Manufacturers often employ the extrusion process to form an object with any cross-section. An experiment was carried out to examine the effect of die angle on the quality of the extruded product. The four types of extrusion dies were designed for finding the desirable quality of aluminium composite extruded billet. The five percentages of the Silicon carbide have been chosen as reinforcement with aluminium alloys. Further, the various extrusion dies configurations were considered as 12:8, 12:2, 12:4, and 8:4 for producing the extruded billets. In addition, the die angles that correspond to the required minimum extrusion load were determined. According to the findings, 12:8 extrusion configurations with a 30° die angle produced the desired quality billet and fine grain structure of extruded product with reduced extrusion load. The extruded billet surface quality was analyzed by scanning electron microscopy.
Asymmetrical joints (joining of the plate with rod) were joined using traditional fusion welding processes. However, the usage of unsuitable filler wire tends to lower weld penetration over the material surface, which also results in the attainment of hot or solidification cracks over the weld surface. To overcome these issues, solid-state welding processes are preferable. This study investigates the rotary friction welding (RFW) of AISI 1018 low carbon steel plate with AISI 1020 low carbon steel rod of asymmetrical joints. The friction welding process parameters such as rotational speed were taken as variable, and other parameters like friction pressure, forging pressure, friction time, and forging time were kept constant in this investigation. The impact of rotational speed on macrostructure, microstructure, and mechanical characteristics of joints such as microhardness, tensile strength, and fractography studies was analyzed. The fractured surface of the tensile specimen was examined through a scanning electron microscope (SEM). The maximum tensile strength of the joint about 452 MPa was observed. Maximum hardness at the weld interface was perceived at about 252Hv. Increasing rotational speed tends to increase the strength of the asymmetrical steel joints in rotary friction welding.
1 November 2020 in IOP Conference Series: Materials Science and Engineering
In this study, an effort has been made more complex multi performance optimization using Response Surface Methodology (RSM) based desirability approach while machining of Al/10%SiC Particulate Aluminum Metal Matrix Composite (PAMMC) produced through stir cast method. The effect of main cutting parameters like Cutting speed (V), Feed rate (F), Depth of cut (D) and Machining time (T) on the output responses of Tool flank wear (VBmax) and Surface roughness (Ra) were investigated. The most significant machining parameters were ascertained using analysis of variance (ANOVA). The contour plots are drawn for study effect cutting parameters and their interactions. From the study found that developed numberical model for tool flank wear and surface roughness is found to be adequate and used for predict the parameters within this experimental range.
1 January 2023 in Journal of the Mechanical Behavior of Materials
The main objective of this study was to analyze the microstructural characteristics and strength performance of dissimilar AISI 431 steel/AISI 1018 steel joints developed using rotary friction welding. The microstructural characteristics of different regions of dissimilar rod-to-plate joints were analyzed using optical microscopy. The tensile properties and microhardness of dissimilar rod-to-plate joints were evaluated to assess the joint performance. The microhardness distribution across the cross-sectional region of dissimilar rod-to-plate joints was recorded and correlated with the tensile failure. Scanning electron microscopy was used to analyze the fractured region of dissimilar rod-to-plate tensile specimens. Results showed that the dissimilar AISI 431 steel/AISI 1018 steel joints steel exhibited a tensile strength of 650 MPa, a yield strength of 452 MPa, and a % elongation of 18%. The microhardness of the weld interface (WI) was higher up to 515 HV 0.5 . The grain growth and resulting lower hardness in heat-affected zone (HAZ) are mainly responsible for the failure of the joints in HAZ only. The superior tensile properties and greater interface hardness of dissimilar AISI 431 steel/AISI 1018 steel joints are correlated with the evolution of finer grain microstructure in the WI zone.