V2O5-WO3/TiO2 as a commercial selective catalytic reduction (SCR) catalyst usually used at middle-high temperatures was modified by loading of MnOx for the purpose of enhancing its performance at lower temperatures. Manganese oxides were loaded onto V-W/Ti monolith by the methods of impregnation (I), precipitation (P), and in-situ growth (S), respectively. SCR activity of each modified catalyst was investigated at temperatures in the range of 100–340 °C. Catalysts were characterized by specific surface area and pore size determination (BET), X-ray diffraction (XRD), temperature programmed reduction (TPR), etc. Results show that the loading of MnOx remarkably enhanced the SCR activity at a temperature lower than 280 °C. The catalyst prepared by the in-situ growth method was found to be most active for SCR.
A new kind DGA modified MIL-101-NH 2 MOFs supported on PVDF composite membrane (DGA-M1N@PVDF) was synthesized, which had superior selectivity, good adsorption capacity and good recycling performance on REEs in waste phosphor.
To overcome the urgency of zirconium and hafnium separation, a novel mesoporous silica sorbent (PS-G1.0-MSNs) modified with phosphorous-functionalized G1.0 PAMAM dendrimers was prepared. The adsorption and separation behaviors of PS-G1.0-MSNs adsorbent on Zr(IV) and Hf(IV) were perfromed as a function of acidity, contact time, temperature, and ion concentrations by batch sorption methods. The maximum adsorption capacities for Zr(IV) and Hf(IV) were 25.7 mg g−1 and 5.36 mg g−1 under optimal experimental conditions, respectively, and the separation factor βHf/Zr = 2.0 > 1 demonstrated that the prepared sorbent had preferential selectivity for Hf(IV) in rich Zr(IV) solution. Moreover, kinetic data indicated that the sorption process on Zr(IV) and Hf(IV) achieved equilibrium within 120 min, and followed the pseudo-first-order model with a rate-determining step. The adsorption amount increased as temperature raised from 283 K to 303 K and the isothermal data plotted with the Langmuir model was better than the Freundlich model with monolayer behavior. Thermodynamic data analysis indicated that the sorption process was spontaneous and endothermic. Furthermore, XPS analysis revealed that the metal ion adsorption was mainly induced by the chemical coordination of Zr(IV) and Hf(IV) ions with N, O, P atoms of amide and phosphate groups. The present work provides good guidelines on the design of high efficient sorbent for the separation of Hf(IV) from Zr(IV) solutions.
Electrochemical seawater splitting is an intriguing strategy for green hydrogen production. Constructing advanced electrocatalysts for the hydrogen evolution reaction (HER) in seawater is extremely demanded for accelerating the sluggish kinetic process. Herein, a Ru nanocluster anchored on boron- and nitrogen-doped carbon (Ru/NBC) catalyst was successfully synthesized for the HER in alkaline/seawater electrolytes. Remarkably, Ru/NBC exhibits outstanding activity and durability, delivering low overpotentials@10 mA cm−2 in 1.0 M KOH (30 mV) and 1.0 M KOH + seawater electrolyte (35 mV), outperforming Pt/C, Ru/NC, Ru/BC and Ru/C. Additionally, Ru/NBC also provides a high specific activity of 0.093 mA cm−2ECSA at an overpotential of 150 mV, which is higher than those of Ru/NC, Ru/BC and Ru/C, respectively. Density functional theory calculation results demonstrate that the Ru–B formed interfacial chemical bond can regulate the electronic structure of Ru active sites of Ru/NBC, which can facilitate the adsorption of water and hydrogen in alkaline media. This work provides a feasible strategy to fabricate outstanding electrocatalysts for the HER in alkaline/alkaline seawater electrolytes.
20 August 2018 in Journal of Electrochemical Energy Conversion and Storage
The effects of particle size distribution on compacted density of as-prepared spherical lithium iron phosphate (LFP) LFP-1 and LFP-2 materials electrode for high-performance 18650 Li-ion batteries are investigated systemically, while the selection of two commercial materials LFP-3 and LFP-4 as a comparison. The morphology study and physical characterization results show that the LFP materials are composed of numerous particles with an average size of 300–500 nm, and have well-developed interconnected pore structure and a specific surface area of 13–15 m2/g. For CR2032 coin-type cell, the specific discharge capacities of the LFP-1 and LFP-2 are about 165 mAh/g at 0.2 C. For 18650 batteries, results indicate that the LFP-3 material has the highest compacted density of 2.52 g/cm3 at a concentrated particle size distribution such as D10 = 0.56 μm, D50 = 1.46 μm, and D90 = 6.53 μm. By mixing two different particle sizes of LFP-1 and LFP-2, the compaction density can be increased significantly from 1.90 g/cm3 to 2.25 g/cm3.