Foam concrete is fire resistant and durable and has broad applicability as a building insulation material. However, cement has high energy consumption and causes pollution, necessitating an environment-friendly cementitious material to replace the cement used to prepare foam concrete. In this study, foam concrete was prepared through chemical foaming. The influence of the foaming agent material, foam stabiliser, and fly ash on the basic properties of the foam concrete, including the dry bulk density, compressive strength, and thermal conductivity, was studied, and the pore structure was characterised. The results show that with an increase in the hydrogen peroxide (H2O2) content, the dry bulk density, compressive strength, and thermal conductivity of foam concrete decreases, whereas the pore diameter increases (0.495 to 0.746 mm). When the calcium stearate content is within 1.8%, the pore size tends to increase (0.547 to 0.631 mm). With increase in the fly ash content, the strength of foam concrete gradually decreases, and the dry bulk density first decreases and then increases. When the blending ratio of fly ash is 10–40%, the thermal conductivity gradually decreases; an extreme thermal conductivity of 0.0824 W/(m·K) appears at the blending ratio of 40%, and the dry bulk density is 336 kg/m3.
15 April 2024 in Construction and Building Materials
To study the durability of concrete with fly ash as fine aggregate subjected to alternative attacks of freeze‐thaw and carbonation, the appearance, mass loss, relative dynamic modulus of elasticity, relative compressive strength, and carbonation depth of the concrete are investigated using cyclic tests under single carbonation, single freeze‐thaw, and alternation of freeze‐thaw and carbonation. In addition, microstructural analysis techniques including scanning electron microscope and X‐ray diffraction are adopted to reveal the deterioration mechanism of alternating freeze‐thaw and carbonation. Results show that carbonation is beneficial for refining the pore structure and increasing concrete strength in the initial alternative cycle, which delays the damage from freeze‐thaw cycles. Damage from freeze‐thaw causes crack propagation in concrete, which leads to carbonation intensification. Compared with other test modes, concrete under alternative freeze‐thaw and carbonation causes the greatest degree of deterioration during the initial freeze‐thaw cycles. The carbonation depth under alternative freeze‐thaw and carbonation is positively correlated with the carbonation time and the water‐to‐cement ratio. However, as the reactant is continuously consumed due to the expansion of crystalline ice and CaCO3, alternative cycles result in the appearance of many more new cracks in the concrete.