V2O5-WO3/TiO2 as a commercial selective catalytic reduction (SCR) catalyst usually used at middle-high temperatures was modified by loading of MnOx for the purpose of enhancing its performance at lower temperatures. Manganese oxides were loaded onto V-W/Ti monolith by the methods of impregnation (I), precipitation (P), and in-situ growth (S), respectively. SCR activity of each modified catalyst was investigated at temperatures in the range of 100–340 °C. Catalysts were characterized by specific surface area and pore size determination (BET), X-ray diffraction (XRD), temperature programmed reduction (TPR), etc. Results show that the loading of MnOx remarkably enhanced the SCR activity at a temperature lower than 280 °C. The catalyst prepared by the in-situ growth method was found to be most active for SCR.
Manganese oxide-supported palygorskite (MnOx/PG) catalysts are considered highly efficient for low-temperature SCR of NOx. However, the MnOx/PG catalyst tends to be poisoned by SO2. The effect of SO2 on activity of the SO2-pretreated poisoning catalysts under ammonia-free conditions was explored. It was determined that the MnOx/PG catalyst tends to be considerably deactivated by SO2 in the absence of ammonia and that water-washed regeneration can completely recover activity of the deactivated catalyst. Based on these results and characterizations of the catalysts, a reasonable mechanism for the deactivation of MnOx/PG catalyst by SO2 was proposed in this study. SO2 easily oxidized to SO3 on the surface of the catalyst, leading to the formation of polysulfuric acid, wrapping of the active component and blocking the micropores. The deactivation of the MnOx/PG catalyst is initially caused by the formation of polysulfuric rather than the deposition of ammonia sulfate, which occurs later.
3 February 2022 in Journal of Environmental Chemical Engineering
MnO2-CeO2/PG-FA catalysts were prepared by supporting MnO2-CeO2 to PG-FA and used to remove Hg0 in simulated flue gas. The results show that MnO2-CeO2/PG-FA catalyst had excellent and stable Hg0 removal activity, which was mainly due to the combination effect of the catalytic oxidation activity by MnO2-CeO2 and the adsorption ability by PG-FA. Mn8-Ce0.5/PG-FA (with 8.0% MnO2 and 0.5% CeO2 loading) catalyst showed the highest Hg0 removal efficiency at 140 °C and Hg0 removal efficiency could be maintained above 95% with the space velocity of 6000 h−1 and Hg0 concentration of 160 μg/m3. O2 promoted Hg0 removal by MnO2-CeO2/PG-FA catalyst, while SO2 and H2O had inhibitory effects. In the presence of O2, the inhibitory effect of SO2 and H2O can be obviously weakened. MnO2-CeO2/PG-FA catalysts were characterized with scanning electron microscope (SEM), X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and temperature-programmed desorption experiments (TPD). The results of SEM and XRD showed that the active components MnO2-CeO2 dispersed well on the surface of PG-FA support. The results of XPS and TPD show that the Hg0 removal process over MnO2-CeO2/PG-FA catalyst included adsorption and oxidation, HgO and HgSO4 were generated and adsorbed on the catalyst. MnO2-CeO2/PG-FA catalyst also showed excellent regeneration performance after Hg0 removal.