Ni-gadolinia-doped ceria (GDC) based electrode materials have drawn significant attention as an alternative fuel electrode for solid oxide cells (SOCs) owing to mixed ionic conductivity of GDC and high electronic and catalytic activity of Ni. Moreover, the catalytic activity and electrochemical performance of the Ni-GDC electrode can be further improved by dispersing small quantities of other metal additives, such as gold or molybdenum. Therefore, herein, we considered gold and molybdenum modified Ni-GDC electrodes and focused on the upscaling; hence, we prepared 5 × 5 cm2 electrolyte-supported single cells. Their electrochemical performance was investigated at different temperatures and fuel gas compositions. The long-term steam electrolysis test, up to 1700 h, was performed at 900 °C with −0.3 A·cm−2 current load. Lastly, post-test analyses of measured cells were carried out to investigate their degradation mechanisms. Sr-segregation and cobalt oxide formation towards the oxygen electrode side, and Ni-particle coarsening and depletion away from the electrolyte towards the fuel electrode side, were observed, and can be considered as a main reason for the degradation. Thus, modification of Ni/GDC with Au and Mo seems to significantly improve the electro-catalytic activity of the electrode; however, it does not significantly mitigate the Ni-migration phenomenon after prolonged operation.
High-temperature electrolysis using solid oxide electrolysis cells (SOECs) is an innovative technology to temporarily store unused electrical energy from renewable energy sources. However, they show continuous performance loss during long-term operation, which is the main issue preventing their widespread use. In this work, we have performed the long-term stability tests up to 1000 h under steam and co-electrolysis conditions using commercial NiO-YSZ/YSZ/GDC/LSC single cells in order to understand the degradation process. The electrolysis tests were carried out at different temperatures and fuel gas compositions. Intermittent AC- and DC- measurements were performed to characterize the single cells and to determine the responsible electrode processes for the degradation during long-term operation. An increased degradation rate is observed at 800 °C compared to 750 °C under steam electrolysis conditions. Moreover, a lower degradation rate is noticed under co-electrolysis operation in comparison to steam electrolysis operation. Finally, the post-test analyses using SEM-EDX and XRD were carried out in order to understand the degradation mechanism. The delamination of LSC is observed under steam electrolysis conditions at 800 °C, however, such delamination is not observed during co-electrolysis operation. In addition, Ni-depletion and agglomeration are observed on the fuel electrode side for all the cells.
Chemical industries rely heavily on fossil resources for the production of carbon-based chemicals. A possible transformation towards sustainability is the usage of carbon dioxide as a source of carbon. Carbon dioxide is activated for follow-up reactions by its conversion to carbon monoxide. This can be accomplished by electrochemical reduction in solid oxide cells. In this work, we investigate the process performance of the direct high-temperature CO2 electrolysis by current-voltage characteristics (iV) and Electrochemical Impedance Spectroscopy (EIS) experiments. Variations of the operation parameters temperature, load, fuel utilization, feed gas ratio and flow rate show the versatility of the procedure with maintaining high current densities of 0.75 up to 1.5 A·cm−2, therefore resulting in high conversion rates. The potential of the high-temperature carbon dioxide electrolysis as a suitable enabler for the activation of CO2 as a chemical feedstock is therefore appointed and shown.