An in-situ, catalyst-free method for synthesizing 3C-SiC ceramic nanowires (SiCNWs) inside carbon–carbon (C/C) composites was successfully achieved. Obtained samples in different stages were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), and Raman scattering spectroscopy. Results demonstrated that the combination of sol-gel impregnation and carbothermal reduction was an efficient method for in-situ SiCNW synthesis, inside C/C composites. Thermal properties and mechanical behaviors—including out-of-plane and in-plane compressive strengths, as well as interlaminar shear strength (ILLS) of SiCNW modified C/C composites—were investigated. By introducing SiCNWs, the initial oxidation temperature of C/C was increased remarkably. Meanwhile, out-of-plane and in-plane compressive strengths, as well as interlaminar shear strength (ILLS) of C/C composites were increased by 249.3%, 109.2%, and 190.0%, respectively. This significant improvement resulted from simultaneous reinforcement between the fiber/matrix (F/M) and matrix/matrix (M/M) interfaces, based on analysis of the fracture mechanism.
This paper examines the influence of temperature and oxygen on the growth of large-scale silicon carbide nanowires by using a combination of sol–gel impregnation and carbothermal reduction methods. To investigate the growth process of SiC nanowires, the microstructural changes of nanowires at different temperatures from 1050 °C to 1550 °C were observed using SEM. In addition, XRD, TEM and FTIR were also used to analyze the nucleation, crystal structure and chemical phase of the SiC nanowires. XPS revealed the chemical reactions that occur during the growth of SiC nanowires. In this paper, we also evaluated the impacts of temperature and oxygen from SiOC (an intermediate) on the growth of SiC nanowires. The results show that a proper temperature was necessary for the nucleation and growth of SiC nanowires. The findings also indicate that the presence of O2 could contribute to the growth of longer SiC nanowires.
10 July 2014 in Acta Metallurgica Sinica (English Letters)
SiC-coated C/C composites with mechanical damage were repaired by the heat treatment method and slurry painting–preoxidation. The effects of different process parameters on the microstructure, interface bonding and oxidation resistance of Si-SiC repair coatings at 1773 K for 10 h were studied. The results show that the repair coating is tightly bonded to the original coating and the C/C substrate, and there is no obvious interface. Under the optimal parameters, the weight reduction in the repaired specimen merely amounted to 0.32% subsequent to oxidation at 1773 K for 10 h, and the mass loss was 74.79% lower than that of the damaged specimen, being proximate to that of the intact specimen. The objective of this work lies in achieving a greater density of the coating within the repair zone by manipulating the diverse powder ratios and preoxidation temperatures in the repair slurry, thereby safeguarding the C/C composite material against oxidation during its service. It offers a convenient and highly efficient approach for the repair of coatings with substantial size defects, significantly prolonging the service life of the material.
The bonding strength, mechanical properties and high-temperature thermal shock resistance of C/C–SiC composites after undergoing simulated low earth orbit environment including cryogenic thermal cycles (CTCs) between 153 and 393 K for 200 times with high-vacuum state of 1.3 × 10−3 Pa were investigated. Results of the tests showed that, the bonding strength at coating/substrate interface monotonically decreased as the CTCs increased. After 100 CTCs, the flexural strength of C/C–SiC composites enhanced and the percentage of remaining strength was 102.60%, while, the mass loss of specimens decreased from 2.08 to 0.89% after thermal shock resistance test between 1773 K and room temperature for 15 times. Once CTCs exceed 100 times, the mass loss increased, the flexural strength reduced and remained only 87.40% of initial strength after 200 CTCs. The fractural behaviour of CTCs-treated modified composites exhibited typical brittle mode. A model based on the evolution of the residual thermal stress after CTCs treatment was proposed to explain the oxidation failure mechanism of C/C–SiC specimens.