraction instrument and scanning electron microscope. The results showed that the mass-loss percentage of the coated specimen was 9.5% after being oxidized for 20 h. The oxidation failure of the SiC ceramic coating at 1773 K was analysed by non-destructive X-ray computed tomography. The effective self-healing of cracks with widths below 12.7 μm introduced during the coating preparation process and generated while the specimens cooled down from the high oxidation temperature prevented the oxidation of carbon/carbon composites. X-ray computed tomography was used to obtain three-dimensional images revealing internal damage caused by spallation and open holes on the coating. Stress induced by heating and cooling caused the formation, growth and coalescence of cracks, which in turn led to exfoliation of the coating and subsequent failure of oxidation protection.
Surface modified carbon/carbon(C/C) composites were joined to Li2CO3-Al2O3-SiO2(LAS) glass ceramic by hot pressing bonding using MgO-Al2O3-SiO2(MAS) glass with different thicknesses as the joining material.The effect of interlayer thickness on the joint strength was discussed.Microstructures and mor-phologies of the as-received joints and fractured surfaces were characterized by scanning electron microscope.The results indicated that the LAS glass was directly joined to the surface modified C/C composites at 1200℃,and the room-temperature shear strength of the joints was only 10MPa,due to its poor wettability with base material.When the MAS glass was applied as interlayer,the joint shear strength increased at first and then decreased with the increase of the interlayer thickness.The maximum value of the shear strength reached 26.61MPa when interlayer thickness was 80μm.
In order to achieve the highly efficient preparation of high-performance carbon/carbon (C/C) composites, epitaxial grown carbon nanotubes (CNTs) and a pyrocarbon matrix were simultaneously synthesized to fabricate CNT-reinforced C/C composites (CC/C composites). With precise control of the temperature gradient, CNTs and the pyrocarbon matrix could grow synchronously within a 2D needle-punched carbon fiber preform. Surprisingly, the CNTs remained intact within the pyrocarbon matrix at the nano-level, and the CNT-reinforced nano-pyrocarbon matrix was compact, with virtually no gaps and pores, which were tightly connected with the carbon fibers without cracks. Based on the results of Raman analysis, there is less residual stress in the CNT-reinforced pyrocarbon matrix and carbon fibers, and less of a mismatch between the coefficient and thermal expansion. Additionally, CC/C composites fabricated by this method could achieve a low density, open porosity with a large size, and improved mechanical properties. More importantly, our work provides a rational design strategy for the highly efficient preparation and structural design of high-performance CNT-einforced C/C composites.
20 February 2010 in Journal of Inorganic Materials
The 2D C/C composites with different microstructures were fabricated by isothermal-isobaric chemical vapor infiltration (ICVI). The mechanical properties of the 2D C/C composites were investigated by 3-point bending tests. The microstructures of the pyrocarbon matrix were observed by polarized light microscope (PLM), scanning electron microscope (SEM), transmission electron microscope (TEM) combining selected area electron diffraction (SAED). The results show that 2D C/C composites with dominant layered-HT pyrocarbon matrix exhibit a pseudo-plastic failure behavior. The flake-like fragments MT and granular-like particles ISO are in favor of increasing the flexural strength of the materials. It exists a good interfacial bonding between the fiber and HT layer. The non-HT layer does not exist at the interface, but the orientation angle (OA) of the matrix slightly increases
1 October 2009 in Journal of Wuhan University of Technology-Mater. Sci. Ed.