Highly ordered TiO2 nanotubes (TNTs) decorated with a series of lanthanide ions (Ln3+ = Ho3+, Tb3+, Eu3+, Yb3+, and Er3+) were prepared through an electrochemical process and anodization. The composition, structure, and chemical bond of the as-prepared photocatalysts were characterized through scanning electron microscopy, X-ray diffraction, X-ray photoelectron spectroscopy, ultraviolet photoelectron spectroscopy, and ultraviolet diffuse reflectance spectroscopy. Furthermore, the electrochemical characteristics of the catalysts were analyzed and photoelectrochemical properties were investigated through water splitting. All samples were prepared in the anatase phase without changing the crystal structure. The holmium-doped TNT photocatalyst exhibited the best performance with a hydrogen evolution rate of 90.13 μmol cm−2h−1 and photoconversion efficiency of 2.68% (0 V vs. RHE). Photocatalytic efficiency increased because of the expansion of the absorption wavelength range attributed to the appropriate positioning of the band structure and reduced electron/hole pair recombination resulting from the unhindered electron movement. This study demonstrated the preparation of high-potential solar-active photocatalysts through the synergetic effects of the work function, band edge, and bandgap changes caused by the series of lanthanide combinations with TNTs.
Ni (hydr)oxide is a promising and inexpensive material for oxygen evolution reaction (OER) catalysts and is known to dramatically increase the activity when used with Fe. Herein, we basified a Ni(II) solution and coated layered Ni(OH)2 on Ni coins to prepare a template with high stability and activity. To evaluate the stability and catalytic activity during high-current-density operation, we analyzed the electrochemical and physicochemical properties before and after constant current (CC) operation. The electrode with a Ni(OH)2 surface exhibited higher initial activity than that with a NiO surface; however, after the OER operation at a high-current density, degradation occurred owing to structural destruction. The activity of the electrodes with a NiO surface improved after the CC operation because of the changes on the electrode-surface caused by the CC operation and the subsequent Fe incorporation from the Fe impurity in the electrolyte. After confirming the improvement in activity due to Fe, we prepared NiFe-oxide electrodes with improved catalytic activity and optimized the Ni precursor and Fe loading solution concentrations. The Ni-Fe oxide electrode prepared under the optimal concentrations exhibited an overpotential of 287 mV at a current density of 10 mA/cm2, and a tafel slope of 37 mV dec−1, indicating an improvement in the OER activity.
28 February 2020 in Transactions of the Korean hydrogen and new energy society
In this study, we investigated the oxygen evolution reaction (OER) characteristics of Ni–Zn–Fe electrodes by varying plating current density and Ni:Fe ratio in a plating bath. The activity of the OER increased up to the plating current density of 160 mA/cm2, as the Fe content of the deposited electrode increased and electrochemical surface area (ECSA) increased after Zn dealloying. However, for the plated electrode with higher than 160 mA/cm2 of current density, the change in composition caused by underpotential deposition led to decreased activity due to decreasing Fe content and diminishing Zn dealloying. Moreover, when the Ni:Fe ratio in the plating bath was varied, outstanding OER activity was observed at Ni:Fe = 2:1. When the Fe content of the bath increased beyond this ratio, Fe could not restrain Ni oxidation and formed Fe oxides in OER reaction, and oxygen vacancy decreased. These caused a degradation of the OER activity.
Cubic delta-tantalum nitride (δ-TaN) nanoparticles were selectively prepared using a K2TaF7 + (5 + k) NaN3 + kNH4F reactive mixture (k being the number of moles of NH4F) via a combustion process under a nitrogen pressure of 2.0 MPa. The combustion temperature, when plotted as a function of the number of moles of NH4F used, was in the range of 850°C to 1,170°C. X-ray diffraction patterns revealed the formation of cubic δ-TaN nanoparticles at 850°C to 950°C when NH4F is used in an amount of 2.0 mol (or greater) in the combustion experiment. Phase pure cubic δ-TaN synthesized at k = 4 exhibited a specific surface area of 30.59 m2/g and grain size of 5 to 10 nm, as estimated from the transmission electron microscopy micrograph. The role of NH4F in the formation process of δ-TaN is discussed with regard to a hypothetical reaction mechanism.