The aim of this study was to investigate the effect of inorganic cations (Na+, Ca2+, Ba2+, Fe3+, Al3+) with different valence and concentration on the swelling behaviors of montmorillonite. Na-montmorillonite, obtained from China, was chosen as experimental objective. It was first characterized through the measurements of swelling capacity and zeta potential. Then, swelling properties of Na-montmorillonite influenced by cation concentration, valence, and hydration analyzed were studied. The results showed that the swelling capacity was much inhibited by cations of higher concentrations, higher valences, or weaker hydration. This work also verified the conclusion that the decreased degree of potential is more significant caused by cations of higher valence. GRAPHICAL ABSTRACT
The delamination of montmorillonite in water leads to sliming in ore slurry, which is detrimental to mineral flotation and solid/water separation. In this work, the delamination of Na-montmorillonite (Na-MMT) has been restrained by sodium dodecyl sulfate (SDS) or octadecyl trimethyl ammonium chloride (1831) through the adsorption on the edge of the mineral. The experimental results have shown that the pretreatment by adding SDS and 1831 could greatly reduce the Stokes size percentage of −1.1 µm particles in the aqueous Na-MMT suspension. From the X-ray diffractometer (XRD) results, the interlayer spacing of the MMT pre-treated by SDS and 1831 is smaller than that of original MMT particles. Adsorption position of SDS and 1831 on MMT surfaces was analyzed by the measurements of adsorption capacity of SDS and 1831, inductively-coupled plasma spectra, and zeta potential before and after the plane surface of MMT was covered with tetraethylenepentaminecopper ([Cu(tetren)]2+). The results indicated that SDS and 1831 are adsorbed on the edge and the whole surface of Na-MMT, respectively. Delamination of MMT could be well restrained by the adsorption of SDS and 1831 on the edges of MMT.
Mining tailings as a raw material for preparing autoclaved bricks have attracted much attention. The tailings subjected to milling always have the characteristic of fine granularity. However, the proportion of the fine aggregates in autoclaved bricks was very low using the current gradation formula, which impeded the utilization of the tailings. In this work, a novel model of aggregate gradation for autoclaved bricks from tailings has been presented, which was established through the following steps: (1) 91 groups of autoclaved bricks with different aggregate gradations were prepared, with the proportion of the fine aggregates (−0.15 mm) in the range of 40% to 100%; and (2) the particle size distributions of the finest and coarsest aggregates in the high-strength region were fitted to establish the model. The proportion of the fine aggregates calculated by the model could increase significantly compared with that using the current formula. To verify the novel model, autoclaved bricks from iron ore tailings were prepared using the model, with their mechanical and freezing resistance properties meeting the requirement of the highest-strength level. It was observed by SEM that the autoclaved bricks had compact structures with a few small pores owing to the reasonable aggregate gradation.
13 March 2017 in Asia-Pacific Journal of Chemical Engineering