T Dhamothara Kannan

Mr. T Dhamothara Kannan

orcid

Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
19 January 2023 in International Journal on Interactive Design and Manufacturing (IJIDeM)
Verified
Journal Article
Closed access
PDF file
TKT Dhamothara Kannan
T Dhamothara Kannan
PSP. Sivaraj
P. Sivaraj
VBV. Balasubramanian
V. Balasubramanian
Tushar SonarTushar Sonar
Tushar Sonar
MIMikhail A. Ivanov
Mikhail A. Ivanov
SSS. Sathiya
S. Sathiya

5 December 2022 in Forces in Mechanics
Verified
Journal Article
Open access
TKT Dhamothara Kannan
T Dhamothara Kannan
PSP. Sivaraj
P. Sivaraj
VBV. Balasubramanian
V. Balasubramanian
SMS. Malarvizhi
S. Malarvizhi
TSTushar Sonar
Tushar Sonar
SSS. Sathiya
S. Sathiya

1 November 2022 in Materials Testing
Verified
Journal Article
Closed access
TKT Dhamothara Kannan
T Dhamothara Kannan
SPSivaraj Paramasivam
Sivaraj Paramasivam
SMSeeman Murugesan
Seeman Murugesan
BVBalasubramanian Visvalingam
Balasubramanian Visvalingam
Asymmetrical joints (joining of the plate with rod) were joined using traditional fusion welding processes. However, the usage of unsuitable filler wire tends to lower weld penetration over the material surface, which also results in the attainment of hot or solidification cracks over the weld surface. To overcome these issues, solid-state welding processes are preferable. This study investigates the rotary friction welding (RFW) of AISI 1018 low carbon steel plate with AISI 1020 low carbon steel rod of asymmetrical joints. The friction welding process parameters such as rotational speed were taken as variable, and other parameters like friction pressure, forging pressure, friction time, and forging time were kept constant in this investigation. The impact of rotational speed on macrostructure, microstructure, and mechanical characteristics of joints such as microhardness, tensile strength, and fractography studies was analyzed. The fractured surface of the tensile specimen was examined through a scanning electron microscope (SEM). The maximum tensile strength of the joint about 452 MPa was observed. Maximum hardness at the weld interface was perceived at about 252Hv. Increasing rotational speed tends to increase the strength of the asymmetrical steel joints in rotary friction welding.

1 December 2022 in Multidiscipline Modeling in Materials and Structures
Verified
Journal Article
Closed access
TKT Dhamothara Kannan
T Dhamothara Kannan
SPSivaraj Paramasivam
Sivaraj Paramasivam
BVBalasubramanian Visvalingam
Balasubramanian Visvalingam
Tushar SonarTushar Sonar
Tushar Sonar
SSSathiya Sivaraj
Sathiya Sivaraj
Purpose: Rotary friction welding (RFW) was used to solve the issues in fusion welding of rod to plate joints of low carbon steel (AISI 1020 steel/AISI 1018 steel) such solidification cracking, wider heat affected zone (HAZ), lower HAZ hardness, high residual stresses and distortion. The main objective of this investigation is to develop parametric mathematic models (PMMs), 3D response surface analysis to predict tensile strength (TS) and weld interface hardness (WIH) of rod to plate joints and correlate microstructure with TS and WIH of rod to plate joints.Design/methodology/approach: The three-factor x five-level central composite design (CCD) consisting fewer experiments was employed for designing experimental matrix. The tensile and microhardness tests were performed to evaluate mechanical performance of joints. The PMMs of TS and WIH of rod to plate joints were developed using polynomial regression equations incorporating the RFW parameters. The 3D response surfaces were developed using response surface methodology (RSM) to optimize RFW parameters for joining AISI 1020/AISI 1018 rod to plate.Findings: The joints made using friction pressure/friction time (FRNP/FRNT) of 3.71 MPa/s, forging pressure/forging time (FRGP/FRGT) of 3.71 MPa/s and rotational speed (RTSP) of 19.99 rps exhibited higher TS and WIH of 452 MPa and 252 HV0.5. The PMMs accurately predicted TS and WIH of rod to plate joints at less than 1.5% error and 95% confidence. The RTSP revealed greater effect on TS and WIH of rod to plate joints followed by FRGP/FRGT and FRNP/FRNT. The superior TS and WIH of joints developed using optimized process parameters is correlated to the evolution of finer bainitic microstructure in weld interface due to the dynamic recrystallization of grains ensued by optimum frictional heating and plastic deformation.Originality/value: The PMMs were developed for predicting TS and WIH of joints. The RFW parameters were optimized to enhance TS and WIH of joints. Low carbon steel rod to plates joints were developed using RFW for automotive applications without fusion welding defects. The microstructural features of low strength and high strength rod to plate joints were correlated to the TS and WIH of rod to plate joints.

1 January 2023 in Journal of the Mechanical Behavior of Materials
Verified
Journal Article
Open access
PDF file
TKT Dhamothara Kannan
T Dhamothara Kannan
SPSivaraj Paramasivam
Sivaraj Paramasivam
BVBalasubramanian Visvalingam
Balasubramanian Visvalingam
Tushar SonarTushar Sonar
Tushar Sonar
MIMikhail A. Ivanov
Mikhail A. Ivanov
SMSeeman Murugaesan
Seeman Murugaesan
The main objective of this study was to analyze the microstructural characteristics and strength performance of dissimilar AISI 431 steel/AISI 1018 steel joints developed using rotary friction welding. The microstructural characteristics of different regions of dissimilar rod-to-plate joints were analyzed using optical microscopy. The tensile properties and microhardness of dissimilar rod-to-plate joints were evaluated to assess the joint performance. The microhardness distribution across the cross-sectional region of dissimilar rod-to-plate joints was recorded and correlated with the tensile failure. Scanning electron microscopy was used to analyze the fractured region of dissimilar rod-to-plate tensile specimens. Results showed that the dissimilar AISI 431 steel/AISI 1018 steel joints steel exhibited a tensile strength of 650 MPa, a yield strength of 452 MPa, and a % elongation of 18%. The microhardness of the weld interface (WI) was higher up to 515 HV 0.5 . The grain growth and resulting lower hardness in heat-affected zone (HAZ) are mainly responsible for the failure of the joints in HAZ only. The superior tensile properties and greater interface hardness of dissimilar AISI 431 steel/AISI 1018 steel joints are correlated with the evolution of finer grain microstructure in the WI zone.