yayun he

Dr. yayun he


Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
27 July 2024 in Materials
Verified
Journal Article
Open access
PDF file
YHyayun he
yayun he
XZXi Zhao
Xi Zhao
MJMinhang Jiao
Minhang Jiao
XRXianwei Ren
Xianwei Ren
HLHongbin Liu
Hongbin Liu
HLHailong Liu
Hailong Liu
In this paper, the effect of thermomechanical treatment process on the hardening behavior, grain microstructure, precipitated phase, and tensile mechanical properties of the new high-strength and high-ductility Al-10.0Zn-3.0Mg-2.8Cu alloy was studied, and the optimal thermomechanical treatment process was established. The strengthening and toughening mechanisms were revealed, which provided technical and theoretical guidance for the engineering application of this kind of high strength-ductility aluminum alloy. Al-10.0Zn-3.0Mg-2.8Cu alloy cylindrical parts with external longitudinal reinforcement were prepared by a composite extrusion deformation process (reciprocal upsetting + counter-extrusion) with a true strain up to 2.56, and the organizational evolution of the alloys during the extrusion deformation process and the influence of pre-stretching treatments on the subsequent aging precipitation behaviors and mechanical properties were investigated. The results show that firstly, the large plastic deformation promotes the fragmentation of coarse insoluble phases and the occurrence of dynamic recrystallization, which results in the elongation of the grains along the extrusion direction, and the volume fraction of recrystallization reaches 42.4%. Secondly, the kinetic study showed that the decrease in the activation energy of precipitation increased the nucleation sites, which further promoted the diffuse distribution of the second phase in the alloy and a higher number of nucleation sites, while limiting the coarsening of the precipitated phase. When the amount of pre-deformation was increased from 0% to 2%, the size of the matrix precipitated phase decreased from 5.11 μm to 4.1 μm, and when the amount of pre-deformation was increased from 2% to 7%, the coarsening of the matrix precipitated phase took place, and the size of the phase increased from 4.1 μm to 7.24 μm. The finalized heat treatment process for the deformation of the aluminum alloy tailframe was as follows: solution (475 °C/3 h) + 2% pre-stretching + aging (120 °C/24 h), at which the comprehensive performance of the alloy was optimized, with a tensile strength of 634.2 MPa, a yield strength of 571.0 MPa, and an elongation of 15.2%. The alloy was strengthened by both precipitation strengthening and dislocation strengthening. After 2% pre-stretching, the fracture surface starts to be dominated by dense tough nest structure, and most of them are small tough nests, and small and dense tough nests are the main reason for the increase in alloy toughness after 2% pre-stretching deformation.

24 February 2023 in Materials
Verified
Journal Article
Open access
PDF file
SWSi-Qi Wang
Si-Qi Wang
XZXi Zhao
Xi Zhao
XRXianwei Ren
Xianwei Ren
ZZZhimin Zhang
Zhimin Zhang
XTXue-Dong Tian
Xue-Dong Tian
YHyayun he
yayun he
In this paper, a hot processing map that takes into the strengthening effect into account is optimized for the Al–10.0Zn–3.0Mg–2.8Cu alloy, mainly considering the crushing and dissolving behavior of the insoluble phase. The hot deformation experiments were performed by compression testing with strain rates ranging from 0.001 to 1 s−1 and the temperature ranging from 380 to 460 °C. The hot processing map was established at the strain of 0.9. It exhibits that the appropriate hot processing region is located at the temperature from 431 to 456 °C and its strain rate is within 0.004–0.108 s−1. The recrystallization mechanisms and insoluble phase evolution were demonstrated using the real-time EBSD-EDS detection technology for this alloy. It is verified that the work hardening can also be consumed by the coarse insoluble phase refinement with the strain rate increasing from 0.001 to 0.1 s−1, besides the traditional recovery and recrystallization, but the effect of the insoluble phase crushing was weakened when strain rate increased over 0.1 s−1. Better refinement of the insoluble phase was around strain rate in 0.1 s−1, which exhibits adequate dissolving during the solid solution treatment, leading to excellent aging strengthen effects. Finally, the hot processing region was further optimized, so that the strain rate approaches 0.1 s−1 instead of 0.004–0.108 s−1. This will provide a theoretical support for the subsequent deformation of the Al–10.0Zn–3.0Mg–2.8Cu alloy and its’ engineering application in aerospace, defense and military fields.

7 June 2022 in Coatings
Verified
Journal Article
Open access
PDF file
JLJun Li
Jun Li
YHyayun he
yayun he
XZXi Zhao
Xi Zhao
Chan Kyung KimChan Kyung Kim
Chan Kyung Kim
Herein, composite extrusion deformation and heat treatment process at various temperatures were studied on a new type of Al-Zn-Mg-Cu alloy billet. The influence of pre-deformation and the final forming of extrusion and heat treatment of annular channel corner extrusion on the microstructure evolution and mechanical properties were explored. The results show that the extrusion process could further refine the structure and break the coarse θ phase. The grains can be refined again after the deformed sample was treated by solution-aging treatment. At the same time, a fine, dispersed second phase is precipitated around the fine recrystallized grains. This is the main reason for the increase in alloy elongation and tensile strength. The best heat treatment process parameters for the formed cup-shaped structure are 480 °C × 1 h solid solution and 120 °C × 24 h aging. The strengthening of the alloy mainly includes three mechanisms: fine grain strengthening, precipitation strengthening, and dispersion strengthening.