The main goal of this paper was to study the dielectric properties of hybrid binary and ternary composites based on biodegradable polymer Ecoflex®, single walled carbon nanotubes (SWCN), and liquid crystalline 4′-pentyl-4-biphenylcarbonitrile (5CB) compound. The obtained results were compared with other created analogically to Ecoflex®, hybrid layers based on biodegradable polymers such as L,D-polylactide (L,D-PLA) and polycaprolactone (PCL). Frequency domain dielectric spectroscopy (FDDS) results were analyzed taking into consideration the amount of SWCN, frequency, and temperature. For pure Ecoflex®, two relaxation processes (α and β) were identified. It was shown that the SWCN admixture (in the weight ratio 10:0.01) did not change the properties of the Ecoflex® layer, while in the case of PCL and L,D-PLA, the layers became conductive. The dielectric constant increased with an increase in the content of SWCN in the Ecoflex® matrix and the conductive behavior was not visible, even for the greatest concentration (10:0.06 weight ratio). In the case of the Ecoflex® polymer matrix, the conduction relaxation process at a frequency ca. several kilohertz appeared and became stronger with an increase in the SWCN admixture in the matrix. Addition of oleic acid to the polymer matrix had a smaller effect on the increase in the dielectric response than the addition of liquid crystal 5CB. Fourier transform infrared (FTIR) results revealed that the molecular structure and chemical character of the Ecoflex® and PCL matrixes remained unchanged upon the addition of SWCN or 5CB in a weight ratio of 10:0.01 and 10:1, respectively, while molecular interactions appeared between L,D-PLA and 5CB. Moreover, adding oleic acid to pure Ecoflex® as well as the binary and ternary hybrid layers with SWCN and/or 5CB in a weight ratio of Ecoflex®:oleic acid equal to 10:0.3 did not have an influence on the chemical bonding of these materials.
Physical properties of the partially fluorinated compound 3F5FPhF, with hockey stick-like molecules, were studied by complementary methods. Apart from the already reported paraelectric SmA*, ferroelectric SmC* and antiferroelectric SmC*A phases, the presence of the smectic C*α subphase in the phase sequence was proved by differential scanning calorimetry, polarising optical microscopy, electro-optic and dielectric spectroscopy methods. The temperature dependence of the smectic layer thickness and correlation length of the lateral short-range order was determined by X-ray diffraction. Based on dielectric measurements three relaxation processes were revealed in the antiferroelectric SmC*A phase (two collective: PL, PH and one molecular: s-process), two collective ones (Goldstone and soft modes) were found both in the ferroelectric SmC* phase and SmC*α subphase while one relaxation process (soft mode) in the paraelectric SmA* phase. The results were compared with that obtained for other structurally similar compounds, and it was shown that even addition of one methylene group to the side chain influences much on the physical properties.
The molecular dynamics, with an emphasis on the calorimetric and dynamic glass transitions, of non-isocyanate polyhydroxyurethanes (PHUs) produced by the equimolar polyaddition of polyether-based dicyclic carbonates (P-CCs) and various short diamines was studied. The diamine component consisted of a short aliphatic diamine (1,4-diaminobutane, DAB) and a more complex ‘characteristic’ diamine. The study was conducted to investigate (i) the chemical structure of the characteristic amine, (ii) its molar ratio, and (iii) the structure and molar mass of the P-CC. Infrared spectroscopy, differential scanning calorimetry, and broadband dielectric spectroscopy were employed. The P-CC, constituting the bulk of the systems, was the most crucial component for the glass transition. The characteristic amine influenced the glass transition as a result of its bulky structure, but also presumably as a result of the introduction of free volume and the formation of hydrogen bonds. The dynamic glass transition (α relaxation) trace in the Arrhenius plots showed a subtle change at a certain temperature that merits further study in the future. The charge mobility was fully coupled with the molecular mobility, as evidenced by dc conductivity being directly proportional to the characteristic frequency of α relaxation. The fluctuation in carbonyl units (β relaxation) was mildly affected by changes in their immediate environment.
Modification of the physical properties of the (S)-MHPOBC antiferroelectric liquid crystal (AFLC) by doping with low concentrations of gold nanoparticles is presented for the first time. We used several complementary experimental methods to determine the effect of Au nanoparticles on AFLC in the metal–organic composites. It was found that the dopant inhibits the matrix crystallization process and modifies the phase transitions temperatures and switching time, as well as increases the helical pitch and spontaneous polarization, while the tilt angle slightly changes. We also showed that both the LC matrix and Au nanoparticles show strong fluorescence in the green light range, and the contact angle depends on the temperature and dopant concentration.