Citric acid together with sorbitol (SorCA) have been used to modify wood and improve its properties, such as dimensional stability and biological durability, which partly result from its swelling and sorption behavior. However, the underlying mechanism of water interaction with SorCA-treated wood is very complex and not fully understood. Previous research confirmed cell wall bulking and suggested cross-linking, however the extent of their contribution to moisture-induced changes has not been researched. This study investigated the effect of SorCA treatment on sorption properties of wood in the hygroscopic range (0–95% RH). Scots pine sapwood (Pinus sylvestris L.) was chemically modified with an aqueous SorCA solution at different treatment levels and measured by dynamic vapor sorption (DVS). The observed permanent increase in oven-dry dimensions did not result in a decreased swelling compared to untreated specimens. It was ascribed to the excessive expansion of cell wall matrix caused by a degradation of cell wall constituents by the acidic impregnation solution. However, a reduction in moisture content in comparison to untreated reference was detected. Present findings suggest that the SorCA polyester structure is altered after impregnation inside the wood and affects its sorption behavior by covalent bonding and, presumably, cross-linking with wood polymer constituents.
12 May 2021 in Wood Material Science & Engineering
In recent years, a wood treatment system based on sorbitol and citric acid (SorCA) has emerged as a promising alternative to already commercialized modification processes of European-grown wood species. The improvement of dimensional stability and biological durability have been reported. However, the mode of action behind the changes in wood structure leading to these improvements has not been well defined yet, as the research was based on the infrared spectroscopy, which cannot distinguish nor compare the effect of cell wall bulking (CWB), covalent bonding and cross-linking. Moreover, most of the assumptions regarding the reaction mechanism have resulted from the studies of citric acid reactions with wood and wood-based products. Therefore, in this study different analytical chemistry methods have been used to explain the interaction between SorCA and wood at two polymerization temperatures (120 and 140°C). It has been confirmed that the curing temperature is a crucial parameter for achieving the desired fixation. Subsequently, liquid chromatography-mass spectrometry (LC-MS), cross-polarization/magic angle spinning (CP/MAS 13C-NMR) spectroscopy and pyrolysis gas chromatography-mass spectrometry (Py-GC/MS) have been used to determine the contribution caused by an in-situ formation of high molecular-weight SorCA polyesters (resulting in CWB) and a higher rate of esterification of wood polymers.
Recent studies showed treatments with sorbitol and citric acid (SorCA) to significantly improve the dimensional stability and biological durability of wood. The industrialization of this process requires a quality control (QC) method to determine if the fixated chemicals are homogenously distributed within the piece of wood, which is essential for uniform material performance. Therefore, the objective of this work was to evaluate the use of common electromagnetic radiation-based methods to determine the degree of modification in SorCA-treated wood. Both Fourier transform infrared (FTIR) spectroscopy and near-infrared (NIR) spectroscopy have been used to create rough calibrations for the weight percent gain (WPG) prediction models. The FTIR measurements resulted in a high linear correlation between the band area ratio (BAR) and the WPG (R2 = 0.93). Additionally, a partial least square (PLS) regression of NIR spectroscopic data resulted in a model with a high prediction power (R2 = 0.83). Furthermore, X-ray density profiling emerged as a simple alternative for the QC by showing a gradient of modification chemicals inside the sample and differences in chemical uptake between earlywood and latewood. Overall, it can be concluded that the results from FTIR, NIR and X-ray densitometry can serve as indicators of impregnation chemical distribution in SorCA-modified wood.
This study aimed to investigate the relationship between moisture dynamics of sorbitol and citric acid (SorCA) modified wood and its biological durability. Specifically, the research aimed to determine the chemical loading needed for effective protection against wood-destroying basidiomycetes, while also improving the understanding of the moisture behavior of SorCA-modified wood. The SorCA modification process is relatively new, and thus, there is limited knowledge on its moisture behavior and its impact on biological durability. The research focused on Scots pine sapwood (Pinus sylvestris L.) and used the EN 113-2 standard to investigate its durability against wood-destroying basidiomycetes. Moisture behavior was analyzed through short-term water uptake and release tests, capillary water uptake and CEN/TS 16818. Results showed a significant reduction in liquid and water vapor uptake, likely due to a reduction in the maximum moisture capacity within the wood cell wall. The study confirmed that high chemical loadings (i.e., weight percent gain, WPG) are necessary for adequate decay protection.
Scots pine sapwood (Pinus sylvestris L.) was modified with an aqueous solution of sorbitol and citric acid (SorCA) and a commercial phosphorus-based fire-retardant (FR). The aim of this study was to assess whether the fire behavior can be improved when the SorCA solution is supplemented by an FR and if this effect is resistant to leaching. The fire behavior of modified wood was investigated by a Bunsen burner ignition test, mass loss calorimetry (MLC) and thermogravimetric analysis (TGA). The results demonstrated a significantly improved fire-retardancy based on a decreased burning rate and a reduced mass loss in the Bunsen burner test. Also, the induced formation of a protective char barrier facilitated by the addition of a FR, reduced the heat release rate and delayed the ignition. The fire-retardant effect was still observed, to the less extent, after a cold-water (EN 84 2020) leaching of the specimens.